nikotyna1919
Harmless
Posts: 10
Registered: 10-9-2019
Location: reverse poland flag or nusantara
Member Is Offline
|
|
non noble corrosion resistant metal and alloys for storing or reacting corrosive chemicals
what kinds of non noble metals and alloys is corrosion resistant for storing or reacting halogens,corrosive gases mineral acids and salts in any
concentration at room temperature like hydrogen chloride gas, nitrogen dioxide gas, sulfur trioxide gas, hydrobromic acid, hydrochloric acid,
hydroiodic acid, nitric acid, sulfuric acid, phosphoric acid, ammonium chloride, copper chloride, ferrous chloride, stannous chloride
[Edited on 21-6-2020 by nikotyna1919]
[Edited on 21-6-2020 by nikotyna1919]
|
|
nikotyna1919
Harmless
Posts: 10
Registered: 10-9-2019
Location: reverse poland flag or nusantara
Member Is Offline
|
|
are alloys more corrosion resistant than pure metals
i want to know which is better alloy or pure metals in corrosive environments
|
|
j_sum1
Administrator
Posts: 6238
Registered: 4-10-2014
Location: Unmoved
Member Is Online
Mood: Organised
|
|
Depends. Both on the specifics of the metal and also the environment where corrosion is occurring.
Stainless steel is obviously an alloy of steel and manufactured to prevent corrosion. But in a salty water environment, some grades of SS will
actually corrode worse than mild steel: often because they corrode via a different mechanism.
Concentrated sulfuric acid is routinely transported by rail in large vessels of low alloy steel. You might anticipate a very corrosive environment
but the rate is slow and predictable. But many steel alloys would not hold up as well.
Aluminium and aluminium alloys resist corrosion well. But that is due to the protective surface oxide coating that develops on Al. If you have an
alloy that alters the interatomic spacing sufficiently such that the oxide does not adhere as well then you will have something that corrodes rapidly.
Likewise if you have Hg or Ga present then this weakens the metal by diffusing through the grain boundaries as well as into the bulk metal.
Technically, an alloy is formed and it has inferior structural properties to the original metal. Including the fact that it is subject to rapid
oxidation along the now-exposed grain boundaries.
So... depends on context. What metal? What alloy? What environment?
|
|
cyanureeves
National Hazard
Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
brass is more resistant than tin probably but i doubt it beats copper.
|
|
j_sum1
Administrator
Posts: 6238
Registered: 4-10-2014
Location: Unmoved
Member Is Online
Mood: Organised
|
|
Brass is more resistant than zinc. I don't think tin is a valid comparison.
And, in all honesty, it would not surprise me if brass excelled copper in normal outdoor environments. Compare a brass tap with copper sheet roof...
The latter can become quite green.
But I think bronze probably weathers better than copper: hence its use in statues.
|
|
mackolol
Hazard to Others
Posts: 458
Registered: 26-10-2017
Member Is Offline
Mood: Funky
|
|
Chromium is very resistant. All chemical resistant alloys consist of chromium, but I don't know exactly which one of mentioned by you chemicals can be
stored in such containers.
|
|
Texium
|
Threads Merged 21-6-2020 at 06:18 |
Texium
|