Darth-Vang
Harmless
Posts: 22
Registered: 28-6-2019
Member Is Offline
|
|
Sea salt as catalyst for derusting danger?
Hey all, I’m using sea salt as a electrolyte to acquire rust from a railroad spike, the cathode is carbon graphite rod. Is it dangerous to use sea
salt as an electrolyte? I’m currently running it now and I can see that the water is turning green! Running at 6 volts with 2.5ish amps with
variable power supply.

[Edited on 3-7-2022 by Darth-Vang]
|
|
|
clearly_not_atara
International Hazard
   
Posts: 2921
Registered: 3-11-2013
Member Is Offline
Mood: Big
|
|
Iron (II) chloride is green.
|
|
|
Darth-Vang
Harmless
Posts: 22
Registered: 28-6-2019
Member Is Offline
|
|
I guess it looked green at first, but now it’s all blackish color, I see
some white stuff, definitely see rust at the bottom of the jar. What’s the electrochemical equation for this? The water is tap water if I didn’t
mention that.
|
|
|
unionised
International Hazard
   
Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
It's not exactly dangerous.
You will probably find you get chloride in the rust (whether it's sea salt or any other sort of sodium chloride)
You are probably getting ferrous hydroxide which is not only green, but also insoluble.
If you blow air through it you will get ferric hydroxide which is orange/ brown.
What are you seeking to achieve?
|
|
|
Darth-Vang
Harmless
Posts: 22
Registered: 28-6-2019
Member Is Offline
|
|
Quote: Originally posted by unionised  | It's not exactly dangerous.
You will probably find you get chloride in the rust (whether it's sea salt or any other sort of sodium chloride)
You are probably getting ferrous hydroxide which is not only green, but also insoluble.
If you blow air through it you will get ferric hydroxide which is orange/ brown.
What are you seeking to achieve? | My compound of interests is iron oxide. I’m planning to run a small
scale experiment for thermite or other experiments that may include rust in it.
|
|
|
Darth-Vang
Harmless
Posts: 22
Registered: 28-6-2019
Member Is Offline
|
|
Update: Finally got around to filtering the stuff and dry them on the mantle and got iron oxide!
|
|
|