anhydrous calcium iodide for making calcium
What would be the best way to make calcium iodide
I have calcium chloride
Calcium hydroxide
iodine crystals
And
Sodium hydroxide
Making sodium iodide then add to calcium chloride
To acetone to form calcium iodide and insouble sodium chloride
Or decomposition of calcium iodate
It can be prepared by the direct reaction of zinc and iodine in refluxing ether or alcohol with cacium chloride
[Edited on 13-8-2018 by symboom]
|
|
Foeskes
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 156
Registered: 25-2-2017
Member Is Offline
Mood: No Mood
|
|
Well just react Ca(OH)2 and iodine to form CaI2 and Ca(IO3)2.
Dry then react it with a reducing agent i.e. Carbon.
Dissolve in water and filter.
|
|
DJF90
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2266
Registered: 15-12-2007
Location: At the bench
Member Is Offline
Mood: No Mood
|
|
Have you looked in Brauer?
|
|
symboom
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1143
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline
Mood: Doing science while it is still legal since 2010
|
|
That sound like a better path i was thinking of avoiding forming calcium iodate by reducing iodine with zinc. But i could just add carbon
The history of making calcium metal says that he used calcium iodide i have a lot of calcium chloride and a little bit of iodine there are many ways
to get to calcium iodide im also needing it to be anhydrous which makes it easier to melt it so it will react with sodium and leave behind a
crystalized mass of calcium metal.
Not sure if i really need calcium iodide
If the calcium metal melts together in one lump
According to the values below
The reaction seems to occur at 800C to 900C
Calcium metal
Melting point 842°C
Boiling point 1,484°C
Sodium metal
Melting point 97.79°C
Boiling point 882.9°C
Calcium chloride
Melting point 772°C
Boiling point 1,935°C
Calcium iodide
Melting point 779°C
boiling point 1,100°C
Thanks for the reply
[Edited on 20-8-2018 by symboom]
[Edited on 20-8-2018 by symboom]
|
|
Foeskes
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 156
Registered: 25-2-2017
Member Is Offline
Mood: No Mood
|
|
Remember to keep the temp below the boiling point of sodium otherwise you'll convert the calcium back to sodium(the reaction is reversible). By adding
carbon I mean heating the mix at a high temp(couple hundred degrees) to reduce the iodate.
I think heating the iodide will dehydrate it.
[Edited on 21-8-2018 by Foeskes]
|
|