Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Aluminum Powder of Specific Sizes
MineMan
International Hazard
*****




Posts: 1049
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 14-3-2020 at 13:45
Aluminum Powder of Specific Sizes


Hello fellow scientist!

I am working on an independent study for the University and I need to acquire spherical aluminum powder in the following size ranges... I can’t find any suppliers other than China... which I do not completely trust, or US nano, which is around $.50 cents a gram. I need a kilogram or two of the following sizes.

10um-15um
40-50um
100um

Any ideas? It cannot be flake, it must be spherical so milling is out of the question, as far as sieving... I believe it would take too long and I would need to start with 3-5x the amount of material needed.

Where can I acquire these specific sizes?
View user's profile View All Posts By User
Dr.Bob
International Hazard
*****




Posts: 2910
Registered: 26-1-2011
Location: USA - NC
Member Is Offline

Mood: Mildly disgruntled scientist

[*] posted on 14-3-2020 at 14:10


Check in the energetics thread, they might know better. Technically can't buy more than a pound per year as per ATF rules... So it will be hard to find.
View user's profile View All Posts By User
anti
Harmless
*




Posts: 32
Registered: 17-2-2020
Member Is Offline

Mood: Mood: Mood:

[*] posted on 14-3-2020 at 14:16


Hello! A company in my country sells what you want. Tho I don't know what it would cost them to ship to you and if they would.( I haven't ordered anything from them)
This is the catalog they sent me when I asked.
Use Google Translate's document processor.
(They sent it via email, it is 10 MB so I have uploaded it to filedropper)
http://www.filedropper.com/catalogpulberi2020

Hope you will get what you want
Regards
Edit: I can't vouch for them, as I never ordered anything.
They have every imaginable metal powder(1u aluminium for 100$ a killo??? 20u magnesium? Lead powder? 7u tungsten ???? )

[Edited on 14-3-2020 by anti]

[Edited on 15-3-2020 by anti]
View user's profile View All Posts By User
Deathunter88
National Hazard
****




Posts: 570
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline

Mood: No Mood

[*] posted on 15-3-2020 at 00:23


Look at firework hobbyist sites, here are a few:
https://www.skylighter.com/collections/metals?page=1
https://fireworkscookbook.com/product-category/metals/page/4...

To convert mesh to micron:
https://www.skylighter.com/blogs/fireworks-information/mesh-...
View user's profile View All Posts By User
MineMan
International Hazard
*****




Posts: 1049
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 17-3-2020 at 23:53


I did. They don’t have those sizes. Oh well.
View user's profile View All Posts By User
Deathunter88
National Hazard
****




Posts: 570
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline

Mood: No Mood

[*] posted on 18-3-2020 at 00:44


Quote: Originally posted by MineMan  
I did. They don’t have those sizes. Oh well.


You clearly didn't look very hard

9 micron https://www.skylighter.com/collections/metals/products/alumi...

44 micron
https://fireworkscookbook.com/product/aluminum-atomized-sphe...

100 micron is course enough to sift out with a screen from this
https://fireworkscookbook.com/product/aluminum-atomized-alco...
View user's profile View All Posts By User
MineMan
International Hazard
*****




Posts: 1049
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 18-3-2020 at 23:38


Quote: Originally posted by Deathunter88  
Quote: Originally posted by MineMan  
I did. They don’t have those sizes. Oh well.


You clearly didn't look very hard

9 micron https://www.skylighter.com/collections/metals/products/alumi...

44 micron
https://fireworkscookbook.com/product/aluminum-atomized-sphe...

100 micron is course enough to sift out with a screen from this
https://fireworkscookbook.com/product/aluminum-atomized-alco...


Yes, I looked at these before posting... as someone who makes sarcastic T shit designs, I will be the first to say... take it easy on the sarcasm bruh...

Yes, it would take to much of a quantity, and sieving large amounts of a flammable neurotoxic is outside of my willingness for good health.
View user's profile View All Posts By User
ShotBored
Hazard to Others
***




Posts: 124
Registered: 19-5-2017
Location: Germany
Member Is Offline

Mood: No Mood

[*] posted on 19-3-2020 at 10:50


Quote: Originally posted by MineMan  
Hello fellow scientist!

I am working on an independent study for the University and I need to acquire spherical aluminum powder in the following size ranges... I can’t find any suppliers other than China... which I do not completely trust, or US nano, which is around $.50 cents a gram. I need a kilogram or two of the following sizes.

10um-15um
40-50um
100um

Any ideas? It cannot be flake, it must be spherical so milling is out of the question, as far as sieving... I believe it would take too long and I would need to start with 3-5x the amount of material needed.

Where can I acquire these specific sizes?


Hey MineMan. I get aluminum from Toyal that is of pretty high quality. They have flake atomized as well as spherical/spheroidal. http://www.toyala.com/cgi-bin/r.cgi/powders_spherical_aero.h...

A Spanisch colleague of mine gets powdered metals from a company I can't really remember the name of for sure...I thinks it is Jengo or Jango or something. They are European. Hope this helps, Tchuess!
View user's profile View All Posts By User
MineMan
International Hazard
*****




Posts: 1049
Registered: 29-3-2015
Member Is Offline

Mood: No Mood

[*] posted on 24-3-2020 at 20:03


Quote: Originally posted by ShotBored  
Quote: Originally posted by MineMan  
Hello fellow scientist!

I am working on an independent study for the University and I need to acquire spherical aluminum powder in the following size ranges... I can’t find any suppliers other than China... which I do not completely trust, or US nano, which is around $.50 cents a gram. I need a kilogram or two of the following sizes.

10um-15um
40-50um
100um

Any ideas? It cannot be flake, it must be spherical so milling is out of the question, as far as sieving... I believe it would take too long and I would need to start with 3-5x the amount of material needed.

Where can I acquire these specific sizes?


Hey MineMan. I get aluminum from Toyal that is of pretty high quality. They have flake atomized as well as spherical/spheroidal. http://www.toyala.com/cgi-bin/r.cgi/powders_spherical_aero.h...

A Spanisch colleague of mine gets powdered metals from a company I can't really remember the name of for sure...I thinks it is Jengo or Jango or something. They are European. Hope this helps, Tchuess!


Cool!

Thank you!
View user's profile View All Posts By User
ordenblitz
Hazard to Others
***




Posts: 259
Registered: 18-7-2004
Location: Northwest
Member Is Offline

Mood: Bohr'd

[*] posted on 24-3-2020 at 21:30


Quote: Originally posted by ShotBored  
Quote: Originally posted by MineMan  
Hello fellow scientist!

A Spanisch colleague of mine gets powdered metals from a company I can't really remember the name of for sure...I thinks it is Jengo or Jango or something. They are European. Hope this helps, Tchuess!


It's Jengo in Italy but I doubt they would sell a small quantity to a non commercial entity.
https://jengospa.com/htm/en.html
View user's profile View All Posts By User