Dragonjack12
Harmless
Posts: 25
Registered: 24-5-2018
Location: Northern Minnesota
Member Is Offline
Mood: Chlorine trifloride
|
|
Pbo2 solubility?
Does any one know a solvent for lead lV oxide that isn’t acetic acid?
Jack place
|
|
|
Swinfi2
Hazard to Others
 
Posts: 132
Registered: 19-2-2018
Location: England
Member Is Offline
Mood: Catalytic
|
|
I'm pretty sure PbO2 acts like a covalent network. Which is why it resists most solvents, you need to break the bonds to "dissolve" it onto another
species.
I think the easiest would be strong caustics as the plumbate ion (PbO4 -4) is a thing, but solutions of lead are obviously horribly toxic so be
careful and work out how you're going to deal with the product before you make it.
|
|
|
PyroPlatinum
Hazard to Self

Posts: 59
Registered: 21-2-2018
Member Is Offline
Mood: No Mood
|
|
Lead acetate and nitrate are soluble. But toxic tough.
|
|
|
macckone
Dispenser of practical lab wisdom
   
Posts: 2211
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
Lead(IV) Oxide is not going to dissolve easily.
That is one of the nice things about it.
It should be soluble in molten oxidizing salts but it would be unstable, converting to oxygen and lead.
There might be a deep eutectic solvent that would work but I am not aware of any.
This might be an interesting area of research.
|
|
|
phlogiston
International Hazard
   
Posts: 1383
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline
Mood: pyrophoric
|
|
Heating it will convert it to lower oxides of lead that dissolve more readily in acid.
The exact oxide depends on the temperature. Above 600 deg C, it decomposes to PbO.
PbO2 itself does dissolve in nitric acid, it just takes very long.
Probaby, if you give some more information on what you are trying to do, we can give better advice.
What is the reason you do not want to use acetic acid?
-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
|
|
|
Texium
|
Thread Moved 22-1-2019 at 15:20 |
Dragonjack12
Harmless
Posts: 25
Registered: 24-5-2018
Location: Northern Minnesota
Member Is Offline
Mood: Chlorine trifloride
|
|
Were did the thread get moved to?
I don’t want to use acetic acid because it takes a long time to make as much as I will probably need. I am trying to refurbish some old batteries by
Selectively disalving the bridged electrodes.
[Edited on 23-1-2019 by Dragonjack12]
Jack place
|
|
|