I do have a question: If equal parts 68% Nitric Acid and 99.5% anhydrous Ammonia were mixed the resultant Ammonium Nitrate would have a strength of what %?

Thank You




Darryl Paulhus
Greenline Industries
View user's profile View All Posts By User
paulhusd
Harmless
*




Posts: 3
Registered: 14-12-2011
Member Is Offline

Mood: No Mood

[*] posted on 14-12-2011 at 18:45


So you all know I am not trying to make explosives I am part owner in a small fertilizer business in NSW Australia and we are trying to help some farmers out by supplying liquid fertilizers at a better cost.



Darryl Paulhus
Greenline Industries
View user's profile View All Posts By User
hissingnoise
International Hazard
*****




Posts: 3940
Registered: 26-12-2002
Member Is Offline

Mood: Pulverulescent!

[*] posted on 15-12-2011 at 04:17


The reaction of HNO<sub>3</sub> with anhydrous ammonia is quite vigorous.
The hydroxide is preferred in home-synthesis.
NH<sub>4</sub>NO<sub>3</sub> contains ~ 34% nitrogen, appreciably less than urea.
And we excrete urea in urine - nearly an ounce per day . . .


View user's profile View All Posts By User
paulhusd
Harmless
*




Posts: 3
Registered: 14-12-2011
Member Is Offline

Mood: No Mood

[*] posted on 15-12-2011 at 19:17


We are going to be doing this on a commercial scale using a vessel for the reaction. I assume the reaction will create heat likely to raise the fluid to over 140C.



Darryl Paulhus
Greenline Industries
View user's profile View All Posts By User
Bot0nist
International Hazard
*****




Posts: 1559
Registered: 15-2-2011
Location: Right behind you.
Member Is Offline

Mood: Streching my cotyledons.

[*] posted on 15-12-2011 at 19:45


If you have industrial aspirations, perhaps the Haber-Bosch process may be of interest.

http://en.m.wikipedia.org/wiki/NH4NO3
http://en.m.wikipedia.org/wiki/Haber_process

[Edited on 16-12-2011 by Bot0nist]




U.T.F.S.E. and learn the joys of autodidacticism!


Don't judge each day only by the harvest you reap, but also by the seeds you sow.
View user's profile View All Posts By User
Chemistry Alchemist
Hazard to Others
***




Posts: 403
Registered: 2-8-2011
Location: Australia
Member Is Offline

Mood: No Mood

[*] posted on 15-12-2011 at 21:48


HNO3(aq) + NH3(l) → NH4NO3(aq)
(NH4)2SO4 + 2 NaNO3 → Na2SO4 + 2 NH4NO3
Ca(NO3)2 + (NH4)2SO4 → 2 NH4NO3 + CaSO4

Some reactions that produce Ammonium Nitrate (from Wiki)




View user's profile Visit user's homepage View All Posts By User
neptunium
National Hazard
****




Posts: 987
Registered: 12-12-2011
Location: between Uranium and Plutonium
Member Is Offline


[*] posted on 4-1-2012 at 08:35


i`ll go with the Calcium nitrate . no doubt .

twice the NO3- and CaSO4 precipitate out

win win boom !
View user's profile Visit user's homepage View All Posts By User
Pulverulescent
National Hazard
****




Posts: 793
Registered: 31-1-2008
Member Is Offline

Mood: Torn between two monikers ─ "hissingnoise" and the present incarnation!

[*] posted on 4-1-2012 at 09:33


Quote:
i`ll go with the Calcium nitrate . no doubt .
twice the NO3-
win win boom !

The atomic weight of Ca is roughly twice that of Na so they kinda balance out . . .

P

View user's profile View All Posts By User
neptunium
National Hazard
****




Posts: 987
Registered: 12-12-2011
Location: between Uranium and Plutonium
Member Is Offline


[*] posted on 4-1-2012 at 12:33


true
CaSO4 precipitate making a separation easy
View user's profile Visit user's homepage View All Posts By User
neptunium
National Hazard
****




Posts: 987
Registered: 12-12-2011
Location: between Uranium and Plutonium
Member Is Offline


[*] posted on 4-1-2012 at 12:34


true
CaSO4 precipitate making a separation easy
View user's profile Visit user's homepage View All Posts By User
Waffles SS
Fighter
****




Posts: 998
Registered: 7-12-2009
Member Is Offline


[*] posted on 4-1-2012 at 12:37


2 NH3 + 4 O3 → NH4NO3 + 4 O2 + H2O
View user's profile View All Posts By User
Adas
National Hazard
****




Posts: 711
Registered: 21-9-2011
Location: Slovakia
Member Is Offline

Mood: Sensitive to shock and friction

[*] posted on 4-1-2012 at 12:54


Quote: Originally posted by Waffles SS  
2 NH3 + 4 O3 → NH4NO3 + 4 O2 + H2O


Didn't you read they are gonna do it on a large scale?

[Edited on 4-1-2012 by Adas]




Rest In Pieces!
View user's profile Visit user's homepage View All Posts By User
White Yeti
National Hazard
****




Posts: 816
Registered: 20-7-2011
Location: Asperger's spectrum
Member Is Offline

Mood: delocalized

[*] posted on 4-1-2012 at 13:10


Careful!!

HNO<sub>3</sub>(l) + NH<sub>3</sub>(g) → NH<sub>4</sub>NO<sub>3</sub>(s)

This synthesis is not dangerous but it releases lots of heat. It might trigger chain reactions that might lead to disaster if (God forbid) the cooling system were to fail. Watch this:
NH<sub>4</sub>NO<sub>3</sub>(s) ---(heat)----> 2H<sub>2</sub>O (g) + N<sub>2</sub>O(g)

This reaction is actually exothermic (I'm not exactly sure by how much), it is catalysed by the addition of heat, but releases heat overall. According to wikipedia, if the temperature exceeds 240C, uncontrolled decomposition takes place. Notice that the two products are gases, this synthesis could potentially spiral out of control very rapidly.

Urea sounds like a nice alternative, nice and stable :D




"Ja, Kalzium, das ist alles!" -Otto Loewi
View user's profile View All Posts By User
Pulverulescent
National Hazard
****




Posts: 793
Registered: 31-1-2008
Member Is Offline

Mood: Torn between two monikers ─ "hissingnoise" and the present incarnation!

[*] posted on 4-1-2012 at 13:22


Hopefully the OP will take these concerns on board . . .

P
View user's profile View All Posts By User
Poppy
Hazard to Others
***




Posts: 294
Registered: 3-11-2011
Member Is Offline

Mood: † chemical zombie

[*] posted on 4-1-2012 at 15:31


Quote: Originally posted by neptunium  
true
CaSO4 precipitate making a separation easy


Fail. The resulting slurry will have properties much like cement!