[*] posted on 20-8-2015 at 08:50


@Fulmen,
Just asking:
Is the corrosion of your steel pieces not a problem?
I suspect molten nitrate 200-400°C might be rude to them; so will chlorides...




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1706
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 20-8-2015 at 09:03


Corrosion shouldn't be a problem with nitrates. It will probably oxidize the surface, but it should only form a thin layer.



We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
sussyn
Harmless
*




Posts: 7
Registered: 14-8-2015
Member Is Offline

Mood: No Mood

[*] posted on 21-8-2015 at 07:29


I have extra KNO2 if you're also interested in nitrite eutectics. Gotta check shipping costs etc, I'm not too experienced with the exept quantities rules since ORM-D went away, but I'll be happy to learn. There might be some NaNO2 hiding somewhere, too, or I can get some.
Good luck!
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1706
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 21-8-2015 at 11:53


Thank you for the offer, but I think I'll focus on the nitrates for now. This whole project has been delayed as my shop access has been severely restricted lately. But hopefully that will sort itself out during the winter, it would be nice to have this done by that time...



We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
Praxichys
International Hazard
*****




Posts: 1063
Registered: 31-7-2013
Location: Detroit, Michigan, USA
Member Is Offline

Mood: Coprecipitated

[*] posted on 21-8-2015 at 15:59


Lithium salts aren't that hard to come by. Lithium carbonate can be had for about $12/lb. The carbonate is a great point to start making lithium salts; all that is needed is to treat it with various acids.

Just a thought.

http://www.axner.com/lithium-carbonate-fine.aspx




View user's profile Visit user's homepage View All Posts By User
Fulmen
International Hazard
*****




Posts: 1706
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 21-8-2015 at 23:48


That is a fair point, I'll look into that.



We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
The Volatile Chemist
International Hazard
*****




Posts: 1981
Registered: 22-3-2014
Location: 'Stil' in the lab...
Member Is Offline

Mood: Copious

[*] posted on 23-8-2015 at 14:03


I saw the same thing on continentalclay.com. 1lb pack. Not too bad price-wise.



View user's profile Visit user's homepage View All Posts By User
chloric1
International Hazard
*****




Posts: 1116
Registered: 8-10-2003
Location: GroupVII of the periodic table
Member Is Offline

Mood: Stoichiometrically Balanced

[*] posted on 4-2-2018 at 04:50
Lithium salts


I have been trying to find the patent but no luck. Basically, the premise is if you start with lithium chloride and sodium nitrate( also bromide,iodide etc), you would mix strong solutions of the two then raise temperature to reduce volume causing NaCl to drop out. You FILTER HOT and keep reducing volume until another crop of NaCl drops out. Filter hot again. Now you have a strong lithium nitrate solution still contaminated with sodium chloride and perhaps unreacted lithium chloride and sodium nitrate. No here is where it gets interesting. Lithium salts have an uncanny ability to dissolve in polar organic solvents like methanol, ethanol, and acetone. So , as long as your lithium chloride is not in excess, you should be able to add excess alcohol or acetone to salt mix to drop out more sodium chloride as this will shift the equilibrium in favor. Filter again and evaporate your filtrate. Next to seal the deal, take crystal residue and dissolve in neat acetone or alcohol. This should virtually eliminate any further sodium from the lithium nitrate.

This is tedious but cost effective as you would not handle nitric acid. Lithium chloride solution is easily generated by adding the pottery grade lithium carbonate to diluted muriatic acid from home improvement store. Add slight excess of lithium carbonate to remove dissolved metals like iron from acid solution. Hope this is helpful.




Fellow molecular manipulator
View user's profile View All Posts By User
byko3y
National Hazard
****




Posts: 721
Registered: 16-3-2015
Member Is Offline

Mood: dooM

[*] posted on 4-2-2018 at 17:18


chloric1, dunno why you are thinking to mess with LiCl if you have Li2CO3 as a starting material. Solubility of lithium nitrate is only slightly higher in alcohol and acetone than solubility of lithium chloride. In this way you will get a mixture of LiCl+LiNO3.
View user's profile View All Posts By User
S.C. Wack
bibliomaster
*****




Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline

Mood: Enhanced

[*] posted on 5-2-2018 at 13:23


Weird how so many mixtures are supposed to melt at 145C. Fieser says 10 parts KNO3 7 parts NaNO2. Others replace some K with Na: 53:40:7. Or nitrates of K (65.8) and Ca (34.2). Even more Na for 142C: 44.2% KNO3, 48.9% NaNO2, 6.9% NaNO3 google says.



"You're going to be all right, kid...Everything's under control." Yossarian, to Snowden
View user's profile Visit user's homepage View All Posts By User
Texium
Administrator
Thread Moved
27-11-2023 at 11:48
 Pages:  1  2

  Go To Top