extraction of nickel from batteries
what is the best methods to extract nickel metal from batteries
the battery type is nicd and nimh
[Edited on 30-4-2019 by nikotyna1939]
|
|
CarlSagans_RayGuns
Harmless
Posts: 14
Registered: 9-4-2018
Member Is Offline
Mood: No Mood
|
|
Are you wanting nickel metal for recycling $, or are you looking for a salt like nickel chloride, nickel nickel sulfate etc. Because most of the
nickel in both of those batteries is in the form of nickel oxide hydroxide.
|
|