I have for a long time tried to construct different rocket nozzles using different materials like cement, clay, aluminium, copper, stainless steel and
lead sponges. But I've had some difficulties with for example: my motors melting or exploding. What do you guys use for designs (ratios and types) and
what do you use as materials and what tools are involved.
(Ive experimented with cooled nozzles on small scale (like with co2 or water) and with variating success. Ive thought but not done a heat exchanging
nozzle thats cooled by a element in the front of the rocket)
professional chemical taster
|
|
|
metalresearcher
National Hazard
  
Posts: 822
Registered: 7-9-2010
Member Is Offline
Mood: Reactive
|
|
I have no experience with rocket engines (yes, engine, not motor as a motor is electrical), but I bet that Al, Cu or Pb are unsuitable as these metals
have a too low melting point to withstand temperatures of the combustion.
|
|
|
WD40_enjoyer
Harmless
Posts: 22
Registered: 11-7-2025
Location: Sweden
Member Is Offline
Mood: Extremely bored!!
|
|
1. Motor is not bound to electrical 2. Al is for cost/heat transfer, cu is for better heat transfer and high melting point, pb sponge is for high temp
and placeholder for catalysts.
professional chemical taster
|
|
|
bnull
National Hazard
  
Posts: 994
Registered: 15-1-2024
Location: East Woods
Member Is Offline
Mood: Fecking annoyed
|
|
OK, first of all: what propellant are you using? I hope it's not a C-Stoff/T-Stoff sort of combination.
What you need is a refractory alloy. Inconel (nickel-chromium-something else) is a good one, if I'm not mistaken was developed exactly for that kind
of application. How much it will cost? No idea.
|
|
|
WD40_enjoyer
Harmless
Posts: 22
Registered: 11-7-2025
Location: Sweden
Member Is Offline
Mood: Extremely bored!!
|
|
I am pondering different fuels but right now I'm doing some research for hydrazine (and its derivatives) and an oxidiser like n2o and possible high
conc h2o2. Good idea about that alloy, what specs has it and how is it's mechanical properties?
professional chemical taster
|
|
|
bnull
National Hazard
  
Posts: 994
Registered: 15-1-2024
Location: East Woods
Member Is Offline
Mood: Fecking annoyed
|
|
Tish, tish, you'll need to read the literature for that kind of information (Aerospace Materials and Material Technologies, Journal of Aeronautical
Materials, that sort of publication). Inconel is not a single alloy, it comes in many specifications and the right one depends on what fuel and
oxidant you're using. As far as I know, there's no "one-size-fits-all" alloy.
|
|
|
WD40_enjoyer
Harmless
Posts: 22
Registered: 11-7-2025
Location: Sweden
Member Is Offline
Mood: Extremely bored!!
|
|
But for example with n2o and hydrazine at stochimetric amounts what would that consist of? What im getting at is it easy to machine/weld to since if
it for example is super difficult to melt/turn down in a lathe I won't be using that but if not then I might depending on price and such factors.
professional chemical taster
|
|
|
Twospoons
International Hazard
   
Posts: 1392
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
The more usual nozzle materials would be fiber reinforced phenolic resin, or graphite. Assuming compacted Bentonite is not working for you. You
haven't said how big your rockets are.
[Edited on 13-7-2025 by Twospoons]
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
|
WD40_enjoyer
Harmless
Posts: 22
Registered: 11-7-2025
Location: Sweden
Member Is Offline
Mood: Extremely bored!!
|
|
I am currently trying different scales since it can very easily get very large when you try to overengineer everything, but my best working prototype
is about 5-7cm in diameter.
professional chemical taster
|
|
|
Fulmen
International Hazard
   
Posts: 1794
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
You don't give us anything to work with. What sort of motors? And which propellant? Single use or reusable?
We're not banging rocks together here. We know how to put a man back together.
|
|
|
WD40_enjoyer
Harmless
Posts: 22
Registered: 11-7-2025
Location: Sweden
Member Is Offline
Mood: Extremely bored!!
|
|
I've said which propellant, they are de laval nozzles and are supposed to be reusable. I've mostly been focusing on the motors themselves and not the
entire rocket construction (that means i haven't physically made it fully, but the design exists in Fusion 360).
professional chemical taster
|
|
|
Twospoons
International Hazard
   
Posts: 1392
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
Hmm. In that case I would suggest using replaceable graphite inserts as the hot face in your nozzle. You will get nozzle erosion no matter what you
do, so making a small part of the nozzle replaceable would seem sensible. Graphite is easy to obtain, easy to shape, and reasonably priced.
[Edited on 13-7-2025 by Twospoons]
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
|
Fulmen
International Hazard
   
Posts: 1794
Registered: 24-9-2005
Member Is Offline
Mood: Bored
|
|
Ah yes, I found it after a more thorough reading. But my argument still stands, you're not giving people much to work with. It's hard to judge your
level of expertise from your posts. You seem to ask very basic questions while talking about very advanced technologies (liquid fuels). I think you
will get better advice if you share a but more about your work up to this point.
We're not banging rocks together here. We know how to put a man back together.
|
|
|
WD40_enjoyer
Harmless
Posts: 22
Registered: 11-7-2025
Location: Sweden
Member Is Offline
Mood: Extremely bored!!
|
|
Quote: Originally posted by Twospoons  | Hmm. In that case I would suggest using replaceable graphite inserts as the hot face in your nozzle. You will get nozzle erosion no matter what you
do, so making a small part of the nozzle replaceable would seem sensible. Graphite is easy to obtain, easy to shape, and reasonably priced.
[Edited on 13-7-2025 by Twospoons] |
Hmm seems reasonable to have replaceable parts of the engine. I will look in to it.
professional chemical taster
|
|
|
WD40_enjoyer
Harmless
Posts: 22
Registered: 11-7-2025
Location: Sweden
Member Is Offline
Mood: Extremely bored!!
|
|
Quote: Originally posted by Fulmen  | Ah yes, I found it after a more thorough reading. But my argument still stands, you're not giving people much to work with. It's hard to judge your
level of expertise from your posts. You seem to ask very basic questions while talking about very advanced technologies (liquid fuels). I think you
will get better advice if you share a but more about your work up to this point.
|
I'm sorry if I'm not supplying mich information but can you be more specific about the info you want to receive since I'm not fully understanding what
it is you want. All I'm asking is for ideas fro materials that can survive corrosion (so i can for example use h2o2) and can withstand high heat. I'm
not asking for blueprints nor designs. I'm sorry if I haven't made that clear perfectly!
professional chemical taster
|
|
|