I got a crucible for free the other day. It's a good'un, too, capable of going up to at least 1200 C without a problem. Looks to be made of alumina, judging by how many were meant to just be 'thrown away' according to the professor who gave it to me.

My problem is, this particular crucible was used for making cobalt glass, and as such still has a coating of the latter across the bottom. I'd like to remove this, but I'm not sure how - would molten NaOH be sufficient, or would that attack the alumina of the crucible?




Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 9-4-2016 at 15:26


I bought 2 alumina/silicon cruicibles and stuffed a load of NaOH solution into one of them, which sat in there for a few days.

Cannot remember why i did that.

The NaOH worked it's way through the entire structure..

On the outer surface there were mosaic-like lines where the NaOH had penetrated all the way through.

On firing, it exploded.

[Edited on 9-4-2016 by aga]




View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 9-4-2016 at 17:54


Quote: Originally posted by aga  
I bought 2 alumina/silicon cruicibles and stuffed a load of NaOH solution into one of them, which sat in there for a few days.

Cannot remember why i did that.

The NaOH worked it's way through the entire structure..

On the outer surface there were mosaic-like lines where the NaOH had penetrated all the way through.

On firing, it exploded.

[Edited on 9-4-2016 by aga]


...Welp.

Not doing that, then.

Any other suggestions? Composition of the glass is approximately B56Si47O214Na30K20Ba6Zn5, according to my professor.




Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
View user's profile View All Posts By User
hyfalcon
International Hazard
*****




Posts: 1003
Registered: 29-3-2012
Member Is Offline

Mood: No Mood

[*] posted on 9-4-2016 at 20:55


When removing glaze from porcelain, ammonium bifluoride has worked for me, but be careful, it's still nasty stuff.
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6377
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 9-4-2016 at 22:23


Quote: Originally posted by elementcollector1  
Composition of the glass is approximately B56Si47O214Na30K20Ba6Zn5, according to my professor.


I thought you said it was cobalt glass?
I don't see any Co there.
:confused:




View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5135
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 10-4-2016 at 01:27


If it's a (largely) borate glass it might dissolve in molten borax.
Leftover borax can be washed out with warm water.
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 10-4-2016 at 06:25


Quote: Originally posted by j_sum1  
Quote: Originally posted by elementcollector1  
Composition of the glass is approximately B56Si47O214Na30K20Ba6Zn5, according to my professor.


I thought you said it was cobalt glass?
I don't see any Co there.
:confused:


Cobalt is there in trace amounts, i.e. 0.014g per 300g batch. This is actually enough to color the entire glass a strong purple-blue.