NC boiled with NaHCO3, product dissapears partially?
I've always washed my NC with NaHCO3 solution, never noticed any loses in NC like 66% ! (never weigh ...
3-9-2013 at 02:17
by: hossam6006
A rare but interesting method for enhancing detonation performance
[quote]I believe that the exothermic phase transition energy is given off in the detonation wave and ...
28-8-2013 at 23:26
by: hossam6006
Performance measure for Nitrocellulose
@mayko:
I think the calculation isn't correct.
Trinitrate has a molecular weight of 828.56 (Encycl ...
28-8-2013 at 11:27
by: hossam6006
Performance measure for Nitrocellulose
@VladimirLem:
I wouldn't do large-scale primary ... I know someone who make ~2kg of acetone peroxid ...
28-8-2013 at 09:12
by: hossam6006
Performance measure for Nitrocellulose
@Dany:
Thanks. very informative refrence!

@plante1999:
Yes, cotton is cheap :)
looks like nitr ...
28-8-2013 at 07:52
by: hossam6006
Performance measure for Nitrocellulose
There are countless procedures for preparing NC, I usually do it this way:
- mix 5kg of HNO3 (conc ...
27-8-2013 at 15:17
by: hossam6006
Urea Nitrate + Aluminium Reactivity
Thanks guys, problem solved.

Both AN and UN are acidic, but sodium bicarbonate should never be us ...
27-8-2013 at 14:30
by: hossam6006
Urea Nitrate + Aluminium Reactivity
that's true Marvin
But AL powder is a very common additive to many explosives, propellants and oxid ...
21-8-2013 at 14:19
by: hossam6006
Urea Nitrate + Aluminium Reactivity
I tested a mixture of UN:AL / 12:1 many times without problems, but yesterday after 4 hours, the mix ...