underground
National Hazard
  
Posts: 719
Registered: 10-10-2013
Location: Europe
Member Is Offline
|
|
Why NG does not used ?
I just always wonderring why nitroguanidine does not used in military as a TNT substitute or watever, as long as it is very storage stabe, insensitive
with high VoD cheap and easy to make!
|
|
|
Pulverulescent
National Hazard
  
Posts: 793
Registered: 31-1-2008
Member Is Offline
Mood: Torn between two monikers ─ "hissingnoise" and the present incarnation!
|
|
The nitramines, RDX and HMX out-perform both TNT and NG . . .
"I know not with what weapons World War III will be fought, but World War IV will be fought with sticks and stones"
A Einstein
|
|
|
Zyklon-A
International Hazard
   
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
Yeah, TNT isn't used as much anymore ether, but TNT had the advantage that it would explode after it went though a building, (propelled by a rocket or
whatever), thus doing much more damage than if it exploded on contact.
Edit: And, even though NG can be stabilized, it's hard to beat the stability and reliability of TNT.
[Edited on 29-1-2014 by Zyklonb]
|
|
|
Hennig Brand
International Hazard
   
Posts: 1284
Registered: 7-6-2009
Member Is Offline
Mood: No Mood
|
|
Actually, TNT is still one of the most commonly used explosives. It is used for military and industrial applications.
From Wikipedia:
"TNT is one of the most commonly used explosives for military and industrial applications. It is valued partly because of its insensitivity to shock
and friction, which reduces the risk of accidental detonation, compared to other more sensitive high explosives such as nitroglycerin. TNT melts at 80
°C (176 °F), far below the temperature at which it will spontaneously detonate, allowing it to be poured as well as safely combined with other
explosives. TNT neither absorbs nor dissolves in water, which allows it to be used effectively in wet environments. Additionally, it is stable
compared to other high explosives."
I know Wikipedia is not the greatest reference, but it is usually right about most things.
As to the OP's question, a cost benefit analysis would have been done and there would definitely be more than one factor involved. Sometimes when a
resource is in high demand, for more than one application, a substitute will be used if possible for some of those applications so that the original
material can be used for the application where it is most valuable.
[Edited on 29-1-2014 by Hennig Brand]
"A risk-free world is a very dull world, one from which we are apt to learn little of consequence." -Geerat Vermeij
|
|
|
Motherload
Hazard to Others
 
Posts: 245
Registered: 12-8-2012
Location: Sewer
Member Is Offline
Mood: Shitty
|
|
Combat engineers use majority of the TNT in military for demolition.
Wherever a bulk quantity charges are required like cratering charges etc.
I believe naval ordnance still use TNT composition for the fillings.
"Chance favours the prepared mind"
"Fuck It !! We'll do it live !!"
|
|
|
Ral123
National Hazard
  
Posts: 735
Registered: 31-12-2011
Member Is Offline
Mood: No Mood
|
|
The only reason TNT is still interesting is it's castable and can make low sensitivity mixtures. Btw nitroguanidine has less energy density then TNT
and less stability then TATB. What makes it uniquely good, except as a propellant component?
|
|
|
Zyklon-A
International Hazard
   
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
I don't think that's the only reason that it's interesting, but the fact that it's castable is a great ability that it has.
|
|
|
Hennig Brand
International Hazard
   
Posts: 1284
Registered: 7-6-2009
Member Is Offline
Mood: No Mood
|
|
I wasn't suggesting that I thought nitroguanidine was a suitable replacement for TNT, or that it was a great explosive. I was just giving a few
possible reasons why one material might be used over another for a particular application. To tell the truth I don't know much about nitroguanidine,
except that it is a common ingredient in triple base smokeless powders. One of the biggest advantages of TNT is that it makes such good use of
resources. On an industrial scale the production of TNT makes extremely efficient use of resources.
"A risk-free world is a very dull world, one from which we are apt to learn little of consequence." -Geerat Vermeij
|
|
|