Jacob
Harmless
Posts: 23
Registered: 7-4-2019
Member Is Offline
|
|
Wet ether
I added 0.5g of K to 30cc of my old Et2O. It kept fizzling for 15 minutes, with an intensity between coke and effervescent tablets.
Is it done for? Should I get some new ether? Or should I dry it with a sulfate?
No UTFSE results.
|
|
DrP
National Hazard
Posts: 625
Registered: 28-9-2005
Member Is Offline
Mood: exothermic
|
|
Was your 1/2 gram K stretched into a wire or a single lump?
Reduced pressure distillation at low temp? Then leave the K wire in it over night?
\"It\'s a man\'s obligation to stick his boneration in a women\'s separation; this sort of penetration will increase the population of the younger
generation\" - Eric Cartman
|
|
vmelkon
National Hazard
Posts: 669
Registered: 25-11-2011
Location: Canada
Member Is Offline
Mood: autoerotic asphyxiation
|
|
Maybe your diethyl ether was boiling due to the heat of the reaction.
Signature ==== Is this my youtube page? https://www.youtube.com/watch?v=tA5PYtul5aU
We must attach the electrodes of knowledge to the nipples of ignorance and give a few good jolts.
Yes my evolutionary friends. We are all homos here.
|
|
zed
International Hazard
Posts: 2278
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
Yeah. K would be a final drying agent.
Wet ether that is really wet, needs preliminary drying with other agents.
Alkali metals in wet ether, develop a protective coating pretty quickly.
Use the search engine. Should be lots of entries on drying ether.
Most of us, at one time or another, have struggled with it.
http://www.sciencemadness.org/talk/viewthread.php?tid=13844
[Edited on 21-6-2019 by zed]
|
|
UC235
National Hazard
Posts: 565
Registered: 28-12-2014
Member Is Offline
Mood: No Mood
|
|
I would probably rough-dry ether with anhydrous MgSO4, then use something like powdered Na-Pb alloy to do a final drying.
|
|
draculic acid69
International Hazard
Posts: 1371
Registered: 2-8-2018
Member Is Offline
|
|
Did you check for peroxides first you know being old ether and all.might explain the fizzing
|
|
Metacelsus
International Hazard
Posts: 2534
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline
Mood: Double, double, toil and trouble
|
|
Quote: Originally posted by UC235 | I would probably rough-dry ether with anhydrous MgSO4, then use something like powdered Na-Pb alloy to do a final drying. |
I would suggest distillation from Na/benzophenone instead of Na-Pb.
OP, what are you planning to use the ether for? MgSO4 drying might be enough for some reactions.
[Edited on 2019-6-22 by Metacelsus]
|
|
fusso
International Hazard
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Why is benzophenone used?
|
|
BromicAcid
International Hazard
Posts: 3231
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
It's reduced with potassium to the diphenylketyl anion. Thisl is soluble in ether. This lets the drying agent go into solution so it's homogenous
drying instead of heterogenous drying which is less effective/takes more time.
[Edited on 6/22/2019 by BromicAcid]
|
|
Mabus
Wiki Master
Posts: 238
Registered: 3-11-2013
Member Is Offline
Mood: Energetic
|
|
Jacob, did you ether changed color after the reaction?
I had a similar issue a while ago with some ether from car starting fluid. Turns out, the said ether had lots of acetaldehyde, which came from the
manufacturing process.
|
|
Sturge11
Harmless
Posts: 9
Registered: 4-9-2019
Member Is Offline
|
|
Saw someone suggest dry epsom salts, aka dehydrated MgSO4. I would attempt this first.
|
|
Amos
International Hazard
Posts: 1406
Registered: 25-3-2014
Location: Yes
Member Is Offline
Mood: No
|
|
Always use your least expensive drying agent first if you have no idea what the moisture content is. I'd let a small volume like that sit over an
anhydrous salt overnight then go with sieves or alkali metal. Bigger volumes I just reflux under a soxhlet full of sieves a few times.
|
|
Jacob
Harmless
Posts: 23
Registered: 7-4-2019
Member Is Offline
|
|
Thanks all! I reacted it with sodium and dried it with NaOH then distilled. As good as new. The idiots that used it before me confessed that it might
contain acetone.
|
|