Unknown mineral
I have found a rock a unknown mineral. I can not identify it. It was from this quarry in Maine: http://www.mindat.org/loc-6648.html. I will post more pictures.
|
|
|
Liamatpm
Harmless
Posts: 48
Registered: 7-12-2016
Location: Maine
Member Is Offline
Mood: Using the process of cellular respiration to stay (barely) alive
|
|
Another picture
Another picture
|
|
|
Liamatpm
Harmless
Posts: 48
Registered: 7-12-2016
Location: Maine
Member Is Offline
Mood: Using the process of cellular respiration to stay (barely) alive
|
|
Last picture
Last picture
|
|
|
Chlorine
Hazard to Self

Posts: 56
Registered: 26-11-2016
Location: Maine, USA
Member Is Offline
Mood: Brominated
|
|
I'm not entirely sure but It looks like red tourmaline.
|
|
|
Morgan
International Hazard
   
Posts: 1750
Registered: 28-12-2010
Member Is Offline
Mood: No Mood
|
|
Looks kind of like this.
Afghanistan
https://commons.wikimedia.org/wiki/File:Garnet-Group-Quartz-...
Maine
http://www.imgrum.net/media/1266818789329529537_2293719537
http://scontent.cdninstagram.com/t51.2885-15/s480x480/e35/13...
http://www.imgrum.net/media/1266820108538800873_2293719537
garnet = a group of minerals; see almandine, andradite, grossular, spessartine, uvarovite
http://www.maine.gov/dacf/mgs/explore/minerals/guide/chapter...
"For gem identification purposes, a pick-up response to a strong neodymium magnet separates garnet from all other natural transparent gemstones
commonly used in the jewelry trade."
https://en.wikipedia.org/wiki/Garnet
[Edited on 19-12-2016 by Morgan]
|
|
|
crystal grower
Hazard to Others
 
Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline
Mood: Puzzled
|
|
I agree with Morgan, it's most likely a garnet (pyrop or almandine I think..).
|
|
|
Liamatpm
Harmless
Posts: 48
Registered: 7-12-2016
Location: Maine
Member Is Offline
Mood: Using the process of cellular respiration to stay (barely) alive
|
|
I thought it was almandine, but I didn't know if it could be as light as my rock, thanks for the help everyone!
-Liam
|
|
|
Morgan
International Hazard
   
Posts: 1750
Registered: 28-12-2010
Member Is Offline
Mood: No Mood
|
|
Tidbits
https://www.youtube.com/watch?v=U2RZ1NLwcOQ#t=57
https://www.youtube.com/watch?v=3Ncjq0Wb2ZU
|
|
|
diddi
National Hazard
  
Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline
Mood: Fluorescent
|
|
It does have the right structure for garnet and is probably almandine rather than pyrope (which tends to have a more claret colour red) the reason
your rock is not as heavy as you expect for garnet is that it is actually granitic material with little garnets that hardly contribute to the density
of the whole specimen.
[Edited on 19-12-2016 by diddi]