Hello Everyone,

I've encountered an interesting (at least for me) phenomenon: stainless steel became stained (covered in some sort of whitish layer) after prolonged exposure to hot, Na2CO3 containing tap water and oxygen from air.
At first I thought "ah, it is simple, just CaCO3 precipitate formed and it should be easy to remove it by acetic- or citric-acid!"
Wrong! This layer does not seem to react with these acids! It sticks to the steel very hard. Previously it was a highly glossy surface, now it is dull, as if it was covered by a thin layer of flour.

I run a few Google searches but could not come up with anything meaningful. If it is indeed CaCO3 precipitate then what causes its inertness towards acids?


View user's profile View All Posts By User
metalresearcher
National Hazard
****




Posts: 822
Registered: 7-9-2010
Member Is Offline

Mood: Reactive

[*] posted on 9-10-2025 at 09:34


The only thing I might guess is Al2O3 which is stubborn.
But did you use any aluminum foil or sheet with the heating ?
Ca and Mg salts should dissolve in acids.
View user's profile View All Posts By User
Pumukli
National Hazard
****




Posts: 724
Registered: 2-3-2014
Location: EU
Member Is Offline

Mood: No Mood

[*] posted on 9-10-2025 at 10:27


Thanks for the hint, metalresearcher!

Aluminum hmm. I did not check the system so thoroughly but it is something worth considering.
Maybe there is somewhere an aluminum part, a pipe or something that gets in contact with the highly alkaline water (pH is around 11, maybe reaches 12 at times) and slowly gets dissolved as hydroxo-complex. Then the complex reacts not with O2 but with CO2 from air and gets converted into Al2O3.

Anyway, do anyone know a good, reliable way to dissolve Al2O3? I may try NaF, as I remember, Al3+ makes strong complex with fluoride.
View user's profile View All Posts By User
pneumatician
Hazard to Others
***




Posts: 416
Registered: 27-5-2013
Location: Magonia
Member Is Offline

Mood: ■■■■■■■■■■ INRI ■■■■■■■■■■ ** Igne Natura Renovatur Integra **

[*] posted on 11-10-2025 at 16:23


many inox cookware have a last layer of Al to get a wonderfull Alzehimer, thanks to the pigs. :)