Rust on lab equipment


I just purchased a few second hand labware items this morning and among the stuff I bought were some very nice "Fisher" clamps and round flask stands that were unfortunately heavily corroded.

So I filled a bucket with water and added a bit of HCl and dropped the clamps in. The rusted clamps slowly bubble away and it seems to make a dent in the oxide, however, I was wondering if a phosphoric acid 5% solution (Scale Buster) would be better to rid myself of the rust?

Since this is a fairly dilute hydrochloric acid solution (3 or 4%) that my clamps are in right now, I don't think this will affect the metal itself if I leave them in there for 24H, will it?

Robert

P.S.: I just can't believe that I just bought a Kimax 1000 ml ground glass neck erlenmeyer for 10 bucks! I love that place!


all this for 25$




--- Art is making something out of nothing and selling it. - Frank Zappa ---
View user's profile View All Posts By User
bquirky
Hazard to Others
***




Posts: 316
Registered: 22-10-2008
Location: Perth Western Australia
Member Is Offline

Mood: No Mood

[*] posted on 15-1-2011 at 02:13


Great Score !

I once fell into the trap of trying to remove rust with HCL ... ITS A TRAP!!! :)

those chloride ions relly do get everywhere everything in my work area got corroded and the item i was trying to de rust rusted evan worse :(

ive since found out that oxilic acid is much better for more permanent removal of rust but it takes a while.



[Edited on 15-1-2011 by bquirky]
View user's profile View All Posts By User
Random
International Hazard
*****




Posts: 1021
Registered: 7-5-2010
Location: In ur closet
Member Is Offline

Mood: Energetic

[*] posted on 15-1-2011 at 02:16


I would take them out of HCl and then put them in NaHCO3 solution. Leave them for few hours, if there would be later some visible corrosion, I would use phosphoric acid. It is rust remover actually.
View user's profile View All Posts By User
Arthur Dent
National Hazard
****




Posts: 553
Registered: 22-10-2010
Member Is Offline

Mood: entropic

[*] posted on 15-1-2011 at 07:13


Thanks,

I removed my round flask stand from the HCl this morning. Nothing but clean metal. So as you suggested, I rinsed the clamp and dropped in a solution of sodium bi for 2 hours. Rinsed it again and put the clamp on my hot stove element to dry it out and kind of "anneal" it.

It looks pretty good right now. If the surface rust comes back, i'll try the phosphoric way.

Robert




--- Art is making something out of nothing and selling it. - Frank Zappa ---
View user's profile View All Posts By User
cyanureeves
National Hazard
****




Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline

Mood: No Mood

[*] posted on 15-1-2011 at 07:16


Rust Out works great for derusting and cleaning steel prior to nickel plating. it doesnt take much either and cleans lab glass pretty good too.i think its sodium bisulfite.
View user's profile View All Posts By User
BromicAcid
International Hazard
*****




Posts: 3237
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline

Mood: Rock n' Roll

[*] posted on 15-1-2011 at 09:32


Rubbing the piece with oil afterwords will offer some form of future protection. Many stainless steel cleaners are mainly mineral oil in some kind of light hydrocarbon medium (propane / butane / pentane / etc). The scrubbing removes the rust and the thin layer of mineral oil left protects it.



Shamelessly plugging my attempts at writing fiction: http://www.robvincent.org
View user's profile Visit user's homepage View All Posts By User
bfesser
Resident Wikipedian
*****




Posts: 2114
Registered: 29-1-2008
Member Is Offline

Mood: No Mood

[*] posted on 15-1-2011 at 11:26


Where'd you buy all that, anyway?
View user's profile View All Posts By User
cyanureeves
National Hazard
****




Posts: 744
Registered: 29-8-2010
Location: Mars
Member Is Offline

Mood: No Mood

[*] posted on 15-1-2011 at 11:33


iron out is sodium bisulfate and rust out is phosphoric acid and water. iron out is way cheaper.
View user's profile View All Posts By User
peach
Bon Vivant
*****




Posts: 1428
Registered: 14-11-2008
Member Is Offline

Mood: No Mood

[*] posted on 16-1-2011 at 09:46


I spent a good hour or two dipping all of the parts on my clamp stand, and the clamps (from the 70's or so I expect), in sulphuric, pressure washing them, scrubbed the entire thing with wire wool until it sparkled, then resprayed the base and put some new rubber on the jaws.

Took about one afternoons worth of work with hydrogen chloride before it was looking grubby again.

If you want it to stay sparkling, some clear lacquer might help. But that won't help if you're heating with flames on a regular basis or anything particularly nasty gets spilt on it - solvents / strong acids / bases.




View user's profile View All Posts By User
Arthur Dent
National Hazard
****




Posts: 553
Registered: 22-10-2010
Member Is Offline

Mood: entropic

[*] posted on 16-1-2011 at 10:59


Quote: Originally posted by peach  
If you want it to stay sparkling, some clear lacquer might help. But that won't help if you're heating with flames on a regular basis or anything particularly nasty gets spilt on it - solvents / strong acids / bases.


There are heat-resistant paints, like "Tremclad" matte black BBQ spray paint that could be used, but it is likely to smoke away if submitted to a direct, intense flame.

But then the idea of "galvanizing" the metal with a very fine coat of tin, copper or zinc might be a good idea?

I'm tempted to try to electroplate something on the bare iron... mhhhh....:cool:

Robert




--- Art is making something out of nothing and selling it. - Frank Zappa ---
View user's profile View All Posts By User
peach
Bon Vivant
*****




Posts: 1428
Registered: 14-11-2008
Member Is Offline

Mood: No Mood

[*] posted on 17-1-2011 at 04:34


The eastern manufacturers do that all the time with those dirt cheap routers and radiators - chrome straight onto rusty iron.

You know your scraping the bottom the barrel when the chrome is bubbling and flaking new out of the box.

As I always say though, pay shit all, expect it to look like shit. So long as I can very occasionally cut a hole with the router I got with the flaking chrome and rust underneath, it's fine. I've had a DeWalt DW626 (2300 watts), sold that (to someone in Austrialia) and kept the flaky one (partly because I knew no one else would buy it).

You can indeed get high temperature paint for engine blocks. I think the cans at Halfords go to 400 or 500C, but there's one in the Toolstation catalogue here that goes to 650C. 500mls of Pro-cote, £7.11.

In the spirit of Henry Ford, your colours choices are matt black and matt black. Enjoy them at your leisure. :P

So long as you don't hit the paint directly with the flame, it should be fine.

[Edited on 17-1-2011 by peach]




View user's profile View All Posts By User
food
Hazard to Self
**




Posts: 86
Registered: 4-9-2010
Location: the West
Member Is Offline

Mood: mithering

[*] posted on 22-1-2011 at 08:34


Hi

I picked up a bunch of neglected clamps myself recently. Most are made of Al, but for the ferrous(?) pieces I took the rust off electrolytically in a sodium carbonate bath. This works well. The clamp shown was pulled a little prematurely; as you see the jaw has lost less rust due to poorer conductivity over the hinge.

clamp_0.jpg - 188kB

What I'd like to know about is a magical way to melt away the scabby surfaces on some of the alumini*um pieces.
View user's profile View All Posts By User
peach
Bon Vivant
*****




Posts: 1428
Registered: 14-11-2008
Member Is Offline

Mood: No Mood

[*] posted on 22-1-2011 at 09:37


You could try a dunk in NaOH or KOH to etch the surface off.

I did that with mine, going over them with a pan brush to knock the muck off, then gave them a scrub with wire wool, after copious rinsing with the hose pipe.

Top tip: DO NOT leave unattended. :D

[Edited on 22-1-2011 by peach]




View user's profile View All Posts By User
food
Hazard to Self
**




Posts: 86
Registered: 4-9-2010
Location: the West
Member Is Offline

Mood: mithering

[*] posted on 22-1-2011 at 10:40


I'll trial that when I get back to them. There are pieces in various states of ugliness, only a minority are really pitted.
View user's profile View All Posts By User
Arthur Dent
National Hazard
****




Posts: 553
Registered: 22-10-2010
Member Is Offline

Mood: entropic

[*] posted on 22-1-2011 at 14:42
Go away... rust, and never come back...


@ food: Wow! that's pretty nasty rust!

I bought another batch of old clamps, but they only had traces of rust, and the phosphoric acid wash took care of that in a jiffy.

However, my latest acquisition was this vintage but fully functional Fisher stirrer/hotplate, which had heavy surface rust on on the top. For that situation, I decided to go with some ammonia-based soap and a small brass wire brush.

I was surprised at how effective it got the rust off as you can see, which revealed some battlescars like heavy pitting (this thing must have been used with very corrosive reagents that splashed all over).



Anyway, the top still looks a bit grungy, but it's a hell of a lot better-looking than when I acquired it. Bah, only paid 50 bucks for it and it works like a charm.

Robert




--- Art is making something out of nothing and selling it. - Frank Zappa ---
View user's profile View All Posts By User
Arthur Dent
National Hazard
****




Posts: 553
Registered: 22-10-2010
Member Is Offline

Mood: entropic

[*] posted on 22-1-2011 at 15:18
Go away... rust, and never come back...


@ food: Wow! that's pretty nasty rust!

I bought another batch of old clamps, but they only had traces of rust, and the phosphoric acid wash took care of that in a jiffy.

However, my latest acquisition was this vintage but fully functional Fisher stirrer/hotplate, which had heavy surface rust on on the top. For that situation, I decided to go with some ammonia-based soap and a small brass wire brush.

I was surprised at how effective it got the rust off as you can see, which revealed some battlescars like heavy pitting (this thing must have been used with very corrosive reagents that splashed all over).



Anyway, the top still looks a bit grungy, but it's a hell of a lot better-looking than when I acquired it. Bah, only paid 50 bucks for it and it works like a charm.

Robert




--- Art is making something out of nothing and selling it. - Frank Zappa ---
View user's profile View All Posts By User
food
Hazard to Self
**




Posts: 86
Registered: 4-9-2010
Location: the West
Member Is Offline

Mood: mithering

[*] posted on 23-1-2011 at 12:54


Nice. I picked up a used hotplate stirrer myself and the novelty still hasn't worn off. Right now I need to load it up with a flask of malt extract to build up a starter for a beer. It's the right tool for that job as well.

Where the electrolytic cleaning fell down was on the chains on some of the clamps. I may yet see if stitching a bare wire through the links isn't too much aggravation. Otherwise I'll could try the phosporic acid if I can dig any up.
View user's profile View All Posts By User
digitalemu
Harmless
*




Posts: 38
Registered: 21-10-2010
Member Is Offline

Mood: No Mood

[*] posted on 24-5-2011 at 12:10


Oxalic acid works great for rust removal.
View user's profile View All Posts By User
redox
Hazard to Others
***




Posts: 268
Registered: 22-2-2011
Location: The Land of Milk and Honey
Member Is Offline

Mood: Chalcogenetic

[*] posted on 25-5-2011 at 15:22


After you etching bath, use WD-40! WD-40 covers the metal in an oily layer that prevents rust. I cover all my metalware in it, it works like a charm :D



My quite small but growing Youtube Channel: http://www.youtube.com/user/RealChemLabs

Newest video: Synthesis of Chloroform

The difference between chemists and chemical engineers: Chemists use test tubes, chemical engineers use buckets.
View user's profile Visit user's homepage View All Posts By User
azo
Hazard to Others
***




Posts: 163
Registered: 12-2-2008
Member Is Offline

Mood: No Mood

[*] posted on 25-5-2011 at 19:44


85% phosporic acid will clean up rust but the surface will turn black.
Then it would need buffing.

painting with red oxide kills rust , that is why they call it kill rust.

regards azo