Distillation apparatus safety hazard?
I recently bought this distillation apparatus and almost all the pieces have bubbles in them. Is this a safety hazard while distilling at elevated
temperatures?

|
|
Mush
International Hazard
   
Posts: 585
Registered: 27-12-2008
Member Is Offline
Mood: No Mood
|
|
I would say yes. Those trapped air pockets can/will expand upon heating or higher temperature eventually causing hairline cracks. If the first
photo of the water inlet than that is problem. Ask for a replace/refund . If you decide to keep it, test carefully it might last for some time before
it brakes and be prepared for failure always.
One ore two small bubbles may be ok. See this post
http://www.sciencemadness.org/talk/viewthread.php?tid=26847
But on your cooler there are way too much on critical points.
[Edited on 17-1-2022 by Mush]
|
|
RustyShackleford
Hazard to Others
 
Posts: 173
Registered: 10-12-2020
Location: Northern Europe
Member Is Offline
|
|
get your money back, thats not ok to use
[Edited on 17-1-2022 by RustyShackleford]
|
|
LeLaborantin
Harmless
Posts: 6
Registered: 25-1-2021
Location: Belgique
Member Is Offline
|
|
In your case and based on the pictures, it is the water inlet or outlet.
You will never have any problems with this...
I have a lot of glassware and this is something common on glassware that is not high end.
But since this part is not in contact with high temperature at all, there is no problem.
But if it is in a distillation flask or on a part in contact with high temperatures, it is not acceptable.
I wish you a good day.