[Question]nitroglycol


Hi All,

I am thinking to prepare nitroglycol , do any body here have an experience about it and would like to share?

Ref : http://en.wikipedia.org/wiki/Ethylene_glycol_dinitrate
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2552
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 8-3-2014 at 05:24


I suggest you read:

http://www.sciencemadness.org/talk/viewthread.php?tid=27853




As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
Ral123
National Hazard
****




Posts: 735
Registered: 31-12-2011
Member Is Offline

Mood: No Mood

[*] posted on 8-3-2014 at 05:40


One of the easiest materials to cause a runaway. Constant stirring is essential. Good purification involves organic solvents and distilled water.
Initiation: Modern cap No8 or equivalent. Anything less and you might get brisance like smokeless powder.
http://www.youtube.com/watch?v=eFyWvvXosOk
View user's profile View All Posts By User
ecos
Hazard to Others
***




Posts: 464
Registered: 6-3-2014
Member Is Offline

Mood: Learning !

[*] posted on 8-3-2014 at 05:52


Thanks all for the info, I really appreciate it.

I have just few questions :

distilled water means i need purify water myself or water bottles are fine?

what is No8 modern cap ?

sorry if my questions are so newbie but i still learn :)
View user's profile View All Posts By User
Ral123
National Hazard
****




Posts: 735
Registered: 31-12-2011
Member Is Offline

Mood: No Mood

[*] posted on 8-3-2014 at 06:35


Deionized or tapwater can also work, but not optimal.
IMO you should start the hobby with black powder. Apparently you didn't even bother to google cap No8. I've had many accidents, witch are probably waiting for you too. If you have accident with 30ml EGDN because of peroxide detonator, it can be life changing.
View user's profile View All Posts By User
ecos
Hazard to Others
***




Posts: 464
Registered: 6-3-2014
Member Is Offline

Mood: Learning !

[*] posted on 8-3-2014 at 07:40


I tried to google cap No8 but the results seems to be dependent on my country.

do you mean that AP is sensitive to EGDN?
View user's profile View All Posts By User
Zyklon-A
International Hazard
*****




Posts: 1547
Registered: 26-11-2013
Member Is Offline

Mood: Fluorine radical

[*] posted on 8-3-2014 at 09:24


Usually, bottled water is purified first with distillation, then with reverse osmosis. So it is quite pure, minerals are added however, but only small amounts.

The best thing to do is read as much as possible on the subject.
Blasting cap.




View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2200
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 8-3-2014 at 10:03


Quote: Originally posted by Zyklonb  
Usually, bottled water is purified first with distillation, then with reverse osmosis. So it is quite pure, minerals are added however, but only small amounts.

In the US that is far from true, if it say distilled then it is distilled.
If it isn't distilled it is probably tap water boiled to kill bacteria.
Sometime it is carbon filtered or some other process but it is
rare.

Your mileage will vary in other countries which have standards.
View user's profile View All Posts By User
underground
National Hazard
****




Posts: 719
Registered: 10-10-2013
Location: Europe
Member Is Offline


[*] posted on 8-3-2014 at 11:31


Quote: Originally posted by ecos  
I tried to google cap No8 but the results seems to be dependent on my country.

do you mean that AP is sensitive to EGDN?


Why you want to try EGDN ? It will give to you lots of headaches as long as it has the tedency to evaporate. I personally prefer NG for that reason.

[Edited on 8-3-2014 by underground]
View user's profile View All Posts By User
Zyklon-A
International Hazard
*****




Posts: 1547
Registered: 26-11-2013
Member Is Offline

Mood: Fluorine radical

[*] posted on 8-3-2014 at 11:42


Quote:

In the US that is far from true, if it say distilled then it is distilled.

I don't know where you live in the US, but I've never seen a bottle of water that was purified only with distillation in more than five years. How can they charge $2.50 for a bottle of water if it's purified only with distillation.




View user's profile View All Posts By User
Ral123
National Hazard
****




Posts: 735
Registered: 31-12-2011
Member Is Offline

Mood: No Mood

[*] posted on 8-3-2014 at 11:54


Quote: Originally posted by underground  
Quote: Originally posted by ecos  
I tried to google cap No8 but the results seems to be dependent on my country.

do you mean that AP is sensitive to EGDN?


Why you want to try EGDN ? It will give to you lots of headaches as long as it has the tedency to evaporate. I personally prefer NG for that reason.

[Edited on 8-3-2014 by underground]

Do you realize you recommend to a complete novice one of the most volatile and dangerous synthesis that can be done? At least I've had many EGDN runaways and I can confirm non of them has even shown a flame or anything. All the plyol group nitroesters along with MN have quite dangerous synthesis. NC, EGDN, PETN, DEGDN, PGDN are at least somewhat more stable. Also EGDN gives almost twice the NG yield with 60% nitric.
View user's profile View All Posts By User
DubaiAmateurRocketry
National Hazard
****




Posts: 841
Registered: 10-5-2013
Location: LA, CA, USA
Member Is Offline

Mood: In research

[*] posted on 8-3-2014 at 12:07


EGDN has a Impact of 20cm, for 2kg, just a bit better than nitroglycerin! Someone please explain what the OP is trying to do...

Ral123, headache is only for some people, also you can get adapted to EGDN if you've synthesized a few times.
View user's profile View All Posts By User
Ral123
National Hazard
****




Posts: 735
Registered: 31-12-2011
Member Is Offline

Mood: No Mood

[*] posted on 8-3-2014 at 12:41


The headache is uncomfortable, so you suggest that:
http://www.youtube.com/watch?v=7SvW_P0safI
I've washed a NG sample multiple times with NaHCO3 and distilled water. It was crystal clear and still developed a brown-green layer within less then a month. EGDN has never done that and has never been easy to detonate with any kind of hitting.
View user's profile View All Posts By User
roXefeller
Hazard to Others
***




Posts: 463
Registered: 9-9-2013
Location: 13 Colonies
Member Is Offline

Mood: 220 221 whatever it takes

[*] posted on 8-3-2014 at 12:43


It's obvious that the OP is looking for the next step from AP with a simple monomolecular. We should remind him about safety requirements during nitroester production and EM in general. Start small and keep water at hand for drowning. Cool with ice/salt water bath. Add EG gradually. It's similar to nitroglycerin so read all about that but also read about its deadly history of accidents and risks. Sobrero was plagued with headaches because of it. Wash it till you're bored and then doubly before neutralizing. Use air bubbler or propeller to stir, no sticks thermometers or magnets. Bubbler needs glass because of corrosive acid. And finally stop looking for spoonfeeding and start reading more. Then learn stoich and beginner chem so you know the acid amounts. And for heavens sake don't leave it in a jar to vaporize and land in the threads, phlegmatize immediately ( yeah look it up). Although this thread really needs closed are their any EGDN specifics that need mentioned?
View user's profile View All Posts By User
DubaiAmateurRocketry
National Hazard
****




Posts: 841
Registered: 10-5-2013
Location: LA, CA, USA
Member Is Offline

Mood: In research

[*] posted on 8-3-2014 at 13:07


yes, I suggest the OP post on short question thread, most of OP's question's answers could be found here. This forum has covered countless variety of explosives and you can just search the forum. and http://www.sciencemadness.org/talk/viewthread.php?tid=27853
View user's profile View All Posts By User
Ral123
National Hazard
****




Posts: 735
Registered: 31-12-2011
Member Is Offline

Mood: No Mood

[*] posted on 8-3-2014 at 13:12


IMO this is quite a risk but here are some options for novices:
http://www.youtube.com/watch?v=XHT-mq16Y30
Secondaries for novices-AN/Al, UN, ANNMAl and some other less complicated and sensitive. The basecharges/boosters can be a problem.
View user's profile View All Posts By User
ecos
Hazard to Others
***




Posts: 464
Registered: 6-3-2014
Member Is Offline

Mood: Learning !

[*] posted on 9-3-2014 at 01:29



I have knowledge about energetic materials but i lag practical experience, i prepared before AP ,AN/Al ,ANFO ,..

but I never tried something with more power.

I would avoid NG because of its sensitivity and stability , Thats why I was thinking about EGDN

for EDNA : Ethylenedinitramine (EDNA) is a practical and powerful military explosive. Problem is, the routes to EDNA, as published always use either exotic chems or very high or very low pressures to form the precursor - ethyleneurea.

thanks all for the advices and the info shared above

View user's profile View All Posts By User
ecos
Hazard to Others
***




Posts: 464
Registered: 6-3-2014
Member Is Offline

Mood: Learning !

[*] posted on 9-3-2014 at 06:04


today , i will prepare my first sample of EGDN but I am worried a little bit about its storage.

what is the best methods for EGDN storage ?
View user's profile View All Posts By User
Ral123
National Hazard
****




Posts: 735
Registered: 31-12-2011
Member Is Offline

Mood: No Mood

[*] posted on 9-3-2014 at 06:44


Purification with NaHCO3, water and acetone. Store in cold, dark under water layer.
View user's profile View All Posts By User
Zyklon-A
International Hazard
*****




Posts: 1547
Registered: 26-11-2013
Member Is Offline

Mood: Fluorine radical

[*] posted on 9-3-2014 at 06:47


I would say, "don't", you could store it, sure, but it's dangerous.
Good luck.




View user's profile View All Posts By User
ecos
Hazard to Others
***




Posts: 464
Registered: 6-3-2014
Member Is Offline

Mood: Learning !

[*] posted on 9-3-2014 at 08:00


I always do purification with NaHCO3, water and measure the PH !
is it a must to use acetone for purification ?

what if i have excess amount that is not needed anymore... how can I get rid of it?

[Edited on 9-3-2014 by ecos]
View user's profile View All Posts By User
Ral123
National Hazard
****




Posts: 735
Registered: 31-12-2011
Member Is Offline

Mood: No Mood

[*] posted on 9-3-2014 at 08:04


Quote: Originally posted by Zyklonb  
I would say, "don't", you could store it, sure, but it's dangerous.
Good luck.

What's dangerous?
@ ecos, I doubt you can achieve perfect neutral Ph without acetone.
View user's profile View All Posts By User
hissingnoise
International Hazard
*****




Posts: 3940
Registered: 26-12-2002
Member Is Offline

Mood: Pulverulescent!

[*] posted on 9-3-2014 at 08:08


Its stability is appreciably better than that of nitro but its higher solubility makes washing difficult . . .

View user's profile View All Posts By User
ecos
Hazard to Others
***




Posts: 464
Registered: 6-3-2014
Member Is Offline

Mood: Learning !

[*] posted on 9-3-2014 at 08:30


I can reach around PH=7 with water and NaHCO3

I have a problem to understand how can I handle it or even transport it !

[Edited on 9-3-2014 by ecos]
View user's profile View All Posts By User
DubaiAmateurRocketry
National Hazard
****




Posts: 841
Registered: 10-5-2013
Location: LA, CA, USA
Member Is Offline

Mood: In research

[*] posted on 9-3-2014 at 10:33


You can transport in a glass bottle, and use a dropper to take them out, I think you can also pour it but slowly.

I really wont store something almost as sensitive as nitroglycerin in my home, if your parents clean or your sister run into your your room and accidentally drop the bottle, there would be tragedy.

Just burn it, it deflagrates beautifully with blue flame.
View user's profile View All Posts By User