[*] posted on 4-8-2023 at 08:17
How to make the air in my lab less oxidizing??


The air quality in my workspace is pretty terrible, it rusts everything in a matter of days! So it must be extremely oxidizing.

I could really need some ventilation in the space, but I'm not sure how do to it. Ideally, I would want one ventilation for the whole room, and one that I can attach to my (ductless) fume hood, so that anything that does't get stopped by the filter (i.e. H2) will be sucked outside.

Does anybody know a good way to do this?

Also, in the mean time, is there are anything I can spray in order to "reduce" the air and make it less oxidizing?

Any advice would be greatly appreciated!
View user's profile View All Posts By User
charley1957
Hazard to Others
***




Posts: 193
Registered: 18-2-2012
Location: Texas
Member Is Offline

Mood: Hotter than the hinges of Hell!

[*] posted on 4-8-2023 at 08:29


Sounds to me like you’ve got something not well sealed. I had the same problem, as I had some chemicals stored in a steel cabinet which continually rusted, dropping rust all over everything inside and on the countertop when I’d open the door. Turns out I had a not-well-sealed container of a chlorine compound that was being exposed to the air. After I repackaged this material in an airtight container my rusting problem was solved.
So check your chemical storage for oxidizing materials which may not be well sealed. I’ll bet you’ll find your problem.




You can’t claim you drank all day if you didn’t start early in the morning.
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3918
Registered: 8-2-2015
Member Is Offline


[*] posted on 4-8-2023 at 08:42


Rusting immediately makes me think of HCl(g) ,
Assuming that you have HCl(aq) test for escaping vapour using ammonia gas,
just opening a bottle of ammonia solution nearby will cause white ammonium chloride 'smoke'.
If there are HCl fumes, options are:
Get a better sealing bottle
Dilute to azeotropic (c20.2% w/w) to reduce HCl off-gassing.
Store HCl in a shady well ventilated place, preferably outdoors.

Edit: the answer above is better - many compounds off-gas.
eg TCCA pool chlorine.
The ammonia trick should reveal Halogen gasses.
(I store ammonia solution in the same plastic tub as hydrochloric acid, hopefully each partially neutralising fumes from the other)
If no ammonia solution is available,
bakers ammonium bicarbonate raising agent may be available.

[Edited on 4-8-2023 by Sulaiman]




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
Texium
Administrator
Thread Moved
4-8-2023 at 11:54
Monoamine
Hazard to Others
***




Posts: 168
Registered: 25-5-2021
Location: Sweden(ish)
Member Is Offline

Mood: +7

[*] posted on 9-8-2023 at 18:05


I suspect, the bromine in my fridge and the thionyl chloride next to it are partially the culprits. I've tried sealing them into glass vials, but there's too much of it to seal everything.

I have some litmus paper lying on a bench and when I come to it after a few days it's bright red. I'm slightly freaking out tbh.

But it's aight, I guess. I ordered a ventilator that I can build into the roof. Hopefully that will fix it...

Edit: Thank you for the ammonia advice. I will go do try that.

[Edited on 10-8-2023 by Monoamine]
View user's profile View All Posts By User
Lionel Spanner
Hazard to Others
***




Posts: 203
Registered: 14-12-2021
Location: near Barnsley, UK
Member Is Offline


[*] posted on 10-8-2023 at 14:09


Depending on the age and condition of the building and where your lab is located in it, it could also be high humidity.



Industrial chemist rediscovering the practical pleasures of pure chemistry.
Sometimes I make videos - https://www.youtube.com/@yorkshirechemist
View user's profile View All Posts By User
Johanson
Harmless
*




Posts: 39
Registered: 23-3-2023
Member Is Offline


[*] posted on 12-8-2023 at 21:58


"Does anybody know a good way to do this?"
First, your location says "Sweden" so I assume it's cold outside and that's why you don't just crack open a couple windows on opposite sides of the room; you don't want to frickin' freeze.
Just about every standard in the U.S. - Internat'l mechanical code, ASHRAE, OSHA, etc - call for a minimum of 4-12 room-air-changes per hour in laboratories, just to accommodate people, not to remove hazards. Calculate your room volume, and that will give you the minimum m^3/hour necessary. Every cubic meter you discharge will add to your heating/cooling bill, but that's the way it goes. If your room air is turning litmus paper bright red, I wouldn't want to work in it for long periods of time
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2552
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 12-8-2023 at 22:27


Yeah it's probably some HCl or other halogen-containing gas. In high school I made all my dad's tools rust in the garage when I did an experiment with HCl, he was NOT HAPPY.



As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3918
Registered: 8-2-2015
Member Is Offline


[*] posted on 12-8-2023 at 23:59


Quote: Originally posted by Johanson  
...Every cubic meter you discharge will add to your heating/cooling bill, but that's the way it goes...

Balancing comfort (heating cost) and safety in winter is difficult.
In my uk lab/shed there is always some ventilation,
during winter an infra-red heater nearby helps a lot.
I used a portable electric one with 3 bars so I can balance cost (400W per bar/element) vs comfort.
I suppose that UK/EU heating costs have risen significantly since I was home due to the idiotic/suicidal anti-Russian sanctions?




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
Johanson
Harmless
*




Posts: 39
Registered: 23-3-2023
Member Is Offline


[*] posted on 14-8-2023 at 09:48


Sulaiman: "I suppose that UK/EU heating costs have risen significantly since I was home due to the idiotic/suicidal anti-Russian sanctions?"

Is it legal to install a coal burning stove? There's almost more coal under the (UK's) king's bathroom than the rest of the world combined. Is that verboten now?
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 14-8-2023 at 09:59


Quote: Originally posted by Johanson  
Sulaiman: "I suppose that UK/EU heating costs have risen significantly since I was home due to the idiotic/suicidal anti-Russian sanctions?"

Is it legal to install a coal burning stove? There's almost more coal under the (UK's) king's bathroom than the rest of the world combined. Is that verboten now?

You can get coal, but it's not cheap, so why bother?
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4483
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 14-8-2023 at 10:37


Quote: Originally posted by Sulaiman  

I suppose that UK/EU heating costs have risen significantly since I was home due to the idiotic/suicidal anti-Russian sanctions?


Yeah, it would be far less idiotic and suicidal to just let Putin take everything he wants, from Ukraine to East Berlin.




Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4726
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: Seeking gainful employment

[*] posted on 15-8-2023 at 07:56


Quote: Originally posted by Metacelsus  
Yeah it's probably some HCl or other halogen-containing gas. In high school I made all my dad's tools rust in the garage when I did an experiment with HCl, he was NOT HAPPY.
Same! Mine still gives me crap about it sometimes. One day when I have real adult money, I'll buy him a nice new set of tools, then he won't be allowed to complain anymore. :D



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
averageaussie
Hazard to Self
**




Posts: 93
Registered: 30-4-2023
Location: Right behind you
Member Is Offline

Mood: school :(

[*] posted on 15-8-2023 at 17:57


yikes, bromine just leaking.

[Edited on 16-8-2023 by averageaussie]
View user's profile View All Posts By User

  Go To Top