[*] posted on 11-7-2021 at 07:04
Cleaning glassware with limited reagents.


I'd like to clean some brown staining out of my sintered glass buchner funnel. It is a result of filtering Muriate of Potash and i'm guessing it is sticky brown clay residue.

I have 50% Sulphuric Acid, 11% Hydrogen Peroxide, Anhydrous Sodium Bisulphate and 20% HCL.

What would be my best bet to make a good cleaning solution?

[Edited on 11-7-2021 by Chemgineer]
View user's profile View All Posts By User
vmelkon
National Hazard
****




Posts: 669
Registered: 25-11-2011
Location: Canada
Member Is Offline

Mood: autoerotic asphyxiation

[*] posted on 11-7-2021 at 08:53


If it is an oxide/hydroxide/carbonate of some transition metal, then H2SO4 or HCl running through it would remove it.
If it is an organic material, you can make a weak piranha solution with your H2SO4 + H2O2 but you say it is some clay.

Sodium bisulfate is just NaHSO4 which is sort of like having H2SO4

Nitric acid would be worth a try. Add some KNO3 to H2SO4 if you don't have clean nitric acid.

You can also try bases, like a solution of NaOH or sodium hypochlorite but these slowly dissolve glass.




Signature ==== Is this my youtube page? https://www.youtube.com/watch?v=tA5PYtul5aU
We must attach the electrodes of knowledge to the nipples of ignorance and give a few good jolts.
Yes my evolutionary friends. We are all homos here.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5142
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 11-7-2021 at 10:24


One of the best things to do is use water, flush it backwards through the funnel.
View user's profile View All Posts By User
Belowzero
Hazard to Others
***




Posts: 187
Registered: 6-5-2020
Location:                 Member Is Offline
Member Is Offline


[*] posted on 12-7-2021 at 03:18


Grillcleaner or a percarbonate, perhaps your wife or gf might have some for you :P
Often with labels as 'oxy action' or 'oxygen cleaner'
Grillcleaners often contain a or multiple hydroxides, they are suprisingly efficient, might corrode glass though.

[Edited on 12-7-2021 by Belowzero]




My new youtube channel, primary focus will be on industrial chemistry: https://www.youtube.com/channel/UCQNj8r14-dyi4mlyenLwnaw/vid...
View user's profile View All Posts By User
Chemgineer
Hazard to Others
***




Posts: 240
Registered: 25-5-2021
Member Is Offline


[*] posted on 12-7-2021 at 05:17


Thanks for the suggestions, I actually have a few cleaning products.... i'm always reading what might be in them in case they are interesting.
View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4738
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: Seeking gainful employment

[*] posted on 12-7-2021 at 05:33


The suggestions are good, but I would also add, I would recommend getting a classic porcelain Büchner funnel and filter papers for doing these sort of filtrations that leave a lot of nasty, hard to clean residue. I’ve mucked about with cleaning glass frits too many times, and eventually realized that I’d much rather be able to just throw the filter paper away instead of trying to figure out how to clean the funnel. I use a frit now only when the precipitate is precious, or if I’m doing something like filtering a solution through a plug of silica gel, because that doesn’t work well in a traditional Büchner funnel (and generally the nasties stay stuck to the silica and don’t make it through to the frit).



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
Fyndium
International Hazard
*****




Posts: 1192
Registered: 12-7-2020
Location: Not in USA
Member Is Offline


[*] posted on 12-7-2021 at 11:46


Organic solvent, acid, base and lots of water usually does the job. Like citric acid, sodium hydroxide, acetone. I've also flushed sodium percarbonate through it by letting it drain by gravity.

Then there's the piranha of course.

For inert particles, backflushing helps. I put some water in the frit and push air through with hand pump backwards. Curtain of bubbles form, and the water helps dislodge solids. Doing all these steps once or twice has gotten my frits shiny white without piranha every time.
View user's profile View All Posts By User
Mateo_swe
National Hazard
****




Posts: 582
Registered: 24-8-2019
Location: Within EU
Member Is Offline


[*] posted on 15-7-2021 at 09:11


I would also recommend a classic porcelain Buchner funnel and filter papers, especially when i know or suspect it will be hard to clean a fritted funnel.
So easy to discard filter paper and easy cleaning, i prefer using them over fritted funnels.
Boiling water, ethanol, acetone, weak acid, sodium hydroxide solution, strong acid, piranha, something usually works.
Dont let sodium hydroxide be in contact with glass for long time as it slowly dissolves glass.
View user's profile View All Posts By User