RadiumQuetzal
Harmless
*




Posts: 4
Registered: 19-3-2019
Member Is Offline


[*] posted on 13-8-2020 at 14:11
Making Glowing Radium Paint


Hi

I have tried to make radium paint that glows like it used to for quite some time now with decent success. While it does generate some luminescence it is too faint for my liking so I wonder, does anyone know a good method to make paint that glows quite well?

My method

1. Mixed new ZnS:Cu with acetone to remove any kind if adhesive that might cause it to glow less. (Seems to make it work a bit better even tho the ZnS:Cu is brand new)

2. Dissolved around 0.5ug of RaBr2 and mixed it in with the ZnS:Cu

3. Mixed it around over and over again until all the water had dried.

I of course left it in a dark space for 24h before checking if there were any luminescence from the paint. (checked in total darkness during a span of 10min)

Left pic is a measurement of the paint. Detector used is an Eberline ASP-1 with a Ludlum 44-9 probe. Right pic is the paint.

IMG_20200814_000643.jpg - 2MB IMG_20200814_000521.jpg - 1.8MB

[Edited on 13-8-2020 by RadiumQuetzal]
View user's profile View All Posts By User
Cezium
Harmless
*




Posts: 41
Registered: 5-1-2015
Member Is Offline

Mood: No Mood

[*] posted on 17-8-2020 at 01:16


No sure if 10kBq of Ra is enough to glow... Maybe with some really good phosphor.
View user's profile View All Posts By User
RadiumQuetzal
Harmless
*




Posts: 4
Registered: 19-3-2019
Member Is Offline


[*] posted on 17-8-2020 at 13:51


I thought so too but then I realized that some of the clocks with radium contains even less and still used to glow. One of those containing a total of 0.0259ug of Ra-226 and the paint should be ZnS:Cu due to it's age.
View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 17-8-2020 at 17:39


maybe the particle size is smaller? with bigger particles of ZnS only the outside is in contact with the radium salt, i don't know how much the radiation would penetrate inside the particle, or if that internal glow would even be visible to our eye, but in general the finer and more intimate the mixture the better should be the result.




---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
RadiumQuetzal
Harmless
*




Posts: 4
Registered: 19-3-2019
Member Is Offline


[*] posted on 18-8-2020 at 02:20


Hmmm dont think that the particle size should be an issue. The ZnS:Cu I used should be the same type used in clocks. It was sold as clock/watch paint and it seems like really fine powder.
View user's profile View All Posts By User
Cezium
Harmless
*




Posts: 41
Registered: 5-1-2015
Member Is Offline

Mood: No Mood

[*] posted on 30-8-2020 at 13:15


Maybe try with UV light if it even glows at all, ZnS:Cu is quite sensitive to contaminants.
View user's profile View All Posts By User
RadiumQuetzal
Harmless
*




Posts: 4
Registered: 19-3-2019
Member Is Offline


[*] posted on 31-8-2020 at 11:07


It does glow and I have gotten it to glow on it's own to some extent mixing with radium. The luminescence is just too low.

I have a new idea which I'm currently testing.
Clean the paint using chloroform or acetone.
Dissolve the old ZnS in hcl where it is then dried leaving radium and zink chloride.
Then add acetone and the new ZnS, mixing as often as possible.
View user's profile View All Posts By User
FragranceLover89
Hazard to Self
**




Posts: 72
Registered: 13-8-2019
Member Is Offline


[*] posted on 31-10-2020 at 17:16


Have you tried strontium aluminate instead of ZnS?
View user's profile View All Posts By User
p4rtridg3
Harmless
*




Posts: 24
Registered: 28-1-2020
Location: Eastern United States
Member Is Offline


[*] posted on 5-11-2020 at 17:39


AFAIK an important part of the manufacture of Radium dials was getting the ZnS crystal size and shape right. They had some specialized processes for it, but I don't know any details.

Maybe try with one of those kits that supposedly restores the glow in radium watch hands. They can be found on eBay. I believe most just contained the specially made ZnS that could be reapplied after the alpha radiation damaged the original phosphor too much.
View user's profile View All Posts By User
Crazy_Chemist
Harmless
*




Posts: 19
Registered: 22-7-2019
Location: Europe
Member Is Offline

Mood: Radioactive

[*] posted on 9-3-2022 at 07:21


Hi!

I've thougt to do the same, I have bougt some radiumpainted watch-hands om eBay, and I want to solve the radium in some milliliter, but which solvent should I use? Is it more efficient to scrape off the radium from the clock hand? Or maybe it can be dangerous? I know about the radium girls.

Then I want to add a suitable substance so that will shines again and had thought zinc sulphide, or is there something more effective? And how much is it on a clock hand, but of course it depends on the size. Somewhere I read 1 µg, is that correct? It shows about 60,000 Bq on a hand.

Thanks for all the tips!

And I wonder what salt it is in the paint? RaSO4 is said to be completely insoluble in water.
View user's profile View All Posts By User
Crazy_Chemist
Harmless
*




Posts: 19
Registered: 22-7-2019
Location: Europe
Member Is Offline

Mood: Radioactive

[*] posted on 12-3-2022 at 23:34


I ordered two types of zinc sulfide yesterday:
Zinc sulfide: Copper doped https://onyxmet.com/index.php?route=product/product&prod...
Zinc sulfide: Silver doped https://onyxmet.com/index.php?route=product/product&prod...

I expect that the copper doped gives a more green light, and the silver doped a more blue light? So lets say I want do make both. I also bought this...



So how to easy scrape of the radium from all the hands and solve it, maybe wash it too. I don't want to spill aroud the radium or get it in me, so I will make it in a sealed workspace. The average clock hand contains about 1 µg radium, so I maybe get 50 µg radium.

Then, what solve it in? Maybe it's not had to be solved? Maybe it's enough to mix it up? Then I split it in to two miniature cans, one green and one blue. How much ZnS do I need in each can to get efficient exchange?




Amateur chemist, just for fun!
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 13-3-2022 at 03:52


I'm pretty sure that ZnS isn't stable in air and will oxidise to ZnSO4 (with accompanying hydrolysis, and carbonate formation etc).

Even if that's only a surface effect you will still have a problem because the alphas don't penetrate far.

View user's profile View All Posts By User
Crazy_Chemist
Harmless
*




Posts: 19
Registered: 22-7-2019
Location: Europe
Member Is Offline

Mood: Radioactive

[*] posted on 11-4-2022 at 01:47


But how should I solve the zinc sulfide, so I can paint it om the clock hands? It's insolutable in water...



Amateur chemist, just for fun!
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 11-4-2022 at 01:50


You don't dissolve it.
You make a suspension of it.
View user's profile View All Posts By User
JGHFunRun
Harmless
*




Posts: 5
Registered: 11-7-2022
Location: [REDACTED]
Member Is Offline

Mood: V and Y are the best letters

[*] posted on 12-9-2022 at 19:56


Yea I don't work with radiation but most paints exist as suspensions. Prussian blue is insoluble in basically everything but it's easy to make a colloidal form that you can then use with whatever your favorite paint base is. If you don't know how to do that you can look into mixing paint, it's something a lot of artists do when they really want to make the paint their own so there's a decent chunk of information on it

[Edited on 13-9-2022 by JGHFunRun]
View user's profile Visit user's homepage View All Posts By User
JGHFunRun
Harmless
*




Posts: 5
Registered: 11-7-2022
Location: [REDACTED]
Member Is Offline

Mood: V and Y are the best letters

[*] posted on 14-9-2022 at 12:26


Oh and also I hope you know what you're doing, the Styopyro Discord server has had many incidents where people going in the reverse direction (radium from watches) end up having to be decontaminated by the feds. Currently the #science-general chat is discussing the aftermath of someone doing exactly that

[Edited on 14-9-2022 by JGHFunRun]




HeH⁺ HeH⁺ HeH⁺ HeH⁺
View user's profile Visit user's homepage View All Posts By User
WyattDaHooman
Harmless
*




Posts: 5
Registered: 25-8-2025
Member Is Offline

Mood: No Mood

[*] posted on 29-8-2025 at 16:15


How'd you get the radium?
View user's profile View All Posts By User
Radiums Lab
Hazard to Others
***




Posts: 303
Registered: 18-3-2025
Location: India
Member Is Offline

Mood: Experiencing the elegance of science.

[*] posted on 30-8-2025 at 11:10


Quote: Originally posted by WyattDaHooman  
How'd you get the radium?

Yea same question here too.




Water is dangerous if you don't know how to handle it, elemental fluorine (F₂) on the other hand is pretty tame if you know what you are doing.
Check out my youtube channel here:
https://www.youtube.com/@RadiumsLab
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2923
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: Mildly disgruntled scientist

[*] posted on 15-12-2025 at 17:02


Just check out Amazon.Ir or Ebay.Ir. They have all kinds of nuclear items...