Copper Sulfate Production


I set up an electrolytic cell with a copper anode (-) and carbon cathode (+) in a concentrated solution of MgSO4. I'm using DC power source and running about 8V with 2amps. The reaction seems to work at first, but after a while it forms Cu(OH)2. I don't know if I'm running the cel too long or what. Does anyone know if there i a formula for how long it will take for a reaction to carry out with any given number of volts/amps?
View user's profile View All Posts By User
Arthur Dent
National Hazard
****




Posts: 553
Registered: 22-10-2010
Member Is Offline

Mood: entropic

[*] posted on 6-1-2011 at 15:54


Hi!

Perhaps you might want to lower the voltage a bit (5 or 6v), are both of your electrodes releasing gas? If so, your voltage might be too high. Only the negative electrode should bubble.

Robert


[Edited on 7-1-2011 by Arthur Dent]




--- Art is making something out of nothing and selling it. - Frank Zappa ---
View user's profile View All Posts By User
violet sin
International Hazard
*****




Posts: 1483
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline

Mood: Good

[*] posted on 7-9-2012 at 01:35


how well does this method work? I have made a lot of copper hydroxide on purpose, and while experimenting with electrode metals, sizes and spacing. ( before I found this site). with all the batches of hydroxide, I never got a single copper sulfate grain left at the bottom of any of my cells. epsom salt, magnesium hydroxide, copper hydroxide, Cu oxides and tap water scum, sure, but not copper sulfate.

I was running a hacked 230W ATX power supply, and switched off between the 5V, 6A and the 12V, 18A hots w/ common ground (eventually stuck w/ 12v). though I am sure it was only operating at a fraction of that. any how I tried CU, Ti, Fe, Ta and C electrodes for the cell(s), and milk jugs cut in half for containers. up to 3 in a series chain. parallel worked less favorably for me.

I was mainly interested in the Cu(OH)2 for decomp to oxide for colored flames in my copper coil alcohol burner i had just made. ( looked awesome btw) but after I realized that the epsom salt was magnesium sulfate( duh, I know right? ) I tried to intentionally make the copper salt. so if this works I have a big pile of copper and I love blue, my fave color.

do you think with my current power supply I could do that? or would I need to wire one up tailored to a specific voltage/amperage range like listed above?
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8078
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 7-9-2012 at 02:19


It is obvious that this method does not give CuSO4.

At the anode, there is formation of Cu(2+) ions. At the cathode, hydrogen is formed and hydroxide ions. The reaction at the cathode is:

2H2O + 2e --> 2OH(-) + H2

The H2 escapes as gas, the OH(-) ions mostly will react with Mg(2+) to form sparingly soluble Mg(OH)2 and if this comes in contact with the copper ions, then insoluble Cu(OH)2 is formed. Your solution will become turbid soon after starting the electrolysis process.

If you really want a good product, then you need dilute H2SO4. At the cathode, H(+) ions are consumed and at the anode, Cu(2+) ions are formed. There is one complication though. At increasing concentration of Cu(2+) ions, more and more of a side reaction occurs at the cathode, where Cu(2+) will be converted to Cu-metal.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 7-9-2012 at 05:16


Or, you could just use two cells for your electrolysis... Copper anode, random cathode, anolyte concentrated epsom salt, catholyte something conductive.



Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8078
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 7-9-2012 at 08:35


Two cells does not solve the problem. It is just a series connection of two cells and each of the cells behaves exactly as if they were one cell. The piece of metal, which connects the two cells acts as anode in the cell, which is connected to the power supply cathode (negative pole) and it acts as cathode in the cell, which is connected to the power supply anode (positive pole).

A true solution is either a cell with a permeable membrane between anode liquid and cathode liquid, or a solution bridge between two cells. One could make a cell with dilute H2SO4 and the other with Na2SO4 and have a bridge between the cells with dilute H2SO4 in it. Such a cell would do the job for quite a long time.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
zed
International Hazard
*****




Posts: 2285
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 12-9-2012 at 12:11


Yup. Probably have to use Sulfuric Acid.

I don't do it that way myself, 'cause I have more Copper Sulfate than I will probably ever use.

I just went up to Home Depot, and bought a big jar full of 99.9% Copper Sulfate root killer.

The way I remember it, for 10 to 15 dollars, I got a few pounds.

Comes in handy if you want to do some Copper plating.



[Edited on 12-9-2012 by zed]
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 12-9-2012 at 16:44


woelen: Not a metal bridge. A tissue paper bridge, as to transfer ions and not electrons. Admittedly, if the sulfuric acid produced in the anolyte gets concentrated enough, this will dissolve away, but I think that with a large enough, etched copper cathode this won't happen (as fast).
This will make copper sulfate from Epsom salt, but not very concentrated and, unless you run the electrolysis for a very long time, not very pure.
Better to just buy it.




Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
kilowatt
Hazard to Others
***




Posts: 322
Registered: 11-10-2007
Location: Montana
Member Is Offline

Mood: nitric

[*] posted on 24-9-2012 at 22:30


I've been down that road of electrolysis before and found it much faster and more efficient to start with copper oxide. A solution of hydrochloric acid and 3% hydrogen peroxide will eat copper at an alarming rate, and you can precipitate copper oxide from that chloride solution. It will dissolve much more readily in the acid. Even more quickly (if you have the apparatus to scrub the gas) you can just add sulfuric acid right to the chloride solution and drive off HCl, but you will either have to contend with a little excess sulfuric acid to drive off, or be left with some CuCl2 impurity. I did something like this (actually with CuCl2 that I had made from the precipitated and filtered oxide) with a very slight excess of sulfuric acid once and bubbled the HCl into water, eventually obtaining white anhydrous CuSO4 which naturally rehydrated to blue.