24/40 ptfe sleeves required


Can anyone point me to a cheap source for 24/40 ptfe sleeves ?


Although my Chinese NS24 glassware is good value,
I feel that the joints do not fit/seal as well as my Quickfit glassware,
also
I do not like the trade-off between potentially frozen joints, and grease pollution.


(I am in UK)




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
PirateDocBrown
National Hazard
****




Posts: 570
Registered: 27-11-2016
Location: Minnesota
Member Is Offline

Mood: No Mood

[*] posted on 18-3-2017 at 05:12


What do you call "cheap"? I know where they can be had in the US, but I'd almost rather have the grease, for the price they want.
View user's profile View All Posts By User
wg48
National Hazard
****




Posts: 821
Registered: 21-11-2015
Member Is Offline

Mood: No Mood

[*] posted on 18-3-2017 at 06:14


Quote: Originally posted by Sulaiman  
Can anyone point me to a cheap source for 24/40 ptfe sleeves ?

Although my Chinese NS24 glassware is good value,
I feel that the joints do not fit/seal as well as my Quickfit glassware,
also
I do not like the trade-off between potentially frozen joints, and grease pollution.

(I am in UK)


I have the same problem with some of my Chinese glassware. I checked the fit with lipstick. Some joints had the angle slightly wrong one appeared to be distorted. I now check all new ones against some quickfit I have.

I searched for ptf sleeves but did not find any that cost less than the price I paid for the glass.

I have tried plumber's PTF tape. Its seems effective but I have not tried it with vacuum.

I have also searched for details of how the joints are ground but only found general info.