Silicon from Silicon dioxide


A while back I researched this intensely with the hopes of finding a possible catalyst for this reaction.

However, I have lost all of my notes and ideas!

I'd like to find the energy profile of SiO2->Si.

Actually I don't know if I even remember how to do this type of thermodynamics. :o

I know that Silicon dioxide at temperatures around >1200° C are mixed with carbon graphite. The reaction goes by
SiO2 + C -> CO2 + Si

It goes through some other steps as well.

I thought perhaps since Si reacts with fluorine so strongly, perhaps fluorine could act as some catalyst at high temps.

At anyrate I thought maybe this could get the ball rolling for some research.
View user's profile View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 31-1-2012 at 08:26


I've made silicon from beach sand via sulfur-boosted thermite, in one of my more popular videos (good choice of tags I guess):

http://www.youtube.co/watch?v=73YmP_JSrlU&feature=relate...

Not very practical for any analytical work I'm sure, but it was fun! I just needed a sample for my element collection, so I'm satisfied.
View user's profile Visit user's homepage View All Posts By User
GreenD
National Hazard
****




Posts: 623
Registered: 30-3-2011
Member Is Offline

Mood: Not really high anymore

[*] posted on 31-1-2012 at 08:35


You do know that silicon is a metalloid, right :D

cool video though.

Maybe industrial scale this could make sense by using all those beer cans./
View user's profile View All Posts By User
Neil
National Hazard
****




Posts: 556
Registered: 19-3-2008
Member Is Offline

Mood: No Mood

[*] posted on 31-1-2012 at 09:31


Check around there are a number of routes already explained on SM. Look for old posts by blogfast.
View user's profile View All Posts By User
Neil
National Hazard
****




Posts: 556
Registered: 19-3-2008
Member Is Offline

Mood: No Mood

[*] posted on 31-1-2012 at 09:31


Check around there are a number of routes already explained on SM. Look for old posts by blogfast.
View user's profile View All Posts By User
Vikascoder
Hazard to Others
***




Posts: 309
Registered: 28-1-2012
Member Is Offline

Mood: No Mood

[*] posted on 4-2-2012 at 01:48


I made silicon by adding sand to 3 micron aluminium powder then igniting it with potassium chlorate and sugar sulphur mix