Hi
so i was thinking about something,
we can't reflux aqueous ammonia,
since its will just leave the solvent,
so i was thinking what about making a chemical reactor out of a paintball co2 bottle, its made of steel i doubt ammonia will attack steel,

so to get an idea about how much a paintball co2 bottle,


Carbon dioxide Vapor pressure
25 Celcius 6445.15 kpa
77 Fahrenheit 934.79 Psi

and water at the temperature that is require for the reaction

water Vapor pressure
130 Celcius 268.2 Kpa
266 Fahrenheit 38.9 Psi


logicaly water heated at 130 celcius exert less pressure than carbon dioxide at 25 celcius
so if we put an solution of ammonia in a paintball bottle and seal it and heat it to 130 celcius,
its should take it easily wihout breaking,
am i right ?
i need some idea for that pressure reactor,

need to handle ammonia solution (25%)
at 130 Celcius wihout anything escaping it for at least 3 hour
View user's profile View All Posts By User
XeonTheMGPony
International Hazard
*****




Posts: 1641
Registered: 5-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 24-1-2016 at 18:14


1800 psi mop

NH4 anhydrous will not attack steel
View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 24-1-2016 at 18:25


You could reflux with a Dewar condenser, couldn't you? Stainless steel holds up well against ammonia, regular steel not so well.... Also worth considering is how pressure will affect the reaction.
View user's profile View All Posts By User
nelsonB
Hazard to Self
**




Posts: 71
Registered: 5-9-2013
Member Is Offline

Mood: No Mood

[*] posted on 24-1-2016 at 19:20


i was thinking finding a way to put an enamel inside of the co2 bottle, incase of corrosion.
View user's profile View All Posts By User
gsd
National Hazard
****




Posts: 847
Registered: 18-8-2005
Member Is Offline

Mood: No Mood

[*] posted on 24-1-2016 at 20:02


If it is only NH3 and Water, corrosion is not much of a problem. Ammonia Absorption Chillers are made from mild steel.
Your problem is not the vapour pressure of water at 130 Deg C. It is the vapour pressure of NH3 + Water system at that temperature. look up for that in the Mollier diagram for NH3 + H2O.

gsd
View user's profile View All Posts By User
Bert
Super Administrator
Thread Moved
24-1-2016 at 20:09
nelsonB
Hazard to Self
**




Posts: 71
Registered: 5-9-2013
Member Is Offline

Mood: No Mood

[*] posted on 25-1-2016 at 08:19


one way to know if its gonna word, its to test it.

I wonder what would be the best way to get a stable temp

sensor inside or outside,
outside would be easier since there will be no stress by pression,
but its less accurate i think,


inside its harder but there more accurate but its could be prone to breakage


[Edited on 25-1-2016 by nelsonB]
View user's profile View All Posts By User
nelsonB
Hazard to Self
**




Posts: 71
Registered: 5-9-2013
Member Is Offline

Mood: No Mood

[*] posted on 26-1-2016 at 15:17


another way i guess would be to not fill it full,
leaving some space so the pressure do not reach some critical high level
View user's profile View All Posts By User