BrF3 Reation


I have an application that require the use of Bromine Trifluoride at High Temperature High Pressure. 500 F, and 25000 PSI. The application uses a Copper part where the HTHP causes the copper to cut in half. My question is: What Kind of metal could be used that could withstand more HTHP
with BrF3. could I use something coated with ceramic or thermal insulator, or graphite?

Thank you.
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 6-1-2006 at 20:48


Why not stainless steel 316?



The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
cutter11
Harmless
*




Posts: 4
Registered: 6-1-2006
Member Is Offline

Mood: Curious

[*] posted on 9-1-2006 at 19:01
BrF3


It prohibits the use of stainless steel since the reaction that takes place prohibit the use of anything that has steel because it reacts with the chemical.
View user's profile View All Posts By User
Fleaker
International Hazard
*****




Posts: 1252
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 10-1-2006 at 18:38


I suggest inconel then, I'm fairly sure that would take it (it takes 250*C elemental bromine at 150psi).

I guess my question is, what are you using this for!?!!?
View user's profile View All Posts By User
BromicAcid
International Hazard
*****




Posts: 3231
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline

Mood: Rock n' Roll

[*] posted on 10-1-2006 at 18:54


So, copper lacks the mechanical strength, that is what bromine triflouride and the exceedingly vicous pentaflouride are produced in. How about the other metals that are famous for the confinement of the halogens, monel metal and if desperation calls, nickel?



Shamelessly plugging my attempts at writing fiction: http://www.robvincent.org
View user's profile Visit user's homepage View All Posts By User
Fleaker
International Hazard
*****




Posts: 1252
Registered: 19-6-2005
Member Is Offline

Mood: nucleophilic

[*] posted on 11-1-2006 at 16:11


Just what I suggested: inconel is a high strength copper/nickel alloy with a bit more tenacity than plain ol' monel.


Alloy Composition
Alloy: Inconel 625
Nominal Composition in Percent:
Ni
58.00
Co
1.00
Cr
21.50
Mo
9.00
Fe
5.00
Si
0.50
Mn
0.50
C
0.100
Al
0.400
Ti
0.400
P
0.015
S
0.015
Cb+Ta
3.65
View user's profile View All Posts By User
mick
Hazard to Others
***




Posts: 338
Registered: 3-10-2003
Member Is Offline

Mood: No Mood

[*] posted on 15-1-2006 at 10:56


Expensive but tantalum might work.

mick
View user's profile View All Posts By User
cutter11
Harmless
*




Posts: 4
Registered: 6-1-2006
Member Is Offline

Mood: Curious

[*] posted on 21-8-2006 at 10:54


I am sorry guys, I did not reply for a long time, But read ur replies.
I have tried Nickel by itself, it was a disaster. I am affraid that the high
percentage of nickel in inconel would cause the same problem. Can someone suggest an alloy mainly copper but have higher melting point and higher mechanical properties than copper C110 for example?

Thank you

God Bless
View user's profile View All Posts By User
ordenblitz
Hazard to Others
***




Posts: 259
Registered: 18-7-2004
Location: Northwest
Member Is Offline

Mood: Bohr'd

[*] posted on 21-8-2006 at 17:15


I'm curious how you generate the 25,000 psi.
View user's profile View All Posts By User
cutter11
Harmless
*




Posts: 4
Registered: 6-1-2006
Member Is Offline

Mood: Curious

[*] posted on 22-8-2006 at 05:59


This is a gas pressure application, through burning of solid propellant.
View user's profile View All Posts By User
tumadre
Hazard to Others
***




Posts: 172
Registered: 10-5-2005
Member Is Offline

Mood: No Mood

[*] posted on 29-8-2006 at 17:53


I'm assuming that you are using 100% Cu that is soft like copper wire

did you try using hard drawn copper, or heat the copper to about 900 C (low red color) and slowly cool in air,

I don't know that the hardness will be sustained in 500 F heat. I think it will be