Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Best Vintage for HDD magnets
NEMO-Chemistry
International Hazard
*****




Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 10-9-2016 at 12:42
Best Vintage for HDD magnets


Reading various threads on Neodymium from HDD magnets, it looks like the composition of the magnets has changed over time.

Weeks back i mentioned a computer shop that had closed and dumped a load of gear, in the lot i managed to bring home are some old HDD's.

From the size (storage capacity) and a few of the date codes on them, it looks like i have a few from late 80's right upto around 2005.

There isnt many of them but i wondered what age HDD's have the best magnets for Neodymium? I would like to have a go at extracting some Neodymium compounds, mainly Chloride.silphate and nitrate.

Cheers
View user's profile View All Posts By User
RogueRose
International Hazard
*****




Posts: 1601
Registered: 16-6-2014
Member Is Offline


[*] posted on 10-9-2016 at 18:51


last years of 5.25" HD's and the first years of 3.5" SCSI hard drives. They both had really large magnets
View user's profile View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 12-9-2016 at 07:00


The older they are, the more likely they are to have SmCo magnets rather than Nd. I ran into that a few times when I got excited about some very large magnets, then dissolved them in sulfuric acid only to get a green solution instead of a purple one! So large magnets may not necessarily be a good thing.
View user's profile Visit user's homepage View All Posts By User
NEMO-Chemistry
International Hazard
*****




Posts: 1559
Registered: 29-5-2016
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 12-9-2016 at 08:40


Quote: Originally posted by MrHomeScientist  
The older they are, the more likely they are to have SmCo magnets rather than Nd. I ran into that a few times when I got excited about some very large magnets, then dissolved them in sulfuric acid only to get a green solution instead of a purple one! So large magnets may not necessarily be a good thing.


Ok so green = bad and pink = good! 2 really old ones look a nightmare to get into.
View user's profile View All Posts By User
Deathunter88
National Hazard
****




Posts: 570
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline

Mood: No Mood

[*] posted on 12-9-2016 at 08:53


Quote: Originally posted by NEMO-Chemistry  
Quote: Originally posted by MrHomeScientist  
The older they are, the more likely they are to have SmCo magnets rather than Nd. I ran into that a few times when I got excited about some very large magnets, then dissolved them in sulfuric acid only to get a green solution instead of a purple one! So large magnets may not necessarily be a good thing.


Ok so green = bad and pink = good! 2 really old ones look a nightmare to get into.


Huh? Every time I've dissolved magnets it has resulted in a green solution but it still produced nice pink neodymium sulphate crystals.
View user's profile View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 12-9-2016 at 09:28


I'd guess the green was probably iron(II) in that case, although that is also what's in the purple/pink solutions. Usually the Nd color washes out any iron colors. Weird that it seems in some cases it doesn't. I'll admit I didn't try to process any of my green solutions, because I had plenty of purple/pink ones to go through. Sounds like a good experiment!

[Edited on 9-12-2016 by MrHomeScientist]
View user's profile Visit user's homepage View All Posts By User
Mabus
Wiki Master
***




Posts: 241
Registered: 3-11-2013
Member Is Offline

Mood: Energetic

[*] posted on 13-9-2016 at 09:20


At least one of the earliest types of HDD (a big one) I took apart some time ago had a typical AlNiCo/ferrite magnet, and ferrite (?) shielding. But they're easy to tell apart from Nd magnets: their color is black and don't react fast with acids.



View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4737
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: Seeking gainful employment

[*] posted on 13-9-2016 at 09:38


Quote: Originally posted by MrHomeScientist  
Usually the Nd color washes out any iron colors.
That seems unlikely, being as the magnets contain far more iron than neodymium and the color of neodymium in solution is not incredibly strong.



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3927
Registered: 8-2-2015
Member Is Offline


[*] posted on 13-9-2016 at 10:19


From memory;
washing machine sized drives used huge ferrite magnets
scsi used SmCo
PC HDD used SmCo then Nd
small hdd used Nd and now NdPr

[Edited on 13-9-2016 by Sulaiman]




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User