[*] posted on 22-4-2011 at 15:03
Review of methods to make nanoscale powders


Apologies if this is in the wrong forum but can anyone suggest some references that provide a review of the different manufacturing techniques for making nanoscale powders?

I am particularly interested in:
1) Nanoscale reactive powders - e.g. metals, organic compounds
2) Production capacity estimates
3) Figures for cost per gram
4) Comparison of how the production method, capacity and cost increase as you go from micrometric to nanometric powders
5) Methods that have been tried but were unsuccessful

I am new to the field and just want more bedtime reading :)

I've tried searching for "review nano powder manufacture" on Google Scholar but it just turns up methods for making specific powders rather than a more general introduction.
View user's profile View All Posts By User
condennnsa
Hazard to Others
***




Posts: 217
Registered: 20-4-2010
Location: Romania
Member Is Offline

Mood: No Mood

[*] posted on 22-4-2011 at 15:28


I was also wondering about this, more particularly about the possibility of an amateur to make nanopowders by using a planetary ball mill.
Wikipedia says that a high quality ball mill is capable of producing particles as small as 5 nm.

also on the wiki nanoparticle article , : "There are several methods for creating nanoparticles, including both attrition[disambiguation needed] and pyrolysis. In attrition, macro or micro scale particles are ground in a ball mill, a planetary ball mill, or other size reducing mechanism. The resulting particles are air classified to recover nanoparticles"

[Edited on 22-4-2011 by condennnsa]
View user's profile View All Posts By User
Sedit
International Hazard
*****




Posts: 1939
Registered: 23-11-2008
Member Is Offline

Mood: Manic Expressive

[*] posted on 22-4-2011 at 18:26


Im sorry I can't give much help but perhaps what I remember could give you a hint into the direction to look. I remember reading something.... somewhere.... that spoke of nano scale metal particals being formed thru the precipitation of a metal while using some kind of surfactant to assure that the precipitated metal powders did not conglomerate into larger clusters.

I may have even posted the paper somewhere here but im sorry that my memory fails me quite often as of late. Its quite possible in the defunct ORMUS thread from a few years ago but im not sure.





Knowledge is useless to useless people...

"I see a lot of patterns in our behavior as a nation that parallel a lot of other historical processes. The fall of Rome, the fall of Germany — the fall of the ruling country, the people who think they can do whatever they want without anybody else's consent. I've seen this story before."~Maynard James Keenan
View user's profile View All Posts By User
IndependentBoffin
Hazard to Others
***




Posts: 150
Registered: 15-4-2011
Member Is Offline

Mood: No Mood

[*] posted on 22-4-2011 at 22:44


It would have to be in an inert atmosphere if you're going to use a ball mill to make nanoscale powder. Fe, Cu and Ni powder for example spontaneously ignite below around 10 - 30nm, W at 1 micron and Zr and Na at 10 microns, c.f. "Review of Zirconium-Zircaloy Pyrophoricity," Cooper, T. D. (1984) that is attached. Anything in the nanometer range will probably react so quickly it is liable to explode if there are large quantities of it.

It would be interesting to see if there is a graph of ball mill run time and the statistical particle size distribution. It seems to me that there would be, say, a normal distribution of particle sizes. Particles in the nm range would probably be at the tail end of the normal distribution. Running the ball mill in anything but an inert atmosphere (nitrogen and CO2 probably don't count - you need a noble gas) will probably cause the immediate oxidation of nanometric reactive particles.



Attachment: review_zirconium_zircaloy_pyrophoricity.pdf (953kB)
This file has been downloaded 1273 times

View user's profile View All Posts By User
Sedit
International Hazard
*****




Posts: 1939
Registered: 23-11-2008
Member Is Offline

Mood: Manic Expressive

[*] posted on 22-4-2011 at 23:58


I would be shocked if anything produced in a ball mill would be considered Nano but I could be wrong. I would look more into precipitated metals more then anything. With the right ligin the are able to reach increadibly small scale particals muc smaller then a ball mill could ever achieve,




Knowledge is useless to useless people...

"I see a lot of patterns in our behavior as a nation that parallel a lot of other historical processes. The fall of Rome, the fall of Germany — the fall of the ruling country, the people who think they can do whatever they want without anybody else's consent. I've seen this story before."~Maynard James Keenan
View user's profile View All Posts By User
condennnsa
Hazard to Others
***




Posts: 217
Registered: 20-4-2010
Location: Romania
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2011 at 00:26


Here's an interesting article I found dealing with this:

http://cbe.tulane.edu/faculty/mitchell/JournalArticles/Nanop...

[Edited on 23-4-2011 by condennnsa]
View user's profile View All Posts By User
IndependentBoffin
Hazard to Others
***




Posts: 150
Registered: 15-4-2011
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2011 at 00:33


Thank you, I am reading it now :)

I do recall a method of making nanoscale powders that involved sending an electric pulse through a wire suspended in an inert gas. The wire vapourises and nanoscale powder is produced.

Obviously not an ideal method if you want kgs of the stuff!
View user's profile View All Posts By User
condennnsa
Hazard to Others
***




Posts: 217
Registered: 20-4-2010
Location: Romania
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2011 at 01:03


Yeah, it's really interesting, as it points out that these high energy mills are well capable of going all the way to nano. The major issue is the contamination.
Look at the graph where they milled aluminum powder to test contamination.
With stainless steel jar and media the %SS in the powder was 0.5% after 100 minutes and 1.5% after 1000.
While by using tungsten carbide jar and media contamination was 5% after 100min and a wobbling 35% after 1000! . It seems that harder isn't always better, as the WC really likes to chew itself up.

I've been checking out prices of these machines and it seems they go from $2000 and up :(.

But they shouldn't be too hard to build , the hardest part would be the planetary gear system, for which a machine shop is a must.

Some more stuff I found online:
They make 39-96 nm Al-Cu particles :

Attachment: 0312223627.pdf (271kB)
This file has been downloaded 616 times

An excellent paper with lots of graphs and pictures, making nanoparticles for use in nanofluids:
http://ethesis.nitrkl.ac.in/192/1/final_report.pdf

[Edited on 23-4-2011 by condennnsa]
View user's profile View All Posts By User
IndependentBoffin
Hazard to Others
***




Posts: 150
Registered: 15-4-2011
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2011 at 02:03


I have access to a few machine shops that can do contract work. Their rates are £25/hour for manual operated machines and £35/hour for CNC work. Sorry I can't do it for free as they are subcontractors to me and I have to pass on the costs.

I have a few questions after reading your reference:
1) Does the microstructure of the metal to be nanonised (c.f. micronised) start with make a difference? E.g. a temper-quench specimen with a very fine grain structure vs. a wholly annealed specimen with a large grain structure?

2) In the oxide dispersion strengthened alloys described on Pg 2, does the manufacture process involve a sintering or hot isotactic pressing phase to consolidate the powder?

3) On Pg 4 Figure 3, what is the cause of the initial rise in milling time as particle size increases? I would have thought that particle size is always inversely proportional to milling time.

4) WC probably contaminates the product more than stainless steel because it has a lower toughness. At the point of impact the stresses probably exceed the elastic limit of most materials and the impact energy must be dissipated by surface energy (crushing/cracking and opening up new surfaces), plastic deformation (lacking in WC - hence cracking dominates), elastic waves (vibrations, noise) and heat.

[Edited on 23-4-2011 by IndependentBoffin]
View user's profile View All Posts By User
condennnsa
Hazard to Others
***




Posts: 217
Registered: 20-4-2010
Location: Romania
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2011 at 02:32


Well this is just off the top of my head, after all, everything I know about this is what I've read here and there on the web.
1) I figure that a quenched metal would decrease more rapidly in size in the first period of the milling time, because it will fracture by breaking apart. While an annealed piece, being softer and more ductile, would have to be bent over and over, which will cause it to eventually break apart to smaller pieces, so I figure that it will decrease in size more slowly.
2) I don't know:) I guess so.
3) Well I'm as surpised as you, and I didn't notice that myself.
I really don't have an explanation. Maybe it has to do with figure 2 on page 3, some kind of agglomeration effect. I think this is also related to the material ductility, as until the particles acquire sufficient fatigue in order to break apart, they can agglomerate. Therefore, I would not expect such a graph for brittle materials.


energy_ballmill.bmp - 995kB

Here is a contraption I've come up with for a high energy ball mill design which does not use planetary gears.
Hope my paint sketch is clear enough, it's basically a system which allows to rotate the jar while eliminating its movement of revolution, thus creating high centrifugal forces on the walls. Its actually the same as a planetary system, but less efficient since in a planetary mill the rotating and revolving directions are actually opposite.

[Edited on 23-4-2011 by condennnsa]

[Edited on 23-4-2011 by condennnsa]
View user's profile View All Posts By User
IndependentBoffin
Hazard to Others
***




Posts: 150
Registered: 15-4-2011
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2011 at 03:28


Nice idea, but I don't think it will last very long from the off-axis forces. There are just so many points of mechanical failure: bending of your rods, widening of the holes on the plate, cutting through of the rods by the plates, etc. Imagine spinning that at 300 RPM!

Also the structure is fairly complex from a dynamic point of view. There are many possible modes of vibration and we can not guarantee that from your operating RPMs no modes at all will be excited to resonance. Unless you make the parts out of very stiff materials (natural frequency is proportional to sqrt(E/density)) you would certainly get low frequency resonant modes.

The advantages of the planetary ball mill is that the components are structurally strong and simple. Therefore they are easy to keep from being stressed excessively and the design kept away any resonant modes of vibration.

Frankly I do not think it will cost USD$2000 to build your own planetary ball mill professionally if you pay a workshop to do it. Say 1 day's work (8h @ USD$25 = USD$200), scavenged motorcycle or car engine (you can buy very old ones second hand cars for say USD$300 and other parts USD$500 at most. So it would come up to about USD$1000 and I am being very generous on the figures here. A CNC machine will cut out the gear teeth in no time (like 1h @ USD$35), I've seen really old Fords on sale for USD$50 and you can ask for off-cut stainless steel from steel stockholders. If you're lucky and shrewd about things you can get everything done for USD$500, I think.
View user's profile View All Posts By User
condennnsa
Hazard to Others
***




Posts: 217
Registered: 20-4-2010
Location: Romania
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2011 at 03:45


Yeah you're right, it was only a sketch though to illustrate the mechanism.

With some math and adjustable counterweights i think it could be made to work... like so

I am really tempted to try to build something like this, to see how it'd work for blackpowder. I remember reading somewhere that high energy mills decrease the mill time for BP by an order of magnitude compared to conventional ball milling.

energy_ballmill2.bmp - 995kB


[Edited on 23-4-2011 by condennnsa]
View user's profile View All Posts By User
IndependentBoffin
Hazard to Others
***




Posts: 150
Registered: 15-4-2011
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2011 at 04:20


Quote: Originally posted by condennnsa  
Yeah you're right, it was only a sketch though to illustrate the mechanism.

With some math and adjustable counterweights i think it could be made to work... like so

I am really tempted to try to build something like this, to see how it'd work for blackpowder. I remember reading somewhere that high energy mills decrease the mill time for BP by an order of magnitude compared to conventional ball milling.



Yes this is starting to be more promising :D. You could even mount another jar symetrically so that the off-axis forces cancel out.

Why do you need a ball mill to make black powder? You can already get saltpetre and sulphur in powder form.

Charcoal powder can be bought off Ebay or you can try activated charcoal for water filtration. I think even a plain ball mill will be enough to break up the activated charcoal to a fine enough powder.
View user's profile View All Posts By User
watson.fawkes
International Hazard
*****




Posts: 2793
Registered: 16-8-2008
Member Is Offline

Mood: No Mood

[*] posted on 23-4-2011 at 07:21


Quote: Originally posted by IndependentBoffin  
Frankly I do not think it will cost USD$2000 to build your own planetary ball mill professionally if you pay a workshop to do it. Say 1 day's work (8h @ USD$25 = USD$200), scavenged motorcycle or car engine (you can buy very old ones second hand cars for say USD$300 and other parts USD$500 at most.
If you're looking to scavenge parts, there are planetary gear systems in automatic transmissions.
View user's profile View All Posts By User
497
National Hazard
****




Posts: 778
Registered: 6-10-2007
Member Is Offline

Mood: HSbF6

[*] posted on 27-8-2011 at 21:10


You forgot plasma, which is one of the most promising possibilities in my opinion. I really dig the no moving parts possibility.

www.kona.or.jp/search/25_039.pdf
http://www.sciencedirect.com/science/article/pii/S0167577X05...
joam.inoe.ro/download.php?idu=2355
http://www.springerlink.com/content/k41432716r85416v/
US patent 6689192

I'm curious to see if (possibly pyrophoric) nanopowders could be useful for sensitizing hydrocarbons used for FAE purposes. Potentially you could even make a single event FAE with pyrophoric nanopowders, and the delay could be tuned by adjusting the size and/or concentration of the nanopowder.
I have searched and come up with nothing about nanomaterials in FAEs. Maybe it's all classified?

[Edited on 28-8-2011 by 497]




A word to the wise: NEUROFEEDBACK

http://citizenworks.org/corp/dg/s2r1.pdf
http://www.newscientist.com/mobile/article/mg21228354.500-re...
http://www.shadowstats.com/article/no-414-hyperinflation-spe...

"To expose a 15 Trillion dollar ripoff of the American people by the stockholders of the 1000 largest corporations over the last 100 years will be a tall order of business."
Buckminster Fuller

"No problem can be solved from the same level of consciousness that created it."
Albert Einstein
View user's profile View All Posts By User
HellstormOP
Hazard to Self
**




Posts: 75
Registered: 13-8-2011
Member Is Offline

Mood: No Mood

[*] posted on 27-8-2011 at 23:55


Regarding planetary ball mills, I have good news. Together with one of my friends, who has a machine shop, I'm already working on one. The material is mostly purchased, the major part of the sketches is made, we also have blueprints of some parts. Our system won't need big gears, we will use smaller gears, connected by a drive belt and held in place by an aluminium bar. The jar will be fixed on both sides instead of only one, to increase the stability. I think we should be able to finish it within about 1.5 months. I also will upload some of the sketches I made for it as soon as I can.

[Edited on 28-8-2011 by HellstormOP]
View user's profile View All Posts By User
jimwig
Hazard to Others
***




Posts: 215
Registered: 17-5-2003
Location: the sunny south
Member Is Offline

Mood: No Mood

[*] posted on 29-8-2011 at 08:20
patents


seems like the patents might give some sort of direction

but the term dynamic gas-phase condensation method pops out right away.... as mentioned previously grinding just doesn't seem to approach the magnitude of production.

[Edited on 29-8-2011 by jimwig]




craZy jiM wGGns

--packrat, professional bum. -- once just tired
now REtired.
View user's profile View All Posts By User
Bot0nist
International Hazard
*****




Posts: 1559
Registered: 15-2-2011
Location: Right behind you.
Member Is Offline

Mood: Streching my cotyledons.

[*] posted on 30-8-2011 at 06:52


Quote: Originally posted by IndependentBoffin  

Why do you need a ball mill to make black powder? You can already get saltpetre and sulphur in powder form.

Charcoal powder can be bought off Ebay or you can try activated charcoal for water filtration. I think even a plain ball mill will be enough to break up the activated charcoal to a fine enough powder.


Just mixing finely divided carbon sulfur, and KNO<sub>3</sub> will not make a good black powder. It is necessary to ball mill, or at least pulverize in a mortar and pedestal for long hours to get individual particles of sulfur and oxidizer to become impregnated in the pores of the carbon.

[Edited on 30-8-2011 by Bot0nist]




U.T.F.S.E. and learn the joys of autodidacticism!


Don't judge each day only by the harvest you reap, but also by the seeds you sow.
View user's profile View All Posts By User
AndersHoveland
Hazard to Other Members, due to repeated speculation and posting of untested highly dangerous procedures!
*****




Posts: 1986
Registered: 2-3-2011
Member Is Offline

Mood: No Mood

[*] posted on 30-8-2011 at 07:00


Quote: Originally posted by Bot0nist  
Just mixing finely divided carbon sulfur, and KNO<sub>3</sub> will not make a good black powder. It is necessary to ball mill, or at least pulverize in a mortar and pedestal for long hours to get individual particles of sulfur and oxidizer to become impregnated in the pores of the carbon.


It needs to be soaked in water, then dried. This is so that microcrystals of KNO3 can form around the particles of charcoal. If it is not soaked in water, it will be difficult to get the composition to explode.




I'm not saying let's go kill all the stupid people...I'm just saying lets remove all the warning labels and let the problem sort itself out.