[*] posted on 29-6-2021 at 12:15


Quote: Originally posted by BauArf56  
Once i wanted to see how does propane (or butane) burn in chlorine gas, so i lighted up the blowtorch inside a bottle filled with chlorine. It burned with a bigger flame and it was quite luminous too. After a few seconds of burning inside the bottle there was no smell of chlorine at all, just the typical sweet smell of chlorinated compounds. Can anyone explain which compounds form and if is it possible to isolate them as liquids? Thanks


A wide variety of chlorinated compounds will form. Industrially, chlorinations are done in such a way as to avoid long chain hydrocarbons at high temperatures and high chlorine concentrations. Generally the amount of chlorine is regulated to give a mono, di or tri substituted base. Separating the compounds requires a lot of work unless it is something simple like methyl chloride, methylene chloride, chloroform and carbon tetrachloride.
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3942
Registered: 8-2-2015
Member Is Offline


[*] posted on 3-7-2021 at 06:29
KOH or CaCl2 to dry KI?


I want to dry 20g of KI to weigh it for redox titrations, I intend to use a jam jar as a dessicator

IMG_20210703_220859.jpg - 1.6MB
(disposable lighter for scale reference only)

which would be 'best', CaCl2 or KOH?

I guess that the long narrow neck of the bottle will slow down the dehydration,
but I'm not in a hurry.




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3942
Registered: 8-2-2015
Member Is Offline


[*] posted on 4-7-2021 at 18:32


Answered my own question...I have 3A molecular sieves.
IMG_20210705_102821.jpg - 1.6MB




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1794
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 8-7-2021 at 11:00


Is there any interesting to do with ammonium dihydrogen phosphate from fire extinguishers? I have at least 5kg of the stuff, but it's pretty messy to work with. I don't know if it's treated with anything hydrophobic but it doesn't really mix with water.



We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
BauArf56
Hazard to Self
**




Posts: 68
Registered: 22-8-2019
Location: between the moon and the sun
Member Is Offline

Mood: energetic

[*] posted on 9-8-2021 at 02:42


3 stupid questions:
1. How to make calcium nitrate from potassium nitrate? I tried mixing KNO3 and CaCl2 but i don't really know if it worked and if i can separate it from potassium chloride.
2. How to make ammonium nitrate from KNO3?
3. i distilled a mix of sodium bisulfate and potassium nitrate (40g of NaHSO4 and 20g of KNO3, as NurdRage says) and got a few drops of yellow nitric acid, plus lots of nitrogen dioxide. Strange thing is that it fumed when i blown over it, so could it be the super concentrated stuff? And why a such low yield?
View user's profile View All Posts By User
Keras
International Hazard
*****




Posts: 1143
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 9-8-2021 at 03:56


I would turn KNO₃ into pure nitric acid (you can do that with NaHSO₄, as demonstrated by Nurd Rage's video), and then you neutralise your acid with either calcium carbonate (lime stone) or ammonia, case 1. and 2. I'm pretty sure you can't get Ca(NO₃)₂ from KOH – though that might work to some extent [this is linked to the relative alkalinity of KOH and Ca(OH)₂]. However, NH₃ being a weak base, there's no way to turn KNO₃ into NH₄NO₃.

3. Pay attention to stoichiometry. Nurdrage uses 43 g of KNO₃ and 150 g of NaHSO₄. If you use 20 g of potassium nitrate, you would have to use 80 g of sodium bisulphate to place yourself in the same conditions and get the same yield.
View user's profile View All Posts By User
karolus28
Hazard to Self
**




Posts: 51
Registered: 14-4-2019
Location: EU's Brazil
Member Is Offline

Mood: zgrzyt

[*] posted on 31-8-2021 at 08:09


A question related to the legendary lead chamber processe:
Let me start by saying that I did the lead chamber process but it was kinda shit, 20-25 burning cycles, about 300 ml of water at the bottom, small burning pot on a 250 beaker, the bottom of the beaker would get some nitrosylsulfuric acid after a few burns. I didn't actually do much stoichiometry because I didn't have a good scale and that might explain why it was dilute as shit even after boiling to 20 ml, although it worked since I previouslu used a copper stand and the solution got a bit of blue. Now bact to the problem -the sulfur and KNO3 wouldn't react- both were bought as reagents, mixed together, no matter how much heat would I put into it, the sulfur just burned for a while and then went off leaving clumped/molten KNO3 on the top. I realized that I can use a tiny tiny amount of sugar to make the magic happen, so the plan was to put some KNO3 in the pot(45 degree angle), and then on top put a mixture of sulfur, little bit of sugar, little bit of KNO3 and on top of that put pure sulfur that gives me time to close the bucket before the violent reaction starts that lasts like 10-15 seconds.

The actual question is, how do I make the mix burn like it is in theory mean to burn?
In this video the NO2 fumes are clearly visible: https://youtu.be/7XVt_ca97WE?t=305

This is how I usually ignited all that https://www.youtube.com/watch?v=KwYA7ojSodc


Good God why do I talk so much?
View user's profile View All Posts By User
TheMrbunGee
Hazard to Others
***




Posts: 364
Registered: 13-7-2016
Location: EU
Member Is Offline

Mood: Phosphorising

[*] posted on 31-8-2021 at 11:50


Quote: Originally posted by karolus28  
A question related to the legendary lead chamber processe:
Let me start by saying that I did the lead chamber process but it was kinda shit, 20-25 burning cycles, about 300 ml of water at the bottom, small burning pot on a 250 beaker, the bottom of the beaker would get some nitrosylsulfuric acid after a few burns. I didn't actually do much stoichiometry because I didn't have a good scale and that might explain why it was dilute as shit even after boiling to 20 ml, although it worked since I previouslu used a copper stand and the solution got a bit of blue. Now bact to the problem -the sulfur and KNO3 wouldn't react- both were bought as reagents, mixed together, no matter how much heat would I put into it, the sulfur just burned for a while and then went off leaving clumped/molten KNO3 on the top. I realized that I can use a tiny tiny amount of sugar to make the magic happen, so the plan was to put some KNO3 in the pot(45 degree angle), and then on top put a mixture of sulfur, little bit of sugar, little bit of KNO3 and on top of that put pure sulfur that gives me time to close the bucket before the violent reaction starts that lasts like 10-15 seconds.

The actual question is, how do I make the mix burn like it is in theory mean to burn?
In this video the NO2 fumes are clearly visible: https://youtu.be/7XVt_ca97WE?t=305

This is how I usually ignited all that https://www.youtube.com/watch?v=KwYA7ojSodc


Good God why do I talk so much?


I am unfamiliar with this process, but I have played with KNO3/S pyrotechnic mix, and know they do react. As I understand there is not a lot of KNO3 in that mixture, that is why reaction is not energetic at all.

I would recommend grinding KNO3 (and sulfur) as fine as You can or even use water to mix it with S, making a paste and actively drying it making homogenous mix of molecules, that might help it burning completely. I guess sulfur boiling point is lower than decomposition of KNO3, so it never does. (too lazy to check)




View user's profile Visit user's homepage View All Posts By User
karolus28
Hazard to Self
**




Posts: 51
Registered: 14-4-2019
Location: EU's Brazil
Member Is Offline

Mood: zgrzyt

[*] posted on 31-8-2021 at 12:25


Well, I tried mixing the sublimed sulfur with somewhat powdery KNO3 1:1, blasted it with a mini blowtorch and nothing really happened. If you put a pinch of sugar it burns like rcandy with very bright light. I might try doing this again



Hi, please read about exif data.
View user's profile View All Posts By User
TheMrbunGee
Hazard to Others
***




Posts: 364
Registered: 13-7-2016
Location: EU
Member Is Offline

Mood: Phosphorising

[*] posted on 31-8-2021 at 12:46


Quote: Originally posted by karolus28  
Well, I tried mixing the sublimed sulfur with somewhat powdery KNO3 1:1, blasted it with a mini blowtorch and nothing really happened. If you put a pinch of sugar it burns like rcandy with very bright light. I might try doing this again



I think You need about 1 part of S for 4 parts of KNO3, try that mixture. Otherwise molten sulfur just extinguishes reaction like water would.

Edit: The sulfur melts first, so fineness of it does not matter as much as fineness of KNO3. Only bet to get this working with Your proportions is to get KNO3 as fine as possible, If its doable at all.

[Edited on 31-8-2021 by TheMrbunGee]




View user's profile Visit user's homepage View All Posts By User
karolus28
Hazard to Self
**




Posts: 51
Registered: 14-4-2019
Location: EU's Brazil
Member Is Offline

Mood: zgrzyt

[*] posted on 1-9-2021 at 12:30


Tried 1:4 today, worked. The only difference was that I had the mixture on Al foil with a lighter underneath. It's just that lighting it from the top doesn't work.

thanks




Hi, please read about exif data.
View user's profile View All Posts By User
karlos³
International Hazard
*****




Posts: 1520
Registered: 10-1-2011
Location: yes!
Member Is Offline

Mood: oxazolidinic 8)

[*] posted on 1-9-2021 at 16:44


Ok so I want to follow this theobromine extraction procedure: https://biochemicalponderings.wordpress.com/2017/03/18/theob...

Even made magnesium hydroxide just for this process, but that crappy substance is so hard to filter out :(

My short question would be, can I replace the magnesium hydroxide simply with sodium hydroxide, it is used to form insoluble tannate salts, would NaOH be a suitable substitute for this?




verrückt und wissenschaftlich
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4504
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 1-9-2021 at 17:21


Sodium hydroxide should be okay, but calcium carbonate should also work (that's the base of choice in the caffeine extraction I have notes for), and is less harsh.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
karlos³
International Hazard
*****




Posts: 1520
Registered: 10-1-2011
Location: yes!
Member Is Offline

Mood: oxazolidinic 8)

[*] posted on 1-9-2021 at 17:38


Thank you! :)

I just can't get the Mg(OH)2 I made out of the aqueous suspension it is in, so I guess I'll stick with NaOH.
If it turns out this was not an as well working alternative, then I guess I can still fix any issues resulting from that later, shouldn't be that bad.




verrückt und wissenschaftlich
View user's profile View All Posts By User
UC235
National Hazard
****




Posts: 565
Registered: 28-12-2014
Member Is Offline

Mood: No Mood

[*] posted on 1-9-2021 at 18:25


How about buying some food grade lime? Calcium hydroxide. That will be a lot closer than NaOH.
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4504
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 1-9-2021 at 18:28


You can't get magnesium hydroxide as an antacid where you live? Unflavoured antacid tablets should work just fine for this prep.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
karlos³
International Hazard
*****




Posts: 1520
Registered: 10-1-2011
Location: yes!
Member Is Offline

Mood: oxazolidinic 8)

[*] posted on 1-9-2021 at 21:11


Well I have around 800ml of selfmade "milk of magnesia" now, it just clogs up everything.
I actually took the required amount of MgSO4 7H20, dissolved this in water and added the respective amount of NaOH to precipitate the Mg(OH)2, its just that this annoying fine precipitate is a bit like cement when fresh prepared, or such...

Guess I could try it through a piece of cloth instead, that might work better.
I mean, its the exact quantity and substance I need, even if I can't filter it through the frit, I should still try to filter it out somehow.




verrückt und wissenschaftlich
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6472
Registered: 4-10-2014
Location: Limbo
Member Is Offline

Mood: Just got through yet another "take this job and shove it" moment.

[*] posted on 3-11-2021 at 05:34


Interesting shade of blue encountered while recycling some barium. I wonder if anyone can help me identify it.

IMG20211103213548.jpg - 2.6MB

I did the classic Ba(OH)2 + NH4Cl endothermic reaction and decided to convert the product back to hydroxide.

I first made sure that Ba(OH)2 was in excess. And it was left for a few days so that most of the ammonia had a chance to escape.
I then added water and HCl to dissolve the solid. I thought to convert everything to BaCl2, but there did remain some cloudiness.
I then added a concentrated solution of NaOH to precipitate the Ba as hydroxide. That is when the blue appeared. I thought it was Raleigh scattering at first, but it persisted even when the mixture became fully opaque and also afterwards when the sediment began to settle. There was an ammonia smell indicating that ammonium salts were still present.
It seems that I have two crops of crystals: a fine powder that settled immediately and some larger fluffy ones that crystallised later.
But I am not sure about the blue or what might be causing it.

Thoughts?
View user's profile View All Posts By User
S.C. Wack
bibliomaster
*****




Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline

Mood: Enhanced

[*] posted on 3-11-2021 at 14:58


Perhaps it's something complexed to the ammonia. I'd do things with the filtrate and see what happens.

BTW it takes little excess acid to precipitate the chloride, so the purity of your precipitate is unclear.




"You're going to be all right, kid...Everything's under control." Yossarian, to Snowden
View user's profile Visit user's homepage View All Posts By User
j_sum1
Administrator
********




Posts: 6472
Registered: 4-10-2014
Location: Limbo
Member Is Offline

Mood: Just got through yet another "take this job and shove it" moment.

[*] posted on 4-11-2021 at 01:47


That's much the same conclusion I came to. But I eould not expect Ba to form such a complex. Which leaves impurities. And who knows quite what thry might be.
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4504
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 4-11-2021 at 06:48


Agreed. Ammonia isn't going to complex to barium, and it's tough to imagine a barium compound that's going to be blue because of the barium.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
S.C. Wack
bibliomaster
*****




Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline

Mood: Enhanced

[*] posted on 4-11-2021 at 14:07


The involvement of Ba or not is of course easily decided by removing it. Same for ammonia. After that, changing the oxidation state may help.



"You're going to be all right, kid...Everything's under control." Yossarian, to Snowden
View user's profile Visit user's homepage View All Posts By User
j_sum1
Administrator
********




Posts: 6472
Registered: 4-10-2014
Location: Limbo
Member Is Offline

Mood: Just got through yet another "take this job and shove it" moment.

[*] posted on 4-11-2021 at 16:05


Contamination may have come via the acid. I buy hardware store HCl and I have had issues in the past with titanium contamination of all things. I normally distil out azeotropic HCl for everyday use. However, it is possible that some diluted undistilled acid made its way into the mix.
I have played with Ti complexes before. I do not recall a blue ammonia complex. So that is puzzling to me.

I will test the supernatant liquid and see if I can drtect either ammonia or titanium.

Another possible contaminant is iron. Where I live is a large amount of red dust that is predominantly Fe2O3 snd it gets everywhere. But, again, a blue complex has me stumped.

The NH4Cl is analytical grade. The Ba(OH)2 is old stock of unknown assay rescued from a throw out pile. I fully expect it contains carbonate after probably 30 years of storage, but that should change little.

I have a second batch that I will process the same way but a little more carefully and see if I get the same result. I may as well get some benegit from a failed video.
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1751
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 4-11-2021 at 17:11
Black quartz


What might the black color be from?
https://www.heraeus.com/en/hca/products_hca/hbq_black_quartz...
View user's profile View All Posts By User
walruslover69
Hazard to Others
***




Posts: 243
Registered: 21-12-2017
Member Is Offline

Mood: No Mood

[*] posted on 4-11-2021 at 22:09


probably either magnetite which is what makes obsidian black, or carbon powder. can't be certain though