Getting Discouraged With Organic Chemistry As A Hobby. Failed Steglich Esterification
I have a vacuum pump, ready to try this reaction again after stocking up on a few pounds of dry ice ...
17-7-2020 at 12:16
by: Cou
Getting Discouraged With Organic Chemistry As A Hobby. Failed Steglich Esterification
as far as i know, this is the first attempt of an SM user to do the steglich esterification at home. ...
16-7-2020 at 22:20
by: Cou
Do you think high school chemistry teachers often have students make Breaking Bad jokes?
In 11th grade AP chemistry, some students joked about which chemistry teacher would be best to appro ...
15-7-2020 at 20:23
by: Cou
Do you think high school chemistry teachers often have students make Breaking Bad jokes?
Like, students joking about making you a real life Walter white?
15-7-2020 at 16:21
by: Cou
Lab and insects
[url=https://www.youtube.com/watch?v=99Q1sB8oUtA]https://www.youtube.com/watch?v=99Q1sB8oUtA[/url]
11-7-2020 at 21:07
by: Cou
Chemical Availability Changes from 15 years ago (US)
I don't see why liability would be a concern either. The dollar store sells some really nasty stuff ...
11-7-2020 at 20:52
by: Cou
Cou's esters megathread
my sense of smell is already very weak to begin with (could be the reason why i like esters so much) ...
10-7-2020 at 20:53
by: Cou
Latest chemical order?
100 grams potassium dichromate, for making aldehydes and carboxylic acids from alcohols to find out ...
10-7-2020 at 20:51
by: Cou
Chemical Availability Changes from 15 years ago (US)
I believe the reason it's relatively hard to find chemicals as an amateur is just because demand is ...
10-7-2020 at 18:07
by: Cou
Cou's esters megathread
I read that the anosmia is rarely permanent.
10-7-2020 at 18:02
by: Cou
Cou's esters megathread
Very concerned after finding out that coronavirus can destroy your sense of smell.

It can't be co ...
10-7-2020 at 13:10
by: Cou
U.S. based suppliers that will sell to individuals?
Forgot about www.dudadiesel.com. A very good source of common chemicals such as sulfuric acid, metha ...
9-7-2020 at 00:27
by: Cou
U.S. based suppliers that will sell to individuals?
First I check amazon and ebay
if I can't find it there, I check www.elementalscientific.net (terrib ...
7-7-2020 at 19:39
by: Cou
Cou's esters megathread
Need help removing water from a small scale (0.06 mole) fischer esterification reaction. anhydrous m ...
5-7-2020 at 18:51
by: Cou
How to grow crystals & Why do they form?
Wikipedia is also a good resource.
https://en.wikipedia.org/wiki/Crystal
4-7-2020 at 13:38
by: Cou
Newe YouTube Video: Methyl Iodide Synthesis with Aluminum Foil
very ncie might try this x)
3-7-2020 at 22:12
by: Cou
Preparation of Iodomethane
very nice i might try this x)
3-7-2020 at 22:11
by: Cou
Preparation of elemental phosphorus
I cant find any iron retorts online x( gonna have to learn metalworking at the makerspace, or buy a ...
3-7-2020 at 10:53
by: Cou
Synthesis of longer chain tertiary alcohols
I've been wondering if the Steglich esterification would work for tertiary alcohols such 4-propylhep ...
3-7-2020 at 00:35
by: Cou
I don't really mind opening a new thread just to reply to this
Detritus is a comedy goldmine. I wish mods would open registration so I could laugh at dumb kooks, p ...
3-7-2020 at 00:26
by: Cou
New chemicals for sale !
I have to wait a while for cyclohexanol b/c COVID-19 has limited international shipping.
2-7-2020 at 18:36
by: Cou
Opinions of working with carcinogenic alkyl halides such as bromoethane?
If you want to get serious about organic chemistry, you eventually need to play with alkyl bromides. ...
1-7-2020 at 14:27
by: Cou
what is your take on spending absurd amounts of money on this hobby?
If "LiAbIlItY" is the concern, then why doesn't the dollar store get sued when an idiot drinks bleac ...
30-6-2020 at 09:40
by: Cou
what is your take on spending absurd amounts of money on this hobby?
Unfortunately we have to spend a lot of money on this hobby because most chemical suppliers have a s ...
30-6-2020 at 09:24
by: Cou
Cou's esters megathread
Again I forgot to check EVERY azeotrope before doing the dean-stark technique. 1-pentanol and water ...
29-6-2020 at 11:55
by: Cou