Search |
[Next Page] |
Destructive distillation of polypropylene The resulting oil appears to be completely different to the list of products given. Almost no pentan ... |
26-8-2019 at 01:58 by: 12thealchemist |
Destructive distillation of polypropylene In my case, they're polypropylene:
[file]76829[/file]
I've done destructive distillation of p ... |
26-8-2019 at 01:07 by: 12thealchemist |
Destructive distillation of polypropylene Some years ago I collected together a large quantity of waste polypropylene (PP) plastic in the form ... |
25-8-2019 at 06:38 by: 12thealchemist |
Is there any way to make 3 amino phenol from salicamide? The only issue is how to decarboxylate acetylsalicylic acid without cleaving the ester linkage - in ... |
18-4-2019 at 01:42 by: 12thealchemist |
Is there any way to make 3 amino phenol from salicamide? The Hoffman rearrangement or degradation would work to convert salicamide into 2-aminophenol.
3-a ... |
17-4-2019 at 04:44 by: 12thealchemist |
LiAlH4 via electrolysis I'm not sure at what temperature lithium metal will react with hydrogen, but I don't think it's at a ... |
10-4-2019 at 12:26 by: 12thealchemist |
T-butanol from Citric acid? [rquote=608056&tid=147577&author=fusso]@12ta some of the C in backbone is missing[/rquote]
... |
10-4-2019 at 00:34 by: 12thealchemist |
T-butanol from Citric acid? As I understand it, the proposed route looks something like this:
[file]74855[/file]
I have ... |
9-4-2019 at 01:07 by: 12thealchemist |
T-butanol from Citric acid? What reducing agent do you plan to use to reduce a carboxylic acid to an alkane, or alcohol then alk ... |
8-4-2019 at 12:24 by: 12thealchemist |
Silver nanoparticles [rquote=607275&tid=147281&author=woelen]If you used sterling silver (which normally is 0.925 ... |
3-4-2019 at 09:29 by: 12thealchemist |
Allotropes of Sulpher I've also recrystallised sulphur from toluene to excellent effect - it's fairly soluble in boiling t ... |
3-4-2019 at 08:44 by: 12thealchemist |
chemical waste books I have the offerings of popular YouTube channels? |
2-4-2019 at 11:53 by: 12thealchemist |
Silver nanoparticles My Master's research has been focused mainly on univalent gallium chemistry, but as a byproduct of f ... |
2-4-2019 at 09:05 by: 12thealchemist |
Allotropes of Sulpher There are many allotropes of sulphur. Rhombic and monoclinic are the most common. Rhombic sulphur is ... |
2-4-2019 at 08:39 by: 12thealchemist |
Make Potassium (from versuchschemie.de) My understanding is that typically if the reaction has been successful, visible balls of potassium f ... |
31-3-2019 at 13:06 by: 12thealchemist |
Carbon disulfide synthesis (alternative routes) I went through Reaxys a few months ago and compiled this:
[file]74726[/file]
I stripped out a ... |
31-3-2019 at 09:00 by: 12thealchemist |
Make Potassium (from versuchschemie.de) [rquote=606983&tid=14970&author=S.C. Wack]Is there a superior high yielding process if the g ... |
31-3-2019 at 08:55 by: 12thealchemist |
Make Potassium (from versuchschemie.de) The only issue with tetraglyme and higher glymes is increased cost. Triglyme is the smallest that ha ... |
31-3-2019 at 06:29 by: 12thealchemist |
Preparation of ionic phosphide from red P Is it possible to use some sort of inert heat dissipant, like sand for Zn3P2 or calcium fluoride (fl ... |
15-3-2019 at 05:44 by: 12thealchemist |
Predicting the color of an organic compound This might be of help: https://www2.chemistry.msu.edu/faculty/reusch/virttxtjml/spectrpy/uv-vis/uvsp ... |
12-3-2019 at 09:32 by: 12thealchemist |
Disodium 1,2-ethanediolate Production [rquote=605060&tid=146345&author=fusso]Could toluene azeotrope with the water and boil at lo ... |
12-3-2019 at 01:18 by: 12thealchemist |
Does anyone know much about how the mg catalyzed alkali reduction purification with dioxane works? I suspect that sterics are a factor as well as chelating. Assuming you need chelating properties, eu ... |
7-3-2019 at 01:05 by: 12thealchemist |
Make Potassium (from versuchschemie.de) I don't see why it wouldn't work; I'd have tried it myself but I don't have the capabilities at the ... |
7-3-2019 at 01:03 by: 12thealchemist |
How to concentrate azeotropic HNO3? [rquote=604619&tid=146120&author=fusso]Will H2SO4 dehydrate it into NO2 & O2?[/rquote]
... |
6-3-2019 at 07:38 by: 12thealchemist |
Make Potassium (from versuchschemie.de) You are correct, the catalyst should be added once the initial gas evolution ceases. This will be wh ... |
5-3-2019 at 01:30 by: 12thealchemist |