Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: H2so4 from Cuso4
Tiamat
Harmless
*




Posts: 5
Registered: 17-3-2006
Member Is Offline

Mood: No Mood

[*] posted on 17-3-2006 at 18:25
H2so4 from Cuso4


Anyone has a good recipe? with electrolysis i mean
View user's profile View All Posts By User
Tiamat
Harmless
*




Posts: 5
Registered: 17-3-2006
Member Is Offline

Mood: No Mood

[*] posted on 17-3-2006 at 18:26


recipes pls
View user's profile View All Posts By User
HNO3
Hazard to Others
***




Posts: 211
Registered: 10-11-2004
Location: America
Member Is Offline

Mood: No Mood

[*] posted on 17-3-2006 at 18:58


Search, you!



\"In the beginning, God...\" Wait a minute, God doesn\'t exist!!!!!!!!!! \"OK, in the beginning, ummm, hydrogen...\" Wait a minute, what about the laws of thermodynamics? \"OK, in the beginning, ummm.....UMMMMM, what\'s left to choose from?
View user's profile View All Posts By User This user has MSN Messenger
solo
International Hazard
*****




Posts: 3975
Registered: 9-12-2002
Location: Estados Unidos de La Republica Mexicana
Member Is Offline

Mood: ....getting old and drowning in a sea of knowledge

[*] posted on 17-3-2006 at 19:30


Try google and also why do you double post....think you'll get more help that way?.....wrong, so delete one of your posts as it doesn't help and do some foot work yourself then post what you know and still can't understand then you will get some help..........solo



It's better to die on your feet, than live on your knees....Emiliano Zapata.
View user's profile View All Posts By User
enima
Hazard to Self
**




Posts: 98
Registered: 1-12-2004
Member Is Offline

Mood: No Mood

[*] posted on 17-3-2006 at 19:46


Recipe? http://www.bbc.co.uk/food/recipes/

[Edited on 18-3-2006 by enima]
View user's profile View All Posts By User
praseodym
Hazard to Others
***




Posts: 137
Registered: 25-7-2005
Location: Schwarzschild Radius
Member Is Offline

Mood: crazy

[*] posted on 18-3-2006 at 01:39


I sense sarcasm...
View user's profile View All Posts By User This user has MSN Messenger
rot
Hazard to Self
**




Posts: 62
Registered: 26-1-2006
Member Is Offline

Mood: No Mood

[*] posted on 18-3-2006 at 10:39


this is not possible, sulfuric acid is the only acid that can not be displaced from its salts,
becouse in other situations (e.g. Sodium Chloride and Sulfuric acid yields hydrochloric acid). the acid produced has to be less strong than the acid used to displace it from the salt with. sulfuric acid is stronger than hydrochloric, so this works. becouse there is no acid stronger than sulfuric it won't work.
View user's profile View All Posts By User
neutrino
International Hazard
*****




Posts: 1583
Registered: 20-8-2004
Location: USA
Member Is Offline

Mood: oscillating

[*] posted on 18-3-2006 at 10:40


There was a thread on this over at roguesci.org. As I remember, they got some sulfuric acid by electrolysis of CuSO<sub>4</sub>, but not much.



View user's profile View All Posts By User
Odyssèus
Hazard to Self
**




Posts: 50
Registered: 7-3-2006
Member Is Offline

Mood: No Mood

[*] posted on 18-3-2006 at 11:36


Isnt there a thread around here somewhere on electrolysis from MgSO4?
View user's profile View All Posts By User
hinz
Hazard to Others
***




Posts: 201
Registered: 29-10-2004
Member Is Offline

Mood: No Mood

[*] posted on 18-3-2006 at 11:50


Quote:
Originally posted by rot
this is not possible, sulfuric acid is the only acid that can not be displaced from its salts,
becouse in other situations (e.g. Sodium Chloride and Sulfuric acid yields hydrochloric acid). the acid produced has to be less strong than the acid used to displace it from the salt with. sulfuric acid is stronger than hydrochloric, so this works. becouse there is no acid stronger than sulfuric it won't work.


This isn't the whole reality. As far as I know HCl(pKs-6) is a stronger acid than H2SO4 (pKs-3). The thing is that you need an acid with an higher boiling point than the acid you'll liberate. HCl is very volatile so it will leave the reaction system because the concentrated sulfuric acid you use will capture all water. It's also possible to liberate HCl with AHSO4 (A=>alkali metall) which is a weak acid.

On the other hand it won't be possible to liberate phosphoric acid(weaker acid then HCl) from phosphate with HCl because your gaseous HCl will leave your condensor far before the H3PO4 will do.
View user's profile View All Posts By User
The_Davster
A pnictogen
*******




Posts: 2861
Registered: 18-11-2003
Member Is Offline

Mood: .

[*] posted on 18-3-2006 at 11:56


sulfuric from MgSO4: https://sciencemadness.org/talk/viewthread.php?tid=1739#pid1...
sulfuric from CuSO4: http://www.sciencemadness.org/talk/viewthread.php?tid=1186




View user's profile View All Posts By User