Methanol to gasoline catalyst


Industrially alkanes are synthesized from
methanol with use of zeolite catalysts, through
dehydratation. Could there be alternative OTC
catalysts for this reaction(s)?
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 2-6-2018 at 18:00


Who on earth makes alkanes from methanol? That's definitely not how it's done industrially. Quite the opposite, actually.



View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1706
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 2-6-2018 at 23:21


David: You should research the subject first: http://www.cchem.berkeley.edu/molsim/teaching/fall2009/mto/b...

I actually worked on the development of such a catalyst 25 years ago. Sadly I don't remember anything useful about it, except that it was acidic. I remember characterizing it by weighing a sample in NH3 atmosphere at varying temperatures.

Finding a suitable OTC catalyst would probably be like looking for a needle in a haystack.




We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
battoussai114
Hazard to Others
***




Posts: 235
Registered: 18-2-2015
Member Is Offline

Mood: Not bad.... Not bad.

[*] posted on 3-6-2018 at 09:24


I would say that harder than finding a suitable catalyst would be controlling the reaction on a home lab. I may be mixing things up with the Fischer-Tropsch synthesis but aren't this sort of process usually ran in multitubular reactors because thermal runaway easily makes your product be carbonized material instead of an useful organic compound?

Anyway, you could start by checking on the properties and how to produce the SAPO-34 catalyst since it seems like one of the catalysts that's constantly being studied for MTO.




Batoussai.
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1706
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 3-6-2018 at 10:07


Sorry, I misread the OP. He's after alkanes, not alkenes. Alkanes are chip as dirt, there really isn't any reasons for making it from methanol.



We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 3-6-2018 at 16:15


Quote: Originally posted by Fulmen  
Sorry, I misread the OP. He's after alkanes, not alkenes. Alkanes are chip as dirt, there really isn't any reasons for making it from methanol.


Yeah, I had a brief search and found info about making alkenes from methanol, but there's no way it'd be economical to make alkanes from methanol.

And methanol is produced industrially from syngas (a mixture primarily consisting of hydrogen and carbon monoxide) which in turn is made from natural gas or just about any cheap leftover alkanes.