Rocket Fuel Cool. That is worth trying. Thanks! |
12-10-2015 at 06:02 by: Jasonf |
Rocket Fuel This is planned to be an all year project. This will give us hopefully plenty time to test, prototyp ... |
6-10-2015 at 07:00 by: Jasonf |
Rocket Fuel Because there is so much binder, do you think we should try a less viscous binder? What would you re ... |
6-10-2015 at 03:50 by: Jasonf |
Rocket Fuel We used 22 grams AN, 6 grams Al, 1 gram Sulfur, and 15 grams Silicone Caulk. 15 grams was more than ... |
5-10-2015 at 18:12 by: Jasonf |
Rocket Fuel The group went ahead and bought some silicone caulk. To make our fuel we ground our ammonium nitrate ... |
5-10-2015 at 17:11 by: Jasonf |
Rocket Fuel In our competition we not actually launching our engines into the air. We will put our finalized des ... |
2-10-2015 at 19:51 by: Jasonf |
Rocket Fuel In this article of Richard Nakka's research, neoprene contact cament "burned exceptionally good for ... |
1-10-2015 at 14:47 by: Jasonf |
Rocket Fuel Our group has bought about 55 pounds total of fuel. We got our fuel for a total of about $100. Our r ... |
1-10-2015 at 13:37 by: Jasonf |
Rocket Fuel Good point. I am not able to access my research at the moment but I should be able to post some rese ... |
30-9-2015 at 19:15 by: Jasonf |
Rocket Fuel I am doing a school project that will last the entire year. My team is planning to make a solid fuel ... |
30-9-2015 at 19:03 by: Jasonf |