Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Thorium from monazite sand
samarium14
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 11-8-2022 at 03:02
Thorium from monazite sand


Hello! I'm just interested if it is worth working on sand that contains Th con. 200 g/t - 450 g/t. If it is worth the work, I can go to a particular strip of the Black Sea coast and take several kilos of this sand.

the sand:

Screenshot 2022-08-11 152615.png - 123kB

[Edited on 11-8-2022 by vano]

Edit by Texium: added details to thread title

[Edited on 8-11-2022 by Texium]
View user's profile View All Posts By User
Σldritch
Hazard to Others
***




Posts: 310
Registered: 22-3-2016
Member Is Offline

Mood: No Mood

[*] posted on 11-8-2022 at 06:04


Worth? Probably not, but if you want to have fun trying to separate the Thorium maybe you could improve your results by only collecting the sand that you can pick up with a magnet. That may give you a rare-earth richer sample, or just a bunch of iron, I don't know. It is Monazite sand, right? It is apparently paramagnetic.
View user's profile View All Posts By User
samarium14
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 11-8-2022 at 06:15


thanks! I don't know its name. people call it magnetic sand. The river washes the ore and brings it to the beach.
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2927
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 11-8-2022 at 06:31


Make sure you have an excellent particle filter mask. Thorium outside the body is not dangerous, but thorium in the lungs is a serious hazard.



Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
Rainwater
National Hazard
****




Posts: 993
Registered: 22-12-2021
Member Is Offline

Mood: Break'n glass & kick'n a's

[*] posted on 11-8-2022 at 06:45


It's a fun exercise. its my first step in an assay. You will sometimes be surprised at what you can get in a random sample. Targeting 1 element or compound that will make the process simpler.

With a little research, find the most common compound, typically an oxide, of the element of interest.
Compare the density to that of sand.

In a clear, tall, and slim container place a sample of material. Dissolve a small quantity of laundry detergent into just enough water to cover the sample. Secure the top of the container from splashing and expose it to mild vibration. You want to cause liquefaction of the sample without causing mixing.

Its a balance between force applied and sample movements/ mixing
You want a lot of movement but no mixing.
When you get it just right
You will notice the sample start turning into distinct layers.

If your desired compound has magnetic properties then those can be used as well to aid in separation.

Once separation has occurred comes the more difficult part of extracting the layers.
I stuff my container with cotton tightly, to immobilize the layers, decant the liquid, remove the cotton, and with a little luck can remove the entire sample with one well-practiced thump.




"You can't do that" - challenge accepted
View user's profile View All Posts By User
CharlieA
National Hazard
****




Posts: 646
Registered: 11-8-2015
Location: Missouri, USA
Member Is Offline

Mood: No Mood

[*] posted on 11-8-2022 at 15:04


At 450g per (English) ton, I calculate a content of 0.49g Th per kg or 1/5 part per thousand. Processing so much material for so little product will be a massive undertaking, but a great challenge to try. If you attempt this project, please keep us posted!
View user's profile View All Posts By User
samarium14
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 11-8-2022 at 15:41


maybe ill try excess conc. sulfuric acid. I heat it for a few hours and change the sand, again and again.

information from research about this sand.

Screenshot 2022-08-12 034402.png - 122kB

[Edited on 11-8-2022 by vano]

[Edited on 11-8-2022 by vano]
View user's profile View All Posts By User
B(a)P
International Hazard
*****




Posts: 1139
Registered: 29-9-2019
Member Is Offline

Mood: Festive

[*] posted on 11-8-2022 at 19:31


I attempted a similar thing. There was an old former mine for an ilmenite sand deposit near a property I used to own. I tried initially to use magnetic separation, but that failed. I ended up panning the material to concentrate the heavy minerals then digested it in hot sulfuric acid to remove the iron and leave me with titanium dioxide. While the removal of the ilmenite from the sand matrix was successful, the conversion to titanium dioxide was not. The ilmenite was at a far greater concentration than what you are looking at, but I think you are a far better chemist than I am! Good luck with it, I look forward to hearing how you go.
View user's profile View All Posts By User
samarium14
National Hazard
****




Posts: 661
Registered: 22-3-2019
Location: Georgia
Member Is Offline


[*] posted on 12-8-2022 at 01:15


thank you so much for the information B(a)P!
I think I'll use an electromagnet. I can make a strong electromagnet. I have liters of conc. sulfuric acid. so what I need is time. I think one week will be enough to heat the sand in sulfuric acid for a few hours every day, for example, 4 hours, I change the sand daily.
View user's profile View All Posts By User
Herr Haber
International Hazard
*****




Posts: 1236
Registered: 29-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 12-8-2022 at 15:12


Pretty cool experiment.
How much sand do you want to process ?




The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
View user's profile View All Posts By User
phlogiston
International Hazard
*****




Posts: 1383
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline

Mood: pyrophoric

[*] posted on 12-8-2022 at 15:24


What mineral contains the thorium? I don't know this particular locality, but generally, the thorium in Th-rich sands is present as monazite (or more rarely, thorianite), which isn't magnetic.
An easy and effective first step would be to separate by density, as others have mentioned. Panning is pretty simple and you should be a able to concentrate the thorium 10x-20x times pretty quickly that way. You can then get rid of the magnetic fraction with magnet, which is likely to be a major part of the heavy mineral fraction. So, if you can concentrate the Th quickly that way, perhaps 40x-50x times, you would be left with a fraction containing maybe 10-20 grams of Th per kg. Might be an interesting project to try to extract Th from that.

edit: re-read the title, so apparently monazite indeed. sorry.

[Edited on 12-8-2022 by phlogiston]




-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
View user's profile View All Posts By User
wg48temp9
National Hazard
****




Posts: 789
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline


[*] posted on 13-8-2022 at 00:05


Here is a snip from wiki:

"monazite-(Ce), (Ce,La,Nd,Th)PO4 (the most common member),
monazite-(La), (La,Ce,Nd)PO4,
monazite-(Nd), (Nd,La,Ce)PO4,
monazite-(Sm), (Sm,Gd,Ce,Th)PO4,
monazite-(Pr), (Pr,Ce,Nd,Th)PO4.
The elements in parentheses are listed in the order of their relative proportion within the mineral."

I guess the big advantage of going after the thorium is you can track it easily with a geiger counter.

If you'r successful you may like to try extracting some radium from a ton of uranium ore. Obtaining the ore is probably difficult and protecting yourself from the radiation may be difficult too. But seeing a few glowing mgs in a vial would be spectacular.




I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
View user's profile View All Posts By User
Yamato71
Hazard to Self
**




Posts: 72
Registered: 8-2-2012
Member Is Offline

Mood: Laid Back

[*] posted on 29-10-2022 at 18:06


Would you like a chunky pure specimen of monazite-(ce) to experiment with? I discovered a rare earth pegmatite in central Texas 17 years ago and collected about 25 kg of large brick red monazite crystals ranging from <1g to 2.4 kg. Because of the Th daughters present, these are fairly 'toasty'.

[Edited on 30-10-2022 by Yamato71]
View user's profile View All Posts By User

  Go To Top