Author: Subject: Removing superglue from table
coyote
Harmless
*




Posts: 16
Registered: 5-1-2017
Member Is Offline

Mood: No Mood

[*] posted on 9-5-2022 at 12:46
Removing superglue from table


How would I go about removing spilled superglue from a table? my chem teacher is mad at me.
View user's profile View All Posts By User
Tsjerk
International Hazard
*****




Posts: 3040
Registered: 20-4-2005
Location: Netherlands
Member Is Offline

Mood: Mood

[*] posted on 9-5-2022 at 13:30


You could use a sander or an angle grinder.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 9-5-2022 at 13:34


It depends what the table is made of. Superglue is soluble (or at least,. softened by) acetone.
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6465
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 9-5-2022 at 13:51


Acetone is the go-to here.
If the lab bench cannot handle acetone without disintegrating, you got other problems.
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2905
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: Mildly disgruntled scientist

[*] posted on 9-5-2022 at 16:10


If you soften it with acetone, it will scrap off easily with a razor knife.
View user's profile View All Posts By User
coyote
Harmless
*




Posts: 16
Registered: 5-1-2017
Member Is Offline

Mood: No Mood

smile.gif posted on 10-5-2022 at 07:28


I used some isopropanol and scraped it off with a coin, took like 10 mins but it worked
View user's profile View All Posts By User
Herr Haber
International Hazard
*****




Posts: 1236
Registered: 29-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 10-5-2022 at 15:29


I'd have gone for nitromethane. It's the main component in superglue remover products.
Maybe not in everyone's inventory though.

Ah, there's a thread about it:
http://www.sciencemadness.org/talk/viewthread.php?tid=87866




The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
View user's profile View All Posts By User
SWIM
National Hazard
****




Posts: 970
Registered: 3-9-2017
Member Is Offline


[*] posted on 10-5-2022 at 20:02


The above solvent suggestions are good.

Dimethylformamide can work well too.






[Edited on 11-5-2022 by SWIM]




View user's profile View All Posts By User
ParkinsonWilkinson
Harmless
*




Posts: 5
Registered: 7-5-2022
Location: Singapore
Member Is Offline


[*] posted on 10-5-2022 at 21:07


Methyl acetate should also work, it's the main solvent in many super glue brands
View user's profile View All Posts By User
Keras
International Hazard
*****




Posts: 1136
Registered: 20-8-2018
Location: (48, 2)
Member Is Offline


[*] posted on 10-5-2022 at 21:30


Maybe also butanone (a.k.a. MEK, methyl ethyl ketone). Judging by its smell, it’s the main solvent in a lot of commercial glues (UHU type, in Europe). It should work like acetone, but since it’s a bit less volatile, you have more time ahead to use it.
View user's profile View All Posts By User
monolithic
Hazard to Others
***




Posts: 436
Registered: 5-3-2018
Member Is Offline

Mood: No Mood

[*] posted on 17-5-2022 at 03:14


Nitromethane is an excellent superglue remover, as Herr Haber mentioned. It works far better than acetone. I keep a small bottle of nitromethane just for this purpose. :)
View user's profile View All Posts By User