Megamarko94
Hazard to Self
Posts: 68
Registered: 31-12-2010
Member Is Offline
Mood: No Mood
|
|
Gold salts synthesis, and other precious metal salts.
if you have any gold salt synthesis pls. post it...or any other precious metal salt.....
|
|
LanthanumK
Hazard to Others
Posts: 298
Registered: 20-5-2011
Location: New Jersey
Member Is Offline
Mood: No Mood
|
|
The dissolution of gold and palladium in aqua regia is well known. Platinum also dissolves. All of these form precious metal compounds, although I am
not sure whether they are known as salts.
|
|
cyanureeves
National Hazard
Posts: 737
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
silver nitrate is simply made by dissolving silver in nitric acid. sterling in nitric acid will make a contaminated silver nitrate solution that can
be turned into silver chloride by adding table salt to it. or use a pure silver nitrate solution if you have pure silver.electrolyzing gold in
potassium cyanate will make a gold solution but i've never went as far as evaporating the solution to see what the salt will look like. if you
evaporate gold chloride it will turn syrupy and i dont see why it wouldnt make a salt if further dried.to make the cyanate or cyanide synthesis go to
the preparation of cyanide thread. that is as preciously as i've gone. i've never even touched platinum.
|
|
Neil
National Hazard
Posts: 556
Registered: 19-3-2008
Member Is Offline
Mood: No Mood
|
|
The Chemistry of Gold
M. ConcepciĆ³n Gimeno