4-Stroke
Hazard to Self
**




Posts: 61
Registered: 20-4-2024
Location: Canada
Member Is Offline

Mood: Often Wrong, Never Unsure

[*] posted on 10-11-2024 at 16:11
New (Simpler) Method for Making Sulfur Chlorides


Most of you know that sulfur chlorides are usually prepared by the standard procedure where chlorine gas is generated, dried, passed into molten sulfur, and the sulfur chlorides formed get distilled as soon as they form, all at the same time. This method has a few disadvantages, such as the need for:

-Much sophisticated glassware (a 2/3 neck RBF, stoppers, a chlorine generator, gas addition tube, either a heating mantle (expensive) or an oil bath (messy), a distillation adapter, a condenser, and a receiving adapter & flask)
-Constant monitoring of the reaction
-The horrid cleaning process afterwards
-Longer reaction time

The method I propose removes all of these disadvantages (but note that it still requires you to have some sulfur chlorides to start with). The only equipment needed is:

-Erlenmeyer flask (more accessible, cheaper, and easier to heat than a RBF)
-Condenser (any condenser will work, possibly even an air cooled one)
-Glass tubes (even some plastic ones will work)
-Rubber or silicone bungs
-Filter


Here is my proposed procedure:

Step 1: Setup a chlorine generator (the simplest way I could come up with):
A glass filtering flask is charged with 155 grams of TCCA (or 143 grams of Ca(OCl)2). A separatory funnel with 200ml of muriatic acid (or 270ml if Ca(OCl)2 is used) is placed on top.
Screenshot 2024-11-10 153403.png - 20kB

Step 2: A gas dryer (to dry the chlorine) is set up. A test tube is stoppered with a bung and a glass (or a suitable plastic) tube is inserted to the bottom. A second tube is connected that just barely enters the test tube. The test tube is filled with anhydrous (or monohydrate) calcium chloride.
Screenshot 2024-11-10 154038.png - 13kB

Step 3: 70ml (1 mole, 135 grams) of S2Cl2 is charged into an Erlenmeyer flask. A glass (or a suitable plastic) tube is placed into the S2Cl2.
Screenshot 2024-11-10 154631.png - 12kB

Step 4: The entire apparatus is assembled.
Screenshot 2024-11-10 155356.png - 51kB

Step 5: The muriatic acid is allowed to drip in and the evolution of chlorine is started. The chlorine starts bubbling through the S2Cl2.
Screenshot 2024-11-10 155717.png - 56kB

Step 6: After all of the muriatic acid has been used up, the S2Cl2 should have changed color from yellow to red as it was converted into 2 moles (205 grams, 127ml) of SCl2.
Screenshot 2024-11-10 155920.png - 49kB

Step 7: The chlorine generator, dryer, and input tube is disconnected and removed. The Erlenmeyer flask is charged with an excess (>65 grams) of sulfur, fitted with a condenser, and set up for reflux.
Screenshot 2024-11-10 160335.png - 14kB

Step 8: The solution is refluxed until it changes color to back to yellow and most of the sulfur is gone.
Screenshot 2024-11-10 160542.png - 10kB

Step 9: The condenser is removed and the solution is filtered to remove the unreacted sulfur.
Screenshot 2024-11-10 160958.png - 24kB

Step 10: Done! You should now have more S2Cl2 than you started with. Theoretically, 1 mole (135 grams, 70ml) of S2Cl2 --> 2 moles (205 grams, 127ml) of SCl2 --> 2 moles (270 grams, 140ml) S2Cl2.

I understand that the main problem with this method is getting any sulfur chlorides to start with, but it could be made by a method like this (https://www.youtube.com/watch?v=CgNxJHW513g) on a test-tube scale (or full scale if you have the equipment).

What do you think? Will it work?

[Edited on 11-11-2024 by 4-Stroke]




Ukrainium
View user's profile View All Posts By User
Tsjerk
International Hazard
*****




Posts: 3040
Registered: 20-4-2005
Location: Netherlands
Member Is Offline

Mood: Mood

[*] posted on 10-11-2024 at 21:40


At least, I never worked with sulfur chlorides, you will have problems with suck back, and I guess your drying apparatus won't be sufficiently large. Are you sure your method will be as efficient as you propose here?
Usually, especially with these will known reactions, there is a reason why they are done like the are done
View user's profile View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1253
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 10-11-2024 at 23:16


Sulfur reacts with S2Cl2 to form polysulfur dichlorides SxCl2. So any excess sulfur will react with your S2Cl2. If you want pure S2Cl2, you must distill it to remove unreacted sulfur (SxCl2 break up during distillation back to S2Cl2 and sulfur).
View user's profile View All Posts By User
bnull
National Hazard
****




Posts: 994
Registered: 15-1-2024
Location: East Woods
Member Is Offline

Mood: Fecking annoyed

[*] posted on 11-11-2024 at 06:54


Quote: Originally posted by 4-Stroke  
What do you think? Will it work?

Well, you still need stoppers, a chlorine generator, gas addition tube, some means to heat the stuff in order to purify it (see Brauer's Handbook of Preparative Inorganic Chemistry, p. 370-372), a distillation adapter, a condenser, and a receiving adapter & flask. And sulfur chloride to begin with.

Cleaning sulfur compounds from plastics, if you still intend to use them, is a mess.

In picture 4, you need a trap (I forgot how it is called) after the drying tube to prevent suck back. For the drying tube, a flask with concentrated sulfuric acid. To make it even safer, two traps after the drying tube.

Filter the stuff? No, thanks.

It may work if you make some improvements. But even so I'll stick to the standard procedure. I'm a natural-born pessimist; I tend to see what can go (very) wrong. There is an alternative process described somewhere in old publications, such as those journals of practical chemistry, maybe even in the Journal of Chemical Education (probably before the 1980s).

Edit: Typo.

[Edited on 12-11-2024 by bnull]




Quod scripsi, scripsi.

B. N. Ull

We have a lot of fun stuff in the Library.

Read The ScienceMadness Guidelines. They exist for a reason.
View user's profile View All Posts By User
Boffis
International Hazard
*****




Posts: 1925
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 11-11-2024 at 10:13


I would have thought that you will also need a vent with a chlorine scrubber on the final flask, at least to start with or you will never get the chlorine into the final flask.

I have to say that I don't see any real advantage over the original process apart from slightly simpler and cheaper equipment. Maybe you shouldn't be trying this reaction if you dont have the right equipment. Also chlorine attacks rubber stoppers terribly and you still have the chlorine delivery pipes, drying jar etc.

I thought you might have come up with a one pot process, say adding TCCA to a chlorinated solvent containing a suspension of sulphur and bubbling HCl gas through it :D
View user's profile View All Posts By User
Monoamine
Hazard to Others
***




Posts: 168
Registered: 25-5-2021
Location: Sweden(ish)
Member Is Offline

Mood: +7

[*] posted on 11-11-2024 at 20:38


It's a nice idea, perhaps if you want more S2Cl2. Also, really cool images! It's clear you put a lot of thought and effort into these illustrations. Cudos!

But with the exact same setup you can also just generate S2Cl2 directly by blowing the chlorine into elemental sulphur. And that way, you don't need to already have S2Cl2 on hand.

Actually, since you are refluxing the mixture in the last step anyway, I don't see how this will be less work or use less equipment than just generating S2Cl2. Both approaches would be about the same amount of work and they use the same equipment as you describe in your process.
View user's profile View All Posts By User
4-Stroke
Hazard to Self
**




Posts: 61
Registered: 20-4-2024
Location: Canada
Member Is Offline

Mood: Often Wrong, Never Unsure

[*] posted on 11-11-2024 at 22:43


Quote: Originally posted by Tsjerk  
At least, I never worked with sulfur chlorides, you will have problems with suck back, and I guess your drying apparatus won't be sufficiently large. Are you sure your method will be as efficient as you propose here?
Usually, especially with these will known reactions, there is a reason why they are done like the are done


Nope, I'm absolutely not sure if it is effective (or even viable at all), but that's why I'm asking for advice. And you're right, there probably is a reason, but different methods are often a balance of time, yield, and the required equipment, but because different people need different things, some methods might be "better" for some than for others.

Quote: Originally posted by Bedlasky  
Sulfur reacts with S2Cl2 to form polysulfur dichlorides SxCl2. So any excess sulfur will react with your S2Cl2. If you want pure S2Cl2, you must distill it to remove unreacted sulfur (SxCl2 break up during distillation back to S2Cl2 and sulfur).


Oh, that's interesting. I haven't heard of that before. But even some, the procedure could be repeated many times (each time chlorinating the polysulfur dichlorides all the way to SCl2) and then distilled only once at the end to yield pure S2Cl2.

Quote: Originally posted by bnull  
Quote: Originally posted by 4-Stroke  
What do you think? Will it work?

Well, you still need stoppers, a chlorine generator, gas addition tube, some means to heat the stuff in order to purify it (see Brauer's Handbook of Preparative Inorganic Chemistry, p. 370-372), a distillation adapter, a condenser, and a receiving adapter & flask. And sulfur chloride to begin with.

Cleaning sulfur compounds from plastics, if you still intend to use them, is a mess.

In picture 4, you need a trap (I forgot how it is called) after the drying tube to prevent suck back. For the drying tube, a flask with concentrated sulfuric acid. To make it even safer, two traps after the drying tube.

Filter the stuff? No, thanks.

It may work if you make some improvements. But even so I'll stick to the standard procedure. I'm a natural-born pessimist; I tend to see what can go (very) wrong. There is an alternative process described somewhere in old publications, such as those journals of practical chemistry, maybe even in the Journal of Chemical Education (probably before the 1980s).

Edit: Typo.

[Edited on 12-11-2024 by bnull]


Fine, you still do need some equipment, but NOT a distillation adapter, receiving adapter, or a receiving flask. An Erlenmeyer flask is also a lot easier to heat than a RBF.

Could xylene be used to clean plastic and glass tubes (since sulfur is soluble in it)?

What's so bad about filtering it apart from the smell?

The main point of the procedure is that it's a lot easier (and I suspect faster) than the conventional method. It is also easier to perform on a bigger scale (since less equipment is required). It could also be performed in a lead-lined reaction vessel (anything from a small pot to a 55 gallon drum covered with lead sheet inside) a lot more easily. Also less glassware to clean at the end ;)
But thanks for the references, I'll take a look at those.

Quote: Originally posted by Boffis  
I would have thought that you will also need a vent with a chlorine scrubber on the final flask, at least to start with or you will never get the chlorine into the final flask.


I'm a little confused by what you are saying here. Do you mind explaining?

Quote: Originally posted by Boffis  
I have to say that I don't see any real advantage over the original process apart from slightly simpler and cheaper equipment. Maybe you shouldn't be trying this reaction if you dont have the right equipment.


I actually do have most of the equipment required the standard procedure, but the goal of this one is that it is faster (I think), requires cleaning less glassware, is a lot easier to perform on a larger scale in a lead lined reactor, and is just generally less of a hassle (working with molten sulfur, chlorinating it, an distilling simultaneously vs just bubbling chlorine, adding sulfur, refluxing, and repeat).

Quote: Originally posted by Boffis  
I thought you might have come up with a one pot process, say adding TCCA to a chlorinated solvent containing a suspension of sulphur and bubbling HCl gas through it :D


That's actually quite an idea :D I'll think a bit more about that.

Quote: Originally posted by Monoamine  
It's a nice idea, perhaps if you want more S2Cl2. Also, really cool images! It's clear you put a lot of thought and effort into these illustrations. Cudos!

Thank you! Finally someone noticed :D

Quote: Originally posted by Monoamine  
But with the exact same setup you can also just generate S2Cl2 directly by blowing the chlorine into elemental sulphur. And that way, you don't need to already have S2Cl2 on hand.


Yes, but this setup is still faster, easier to clean, and is much simpler to perform in a lead lined reaction chamber.

Quote: Originally posted by Monoamine  
Actually, since you are refluxing the mixture in the last step anyway, I don't see how this will be less work or use less equipment than just generating S2Cl2. Both approaches would be about the same amount of work and they use the same equipment as you describe in your process.


Yes but this process kind of like separates the entire reaction into different sections, so each one separately is easier to perform than all at once.




Ukrainium
View user's profile View All Posts By User
bnull
National Hazard
****




Posts: 994
Registered: 15-1-2024
Location: East Woods
Member Is Offline

Mood: Fecking annoyed

[*] posted on 12-11-2024 at 08:54


Quote:
Fine, you still do need some equipment, but NOT a distillation adapter, receiving adapter, or a receiving flask. An Erlenmeyer flask is also a lot easier to heat than a RBF.

Nope. You need ALL the original equipment plus the erlenmeyer, the funnel, and the two traps (see below). The chloride is purified by distillation, hence the need for the three pieces of glassware that you intend to ditch. You won't use the crude stuff that you have just filtered, will you?

Quote:
Could xylene be used to clean plastic and glass tubes (since sulfur is soluble in it)?

Glass, yes, obviously; plastic, no. Plastics are usually very fond of solvents. Using xylene to remove sulfur from plastic tubing would make some sulfur diffuse into it.

Quote:
The main point of the procedure is that it's a lot easier (and I suspect faster) than the conventional method. It is also easier to perform on a bigger scale (since less equipment is required).

Try it small scale first. Better yet, perform both processes, the standard and the one you devised, and compare them. This way you can see which one is better, if there is something you missed.

Quote:
It could also be performed in a lead-lined reaction vessel (anything from a small pot to a 55 gallon drum covered with lead sheet inside) a lot more easily. Also less glassware to clean at the end ;)

Why would one need that much sulfur chloride?

Quote:
But thanks for the references, I'll take a look at those.

Please do. Brauer's is a classic.

I understand you want to improve processes and make the life of amateur/home/hobby chemists easier. But hold on: how much sulfur chloride does an amateur chemist need? Not gallons of the stuff, I believe (unless the chemist is making mustard gas).

My advice is, consult the literature, especially the old books on preparative chemistry (we have lots of them in the Library). There is always a reason why the standard procedure became the standard procedure.

The pictures are pretty good, by the way. What program did you use?




Quod scripsi, scripsi.

B. N. Ull

We have a lot of fun stuff in the Library.

Read The ScienceMadness Guidelines. They exist for a reason.
View user's profile View All Posts By User
4-Stroke
Hazard to Self
**




Posts: 61
Registered: 20-4-2024
Location: Canada
Member Is Offline

Mood: Often Wrong, Never Unsure

[*] posted on 12-11-2024 at 11:09


Quote: Originally posted by bnull  
Nope. You need ALL the original equipment plus the erlenmeyer, the funnel, and the two traps (see below). The chloride is purified by distillation, hence the need for the three pieces of glassware that you intend to ditch. You won't use the crude stuff that you have just filtered, will you?

Well, that depends on what you need it for (distillation might not be necessary for some reactions). Alternatively, if sulfur dichloride is desired, the filtered mixture of polysulfur dichlorides and disulfur dichloride can be chlorinated all the way to SCl2, and since (I assume) there are no "more chlorinated" sulfur chlorides, it should be pretty pure SCl2.

Quote: Originally posted by bnull  
Glass, yes, obviously; plastic, no. Plastics are usually very fond of solvents. Using xylene to remove sulfur from plastic tubing would make some sulfur diffuse into it.

Ah yes, I haven't thought of that. Many plastics could even dissolve in solvents, so yeah, that was a pretty dumb suggestion from me.

Quote: Originally posted by bnull  
Try it small scale first. Better yet, perform both processes, the standard and the one you devised, and compare them. This way you can see which one is better, if there is something you missed.

Yes, I will, but we are moving soon, so I can't really do much for the next couple month, that's why I just decided to post this here. But yes, when I can, I definitely will try both methods, I've been wanting to do so for quite a while now.

Quote: Originally posted by bnull  
I understand you want to improve processes and make the life of amateur/home/hobby chemists easier. But hold on: how much sulfur chloride does an amateur chemist need? Not gallons of the stuff, I believe (unless the chemist is making mustard gas).

As much as the chemist wants ;) Well just recently I was asking about lead (and other materials) lined reaction vessels, so I just had to include this here.

Quote: Originally posted by bnull  
My advice is, consult the literature, especially the old books on preparative chemistry (we have lots of them in the Library). There is always a reason why the standard procedure became the standard procedure.

Yes, by now I'm pretty much running out of compelling arguments as to why my procedure is worth it (probably because it isn't ;)).

But I just wanted to ask, what do you think of this (https://www.youtube.com/watch?v=CgNxJHW513g) method? I found it some time ago, and it seems pretty good to me. Just mix TCCA with sulfur and distill. He used the wrong (stoichiometrically) ratio though. What do you think?

Also, another question, why is sulfur chloride produced industrially by bubbling chlorine through barely molten (~120°C) sulfur, but in the standard laboratory preparation method, the sulfur is heated much more (~250°C) and thus the sulfur chloride is distilled immediately as it is formed. Considering that there is about a ~20°C range between sulfur's melting point and disulfur dichloride's boiling point, wouldn't it be easier to just chlorinate the molten sulfur and distill it separately?

Quote: Originally posted by bnull  
The pictures are pretty good, by the way. What program did you use?

Thanks! It isn't a program, just the first website that came up. It's https://chemix.org/.

[Edited on 12-11-2024 by 4-Stroke]




Ukrainium
View user's profile View All Posts By User
bnull
National Hazard
****




Posts: 994
Registered: 15-1-2024
Location: East Woods
Member Is Offline

Mood: Fecking annoyed

[*] posted on 12-11-2024 at 15:00


Quote: Originally posted by 4-Stroke  
But I just wanted to ask, what do you think of this (https://www.youtube.com/watch?v=CgNxJHW513g) method? I found it some time ago, and it seems pretty good to me. Just mix TCCA with sulfur and distill. He used the wrong (stoichiometrically) ratio though. What do you think?

Apart from the sulfur fumes escaping the receiver a short distance from an open flame (O_o) and the possibility of the whole thing blowing up, it is interesting. I wouldn't do it, but it is interesting.

Quote:
Also, another question, why is sulfur chloride produced industrially by bubbling chlorine through barely molten (~120°C) sulfur, but in the standard laboratory preparation method, the sulfur is heated much more (~250°C) and thus the sulfur chloride is distilled immediately as it is formed. Considering that there is about a ~20°C range between sulfur's melting point and disulfur dichloride's boiling point, wouldn't it be easier to just chlorinate the molten sulfur and distill it separately?

This is one thing I have no idea (at least at the moment). You may check these sections on sulfur monochloride and sulfur dichloride from PubChem.

Quote:
Thanks! It isn't a program, just the first website that came up. It's https://chemix.org/.

Just added it to my bookmarks.




Quod scripsi, scripsi.

B. N. Ull

We have a lot of fun stuff in the Library.

Read The ScienceMadness Guidelines. They exist for a reason.
View user's profile View All Posts By User
4-Stroke
Hazard to Self
**




Posts: 61
Registered: 20-4-2024
Location: Canada
Member Is Offline

Mood: Often Wrong, Never Unsure

[*] posted on 12-11-2024 at 15:13


Quote: Originally posted by bnull  

Apart from the sulfur fumes escaping the receiver a short distance from an open flame (O_o) and the possibility of the whole thing blowing up, it is interesting. I wouldn't do it, but it is interesting.

Well, I've boiled gasoline in an open pot over an open flame before, so... But it does seem pretty stable (and the guy says he performed the reaction "dozens" of times) so I think that it shouldn't blow up. But I'll be the one to check that in a couple month.

Quote: Originally posted by bnull  
This is one thing I have no idea (at least at the moment). You may check these sections on sulfur monochloride and sulfur dichloride from PubChem.

Ah I see, that's fine. I'll check those links.

Quote: Originally posted by bnull  
Just added it to my bookmarks.
;)



Ukrainium
View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4743
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: Seeking gainful employment

[*] posted on 12-11-2024 at 16:01


Quote: Originally posted by 4-Stroke  
Well, I've boiled gasoline in an open pot over an open flame before, so...
So… you’re an idiot?



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
4-Stroke
Hazard to Self
**




Posts: 61
Registered: 20-4-2024
Location: Canada
Member Is Offline

Mood: Often Wrong, Never Unsure

[*] posted on 12-11-2024 at 16:38


Well, there wasn't a lot of it, and I was kind of prepared for it to ignite (which it surprisingly didn't). But yes, I guess you could say so :D
But the great chemists of the 19th century distilled diethyl ether with an open flame (albeit not in an open container), so I don't think that what I did was really that dangerous (considering that I was also doing it outside).

[Edited on 13-11-2024 by 4-Stroke]




Ukrainium
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2923
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 13-11-2024 at 09:41


Quote:
I thought you might have come up with a one pot process, say adding TCCA to a chlorinated solvent containing a suspension of sulphur and bubbling HCl gas through it

In theory, following the vanadium-chlorine cycle for thermochemical water splitting, you could follow the wacky chemistry of the vanadium chlorides.

- VCl3 can be dried by heating

- at >350 C, VCl3 (l) disproportionates into VCl2 (s) and VCl4 (g)

- at low temperatures, VCl4 (l, bp 148 C) slowly disproportionates into VCl3 (s) and Cl2 (g)

The equilibrium pressure of chlorine over VCl4 is pretty low, but it continually releases chlorine. The unusual disproportionation is apparently driven by the lattice energy of crystalline VCl3. This was considered decades ago for hydrogen production from water, but probably isn't practical for mass production because there are too many steps.




Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
6dthjd1
Hazard to Self
**




Posts: 94
Registered: 30-6-2018
Member Is Offline


[*] posted on 3-12-2024 at 07:17


Quote: Originally posted by Texium  
Quote: Originally posted by 4-Stroke  
Well, I've boiled gasoline in an open pot over an open flame before, so...
So… you’re an idiot?


I hope this was done outside.
View user's profile View All Posts By User
6dthjd1
Hazard to Self
**




Posts: 94
Registered: 30-6-2018
Member Is Offline


[*] posted on 3-12-2024 at 07:18


Quote: Originally posted by 4-Stroke  
Well, there wasn't a lot of it, and I was kind of prepared for it to ignite (which it surprisingly didn't). But yes, I guess you could say so :D
But the great chemists of the 19th century distilled diethyl ether with an open flame (albeit not in an open container), so I don't think that what I did was really that dangerous (considering that I was also doing it outside).

Do you remember how much they distilled?

[Edited on 13-11-2024 by 4-Stroke]
View user's profile View All Posts By User
6dthjd1
Hazard to Self
**




Posts: 94
Registered: 30-6-2018
Member Is Offline


[*] posted on 3-12-2024 at 07:34


Quote: Originally posted by 4-Stroke  
Well, there wasn't a lot of it, and I was kind of prepared for it to ignite (which it surprisingly didn't). But yes, I guess you could say so :D
But the great chemists of the 19th century distilled diethyl ether with an open flame (albeit not in an open container), so I don't think that what I did was really that dangerous (considering that I was also doing it outside).

Do you remember how much they distilled?

[Edited on 13-11-2024 by 4-Stroke]
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3942
Registered: 8-2-2015
Member Is Offline


[*] posted on 3-12-2024 at 09:36


Bofis:
would have thought that you will also need a vent with a chlorine scrubber on the final flask, at least to start with or you will never get the chlorine into the finalpl flask.

4-stroke:
I'm a little confused by what you are saying here. Do you mind explaining?
.......,...............
The stopper in the Erlenmeyer used for bubbling has only one hole,
there is nowhere for excess gas to escape so internal pressure will increase
the pressurised chlorine gas will bubble up through the addition funnel the next time the stopcock is opened...
If the pressure is high a violent eruption of HCl and chlorine will occur.
Not good

Plus, when bubbling chlorine I always get unreacted bubbles reaching the surface and escaping,
so a scrubber is used to absorb and/or neutralise the excess gas.

PS nice drawings, I must learn one day.
and, moist chlorine gas corrodes rubber quickly - I can vouch for that.!
and, have a brief read about 'suck back'

[Edited on 3-12-2024 by Sulaiman]




CAUTION : Hobby Chemist, not Professional or even Amateur