[*] posted on 3-4-2020 at 10:01
Cuting cerium metal


Hi.

I have small piece of cerium metal (3g). I read that cerium is soft metal which can be cut by knife. But this isn't truth. I tried it and it didn't work.

I want to try cut few small pieces of cerium and dissolve them in different acids.

Have you any experiences or ideas how cut it?
View user's profile View All Posts By User
Heavy Walter
Hazard to Others
***




Posts: 127
Registered: 17-12-2015
Location: Argentina
Member Is Offline

Mood: No Mood

[*] posted on 3-4-2020 at 11:12


Hi
In Mohs´s scale is 2.5 so it is not too hard.
Depening on the shape you can use a cutting plier.
View user's profile View All Posts By User
Herr Haber
International Hazard
*****




Posts: 1236
Registered: 29-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 3-4-2020 at 13:51


Or just a file ?



The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6487
Registered: 4-10-2014
Location: Limbo
Member Is Offline

Mood: Just got through yet another "take this job and shove it" moment.

[*] posted on 3-4-2020 at 16:17


If you use an angle grinder, prepare for sparks.
I have a 1.1kg ingot. I am not planning on cutting it at all. When I get into Ce chemistry it will likely be via CeO2 or purpose bought pellets.
View user's profile View All Posts By User
diddi
National Hazard
****




Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline

Mood: Fluorescent

[*] posted on 3-4-2020 at 17:32


i made a tool from an 8.8 HT bolt which i use as a chisel in a press for cutting (shearing) metals. no sparks and good control. angle grinder blades get shredded by many metals and there is a lot of wastage esp if the sample is small



Beginning construction of periodic table display
View user's profile View All Posts By User
Herr Haber
International Hazard
*****




Posts: 1236
Registered: 29-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 4-4-2020 at 12:37


If it's only 3 grams you could also just fold a paper around it and hammer it a few times.

Somewhere around I have several blocks of Cerium mixed with a bunch of other lanthanides. I bought them from a pyro store but they were all little pyramids at some point. The base was irregular as if it had been broken off a mold or probably sintered.
I remember researching what were their original purpose (never heard of Cerium in pyro unless you count the lighter!) could have been. They are probably used in foundry to add trace lanthanides in some exotic alloys.

Anyway, the last time I found them I made a mess of oxides. I shouldnt have left them in their plastic bag...

@jsum1 The angle grinder could be fun but I thought I could find myself a very tall bridge or tower, heat one of my blocks with a blowtorch and drop it :)




The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6487
Registered: 4-10-2014
Location: Limbo
Member Is Offline

Mood: Just got through yet another "take this job and shove it" moment.

[*] posted on 4-4-2020 at 14:44


I was not serious about using an angle grinder. But it would be spectacular.
If I was to cit the piece I have, I would probably use a hacksaw and collect the filings for making a cerium salt.
View user's profile View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1253
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 4-4-2020 at 15:52


Thanks for suggestions.

Cutting plier is good choice. I tried it today and it's good for cutting small pieces of metal, which is good for test tube scale reactions.