checkmark symbol
It also looks like a short-hand version of "square root."
29-11-2016 at 11:20
by: Ozone
tlc streaks from dipping
Don't dip the plate in your reagent solution.

Put the solution into a spray bottle and lightly mi ...
20-10-2016 at 15:12
by: Ozone
AMmunition from anfo?
It appears that ammonpulver will not fire in a rifle cartridge with the primer alone. A small booste ...
28-9-2016 at 06:45
by: Ozone
Protein powder half-life after mixed with water
Unless I've misunderstood your pictures, the bottle has generated gas. As such, fermentation is occu ...
26-9-2016 at 19:45
by: Ozone
Flat white. Lab style.
Here's how I did it after the power lines went down after hurricane Gustav in 2008.

Cheers,

O3
26-9-2016 at 17:41
by: Ozone
purity of vanillin for tlc stain
Agreed. I've had decent results with tech grade. You should always run a standard (or surrogate comp ...
26-9-2016 at 17:28
by: Ozone
Ridding Apparatus of Water
There is always the glove box, but...

When I'm really worried about water, especially that adsorb ...
26-9-2016 at 17:25
by: Ozone
Purity Testing
I'd look for "contract analytical services" or "enviromental testing."

If I was send this to a la ...
21-9-2016 at 09:23
by: Ozone
What's the most expensive substance you've bought?
WG48 -- I have to agree, that was (in terms of loss, both collateral and emotional) much more expens ...
6-9-2016 at 09:27
by: Ozone
What's the most expensive substance you've bought?
Probably Pediocin A. $252 for 50 micrograms.

Purified peptides are expensive!

O3
3-9-2016 at 07:06
by: Ozone
The trials & tribulations of Thorium production
Correct. It must be first activated to fissile 233-U (which is a natural isotope, but the abundance ...
25-8-2016 at 19:36
by: Ozone
The trials & tribulations of Thorium production
Yeah, that core smoked Harry Daghlian and Louis Slotin. Weapons-grade 239-Pu. Interestingly, the pre ...
24-8-2016 at 17:06
by: Ozone
People working with chloroform without gloves?
Nitrile and latex are awful with chlorinated organics! This is especially true for DCM. They are wor ...
19-8-2016 at 09:31
by: Ozone
Anhydrous AlCl3 handling and storage
Mine keeps well with a wax seal on the lid in a drybox.

O3
10-8-2016 at 18:23
by: Ozone
Unknown Substance
Hmm. Biohazard symbol. Found in a mine. Sounds a little shady, to me (don't you think?). I'd avoid i ...
2-8-2016 at 16:59
by: Ozone
how to prepare sand for chromatography
Just standing next to a good-sized object glowing red (and I mean the whole thing, not merely the bo ...
30-7-2016 at 06:16
by: Ozone
how to prepare sand for chromatography
Honestly, I don't see why you'd want to treat with alkali first (maybe to be rid of amorphous silica ...
29-7-2016 at 15:19
by: Ozone
how to prepare sand for chromatography
I am assuming you plan to use it to bed some other, more useful chromatographic media. We used to wa ...
28-7-2016 at 08:54
by: Ozone
Calcium carbonate solution
Even if you were to get hydroxide (which as you now know is strongly disfavored), it will scrounge C ...
11-7-2016 at 20:28
by: Ozone
Acrylic acid
I should also warn you that acrolein is *nasty*. I've run into few lachrymators that are worse, and ...
10-7-2016 at 08:02
by: Ozone
How to measure fermentable sugar in grass?
Also, I wouldn't recommend fermentation to ethanol as a method of assay--ethanol is but one of sever ...
21-6-2016 at 17:12
by: Ozone
How to measure fermentable sugar in grass?
Sucrose is not a reducing sugar, at all. To detect it via any conventional REDOX assay (e.g. DNS (di ...
21-6-2016 at 16:54
by: Ozone
Help explaining what happened - Oil bath w/ bleach boiling - broken jar..
I'm guessing the NaOH in the bleach may have made some soap and the layer you are looking at is emul ...
16-6-2016 at 17:58
by: Ozone
Can sublimation occur in CH4?
That article is talking about fixing CO2 as limestone.

Aside, the most common form of "solid" met ...
15-6-2016 at 18:29
by: Ozone
purification of ketones
No. IIRC, It works for aldehydes and methyl ketones.

O3
14-6-2016 at 15:34
by: Ozone