Mark Van Adium
Harmless
Posts: 18
Registered: 26-11-2010
Member Is Offline
Mood: No Mood
|
|
Using a microwave to dry silica gel.
Does this work well, it certainly gets hot, I'm just wondering how well aired it needs to be (is a pot ok or does it need to be on a plate?) and if it
getting hot is directly correlated to it drying out.
Anyone have any experience?
|
|
blogfast25
International Hazard
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Use large enough quantities (MWs don’t like running on empty).
A non-UHF-absorbing PP dish or shallow pot is probably best.
Use fairly short bursts: 1 minute or so (on ‘high’), check temp., another minute etc, to avoid overheating.
Once at desired temperature, use low power to hold it there.
Check progress by weighing up the sample several times: constant weight would indicate water loss is complete.
And no: I have no experience with it and may well be talking through my other orifice. Worth experimenting with but make sure you clean the MW prior
to food use.
|
|
IndependentBoffin
Hazard to Others
Posts: 150
Registered: 15-4-2011
Member Is Offline
Mood: No Mood
|
|
I once accidentally had my oven at 220C when drying silica gel, because I was previously using it to dry some calcium sulphate.
The indicator silica gel got charred, with the top layer on the tray looking black-ish.
Hotspots on microwaves are definitely a possibility. I'd stick to using an oven at 120C.
http://www.envirogel.co.uk/improving_silica_gel_reactivation...
I can sell the following:
1) Various high purity non-ferrous metals - Ni, Co, Ta, Zr, Mo, Ti, Nb.
2) Alkex para-aramid Korean Kevlar analogue fabric (about 50% Du Pont's prices)
3) NdFeB magnets
4) High purity technical ceramics
|
|
Panache
International Hazard
Posts: 1290
Registered: 18-10-2007
Member Is Offline
Mood: Instead of being my deliverance, she had a resemblance to a Kat named Frankenstein
|
|
don't run it directly on the glass plate as i shattered mine when drying molecular sieves in the microwave, if you are a good aim, a well positioned
ir thermometer can read temperatures through the microwave grating on the front door. or you could just open the door.
|
|
cyanureeves
National Hazard
Posts: 737
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
i microwaved silica sand with blue indicator crystals used for drying flowers and the fan blew fine dust all over inside my microwave.
|
|
IndependentBoffin
Hazard to Others
Posts: 150
Registered: 15-4-2011
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by cyanureeves | i microwaved silica sand with blue indicator crystals used for drying flowers and the fan blew fine dust all over inside my microwave.
|
http://en.wikipedia.org/wiki/Cobalt#Biological_role
Generally a bad idea to mix cobalt (from the indicator) with food...
Quote: |
After nickel and chromium, cobalt is a major cause of contact dermatitis and is considered carcinogenic. In 1966, the addition of cobalt compounds to
stabilize beer foam in Canada led to cardiomyopathy, which came to be known as beer drinker's cardiomyopathy. |
I can sell the following:
1) Various high purity non-ferrous metals - Ni, Co, Ta, Zr, Mo, Ti, Nb.
2) Alkex para-aramid Korean Kevlar analogue fabric (about 50% Du Pont's prices)
3) NdFeB magnets
4) High purity technical ceramics
|
|
LanthanumK
Hazard to Others
Posts: 298
Registered: 20-5-2011
Location: New Jersey
Member Is Offline
Mood: No Mood
|
|
If the indicator was blue, why would you microwave it?
hibernating...
|
|
Saerynide
National Hazard
Posts: 954
Registered: 17-11-2003
Location: The Void
Member Is Offline
Mood: Ionic
|
|
Put it in the oven on a cookie sheet at 250-275F and bake. I usually leave it for 30-45 min. Comes out dry enough that if i run my hands through it,
I can feel my skin dry out and I have to grab the lotion
"Microsoft reserves the right at all times to monitor communications on the Service and disclose any information Microsoft deems necessary to...
satisfy any applicable law, regulation or legal process"
|
|
cyanureeves
National Hazard
Posts: 737
Registered: 29-8-2010
Location: Mars
Member Is Offline
Mood: No Mood
|
|
no the crystals
were always pink. i didnt know they had to be dried until blue.didnt know about cobalt either.
|
|
Finnnicus
Hazard to Others
Posts: 342
Registered: 22-3-2013
Member Is Offline
|
|
I have lots of experience of drying with microwaves. Mind the balls cracking tho, but I highly recommend it!
|
|