Taoiseach
Hazard to Others
 
Posts: 241
Registered: 16-3-2008
Member Is Offline
Mood: No Mood
|
|
Where did you hear about it? I also doubt it exists.
There seems to be an "zinc acetate-peroxide complex" tough:
http://www.freepatentsonline.com/4172841.html
http://www.freepatentsonline.com/5152996.html
|
|
|
Zelot
Harmless
Posts: 45
Registered: 27-1-2008
Member Is Offline
Mood: hopeful
|
|
Yesterday I did electrolysis of an ammonium nitrate solution with copper electrodes in hopes of getting TACN. After an hour or two at ~5 volts and 1
amp, I filtered the solution and ended up with CuOH in the filter and a very deep blue-violet solution in the container. I assume this is either a
tetraamine copper or tetraamine copper nitrate solution.
You add acetone to precipitate it, right? Flame tests will follow after precipitation.
So... what did you do over the weekend?
|
|
|
Zinc
Hazard to Others
 
Posts: 472
Registered: 10-5-2006
Member Is Offline
Mood: No Mood
|
|
I don't remember where I heard about it.
The acetate complex seems interesting and easy to make. As far as I understand dissolve some zinc in acetic acid, remove the excess piece of Zn, and
then add some H2O2 and heat it so the complex precipitates. Then just filter it, wash and let dry. I will try today and post the results.
Is there perhaps some similar copper complex?
[Edited on 8-4-2008 by Zinc]
|
|
|
Zinc
Hazard to Others
 
Posts: 472
Registered: 10-5-2006
Member Is Offline
Mood: No Mood
|
|
Unfortunately I wont be able to make the complex as I have trouble to make zinc acetate. My Zn doesn't want to dissolve in 80% acetic acid.
|
|
|
Microtek
National Hazard
  
Posts: 994
Registered: 23-9-2002
Member Is Offline
Mood: No Mood
|
|
Just make some Zn(OH)2 and react that with acetic acid to get your acetate.
|
|
|
Zelot
Harmless
Posts: 45
Registered: 27-1-2008
Member Is Offline
Mood: hopeful
|
|
Don't you make Zn(OH)2 by reacting a zinc salt with ammonia?
So... what did you do over the weekend?
|
|
|
not_important
International Hazard
   
Posts: 3873
Registered: 21-7-2006
Member Is Offline
Mood: No Mood
|
|
Check the solubility of zinc acetate (dihydrate), you need enough water to get all of it into solution. I think it's about 1 g/2 cc I think you are
going to want to dilute the acetic acid a bit.
Also try touching a bit of platinum, gold, silver, or even nickel, iron, or copper to the zinc while it is in the acid.
Another thing you could try is to treat the zinc with a little HCl, to get it reacting, then quickly rinse and drop into warm acetic acid.
|
|
|
Zinc
Hazard to Others
 
Posts: 472
Registered: 10-5-2006
Member Is Offline
Mood: No Mood
|
|
Today I added some more acetic acid (quite a lot has evaporated) and diluted it with some warm water.
|
|
|
Zelot
Harmless
Posts: 45
Registered: 27-1-2008
Member Is Offline
Mood: hopeful
|
|
@zinc
Were you successful in making the ZAP yet?
So... what did you do over the weekend?
|
|
|
Zinc
Hazard to Others
 
Posts: 472
Registered: 10-5-2006
Member Is Offline
Mood: No Mood
|
|
Not yet. As my attempt to make Zn acetate failed. Today I am going to dissolve Zn in HCl and later precipitate the hydroxide with NH4OH (first have to
buy that). Then dissolve the hydroxide in acetic acid.
|
|
|
Taoiseach
Hazard to Others
 
Posts: 241
Registered: 16-3-2008
Member Is Offline
Mood: No Mood
|
|
Be careful when you precipate with NaOH because zinc is ampother! If you add too much, the precipate will redissolve:
[Zn(H2O)6]2+(aq) + 2OH-(aq) ---> Zn(OH)2(s) + 6H2O(l)
Zn(OH)2(s) + 2OH-(aq) ---> Zn(OH)42-(aq)
Na2[Zn(OH)4] is well soluble.
If you have sodium carbonate, use that! You will get basic zinc carbonate plus quite some CO2 bubbling. Zinc carbonate does not redissolve in excess
sodium carbonate and it will be easier to neutralise your acetic acid with it. Just add zinc carbonate until no more is dissolve and no more CO2 is
formed, then filter & evaporate the solution.
|
|
|
Zinc
Hazard to Others
 
Posts: 472
Registered: 10-5-2006
Member Is Offline
Mood: No Mood
|
|
Very good. I will then use that method (which is better for me as then I don't have to buy NH4OH and I already have sodium carbonate).
Today I put some Zn in HCl to dissolve and tomorrow I will precipitate the the basic carbonate.
|
|
|
Zinc
Hazard to Others
 
Posts: 472
Registered: 10-5-2006
Member Is Offline
Mood: No Mood
|
|
Right now I am filtering the precipitated Zn carbonate. When it filters I will dissolve it in acetic acid and add 30% H2O2 to precipitate the peroxide
complex.
|
|
|
Zinc
Hazard to Others
 
Posts: 472
Registered: 10-5-2006
Member Is Offline
Mood: No Mood
|
|
When it filtered I dissolved it in an excess of acetic acid and added some 30% H2O2. Nothing precipitated. Only the solution turned to a brown (but
transparent) color. Does anyone know why did it happen?
And one more question, is that complex explosive? As the patent doesn't say that it is.
|
|
|
Zelot
Harmless
Posts: 45
Registered: 27-1-2008
Member Is Offline
Mood: hopeful
|
|
I may have made some TACN by adding a large excess of NH4OH to a CuSO4+NH4NO3 mixture. It became deep blue, almost violet. Some copper metal was
precipitated, but was then formed into CuOH. I filtered to get just the solution. Can you precipitate TACN with rubbing alcohol?
So... what did you do over the weekend?
|
|
|
Zinc
Hazard to Others
 
Posts: 472
Registered: 10-5-2006
Member Is Offline
Mood: No Mood
|
|
I think that it can but I never tried.
|
|
|
Taoiseach
Hazard to Others
 
Posts: 241
Registered: 16-3-2008
Member Is Offline
Mood: No Mood
|
|
TACN should be insoluble in ethanol but copper(II)nitrate is soluble. I doubt you can precipate TACN from a solution containing [Cu(NH3)4](2+),
SO4(2-) and NO3(-) ions. You might be able to get a mix of the tetrammine sulfate and nitrate tough.
|
|
|
Jor
National Hazard
  
Posts: 950
Registered: 21-11-2007
Member Is Offline
Mood: No Mood
|
|
I just made some tetraamminecopper(II) persulphate.
When I put some of the dry material in a test tube, and heat the test tube, it explodes with a small 'Poof' sound.
White smoke evolves and a light green residue remains.
This residue dissolves in dilute hydrochloric acid. Small amounts of gas (bubbles) are evolved while it dissolves.
Now who knows what reaction is taking place when this compound explodes/decomposes? I have no idea.
|
|
|
woelen
Super Administrator
       
Posts: 8150
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
The persulphate ion oxidizes the ammonia in the cuprammine complex, but the compound is highly oxygen deficient, so the explosion is not powerful.
|
|
|
Jor
National Hazard
  
Posts: 950
Registered: 21-11-2007
Member Is Offline
Mood: No Mood
|
|
Yes, I know the persulphate is oxidising the ammonia, but I can't figure out what's really happening... What is the equation?
|
|
|
woelen
Super Administrator
       
Posts: 8150
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
You can't give a precise equation of this. There are so many reactions.
For the oxidation part, you could write: 2NH3 + 3[O] --> N2 + 3H2O
Here, the [O] comes from the persulfate ion: S2O8(2-) --> S2O7(2-) + [O]
The persulfate ion then with the water formed builds two bisulfate ions, free pyrosulfate certainly will not exist under these conditions with ammonia
and water present. These bisulfates consume other ammonia molecules and the heat of decomposition also certainly will expell some ammonia from the
complex as well. This explains why the solid becomes light blue/green, the tetrammine complex is destroyed.
Most likely, there also will be some unreacted persulfate as well. This explains the bubbling when it is added to hydrochloric acid.
[Edited on 29-5-08 by woelen]
|
|
|
Zombiekitten
Harmless
Posts: 4
Registered: 22-6-2008
Member Is Offline
Mood: BRAAAINS! *meow*
|
|
is there tetramminecopper(II) picrate?
|
|
|
Axt
National Hazard
  
Posts: 984
Registered: 28-1-2003
Member Is Offline
Mood: No Mood
|
|
Well, yes there is. However I don't see any reason to pop my eyes out over it.
|
|
|
franklyn
International Hazard
   
Posts: 3026
Registered: 30-5-2006
Location: Da Big Apple
Member Is Offline
Mood: No Mood
|
|
The Combustion of the Salts of Tetraamine Copper (II).
Not a free download yet, but thought I would pass along this citation
http://www.ntis.gov/search/product.aspx?ABBR=AD779649
http://stinet.dtic.mil/oai/oai?verb=getRecord&metadataPr...
http://stinet.dtic.mil/stinet/jsp/docread.jsp?K2DocKey=http%...
Another related thread on TACN
http://www.sciencemadness.org/talk/viewthread.php?tid=2187&a...
and this post
http://www.roguesci.org/theforum/showpost.php?s=a13507bed910...
______________
Just a thought,
It occurs to me that formaldehyde will condense with a coordimated metal amine complex.
Assuming coordination is not completely destroyed releasing the metal oxide, this would add
fuel to the oxygen rich compound.
A Textbook of Inorganic Chemistry Ed. J. Newton Friend
Vol X The Metal Amines M. M..J. Sutherland 1928
This I must have obtained on this forum but the location eludes me so download here
http://www.keepmyfile.com/download/df912e2298535
Explosive Properties of Metal Ammines
Previuosly provided by Roscoe Bodine, here
http://www.sciencemadness.org/talk/viewthread.php?action=att...
Related to my conjecture above
Attachment: Reaction between Formaldehyde and Ammonia.pdf (763kB) This file has been downloaded 2035 times
|
|
|
Taoiseach
Hazard to Others
 
Posts: 241
Registered: 16-3-2008
Member Is Offline
Mood: No Mood
|
|
Interesting stuff, thx 4 the upload!
I wonder if an explosive complex might be obtained by heating Ca(NO3)2 in a steam of dry NH3. Bis-en-copper(II)bromate might also be obtained this
way.
I believe there is some kind of water of hydration in TACN and TACP. Both salts dont burn readily even when completely dry. However, when heated
carefully in a steam of dry air for some time their blue color shifts towards a deep violet color and these violet salts DO burn/explode readily. In
moist air I observed that my putative anhydrous TACP turns deep blue again after a short time. Also I once left a small bottle of TACP in a very hot
spot in the sun (not a wise thing I know :cool and droplets of water deposited
inside and the salt turned violet. When put in a cold place again the droplets disappeared and the color gradually shifted towards the familiar blue
again. Freshly precipated tetammine-Cu-persulphate also forms blue needles. These dont burn very well. After washing with ethanol and heating in a
stream of warm air however a violet powder is obtained which explodes from flame and impact readily.
TACN will decompose in open air into green inert junk when its not completely dry so dont try heating it until its carefully washed with anhydrous
ethanol.
Btw Bisethylenediamine-copper(II)-perchlorate easily precipates from solution when ethanol is added. Its insoluble in ethanol and thus can be obtained
easily in a perfectly dry state. Forms violet needle-shaped crystals and explodes readily from impact however it is slightly hygroscopic.
Slightly off-topic but might be of interest anyways: There is a potassium-chlorate-tartrate double salt which is said to be explosive. I made some of
this by mixing stoichiometric hot solutions of potassium chlorate and potassium tartrate. First little cubes started to crystalize which did not show
any energetic properties - I suppose this was the tartrate alone. Then plate-like crystals appeared which when ignited with a match burned
instantaneously with a little flash. I did not test impact sensitivity tough.
Here's some more double salts you might want to try:
Calcium-acetato-perchlorate: 2/50 mol Ca-acetate are dissolved in 50ccm H2O and 1/50Mol 50% HClO4 is added. The sol is evaporated over H2SO4.
Barium-sodium-acetato-nitrate: 54g Ba-acetate and 34g sodium nitrate are dissolved in 120cc hot H2O and left to evaporate @RT. First Ba(NO3)2 will
crystalize; the double salt forms long prisms and explodes upon heating.
Theres also a lead-sodium-acetato-nitrate double salt which should be easy to prepare: 15,2g lead acetate and 3,4g sodium nitrate are disolved in
80ccm H2O and left to evaporate at RT. The double salt forms small leaflets and cannot be recrystallized from water w/o decomposition.
|
|
|