Daniell cell secondary?


This is something that's been bugging me to the point where I've looked, found nothing and I have to ask.
Back to the basic Zn-Cu cell and all the explanations on how it produces current flow while the redox reactions occur - fine.

But what stands in the way of it being electrically rechargeable?

There must be a crucial piece of theory here that I'm completely missing.




We salute the improvement of the human genome by honoring those who remove themselves from it.
Of necessity, this honor is generally bestowed posthumously. - www.darwinawards.com
View user's profile View All Posts By User
bquirky
Hazard to Others
***




Posts: 316
Registered: 22-10-2008
Location: Perth Western Australia
Member Is Offline

Mood: No Mood

[*] posted on 19-1-2011 at 03:44


Nothing.

They are rechargeable

But what happens over time is that the zinc electrode changes shape and looses structural integrity

Ive built one and cycled it about 20 times.

I found that the mossy bits of zinc fall down from the electrodes into the Copper sulfate and turn back in to Cu and Zinc Sulfate



[Edited on 19-1-2011 by bquirky]
View user's profile View All Posts By User
froot
Hazard to Others
***




Posts: 347
Registered: 23-10-2003
Location: South Africa
Member Is Offline

Mood: refluxed

[*] posted on 19-1-2011 at 04:44


Fantastic. That was the only answer that made sense to me, thanks.

How did it perform? In terms of internal resistance, self discharge, comparative amount of energy it stored?

[Edited on 19-1-2011 by froot]




We salute the improvement of the human genome by honoring those who remove themselves from it.
Of necessity, this honor is generally bestowed posthumously. - www.darwinawards.com
View user's profile View All Posts By User
bquirky
Hazard to Others
***




Posts: 316
Registered: 22-10-2008
Location: Perth Western Australia
Member Is Offline

Mood: No Mood

[*] posted on 19-1-2011 at 05:20


yeah the internal resistance was quite high.

It put out about 100ma but it supplied that for hours and hours on end

oh and i made it in a 200ml beaker to give you some idea of size

[Edited on 19-1-2011 by bquirky]
View user's profile View All Posts By User
froot
Hazard to Others
***




Posts: 347
Registered: 23-10-2003
Location: South Africa
Member Is Offline

Mood: refluxed

[*] posted on 19-1-2011 at 07:14


Great, thanks.



We salute the improvement of the human genome by honoring those who remove themselves from it.
Of necessity, this honor is generally bestowed posthumously. - www.darwinawards.com
View user's profile View All Posts By User

  Go To Top