Raney Nickel
I was recently looking at how to make bipy, and a procedure I found in OrgSyn calls for Raney nickel. Does anyone know of a good and easily-accessible
source for 50/50 aluminum-nickel alloy?
[Edited on 24-10-2017 by JJay]
|
|
|
CRUSTY
Hazard to Others
 
Posts: 139
Registered: 5-6-2016
Location: Nearby
Member Is Offline
Mood: High-Order
|
|
Sigma carries a 50-50 nickel-aluminum alloy that doesn't say it's a powder like other listings for the alloy on Sigma, but it may very well
just be a powder that isn't labeled as such online. Even if it were solid though, it's Sigma; you can't buy individually. I suspect you'll either have
to make the alloy yourself through melting the two together, or just buy the straight Raney nickel.
|
|
|