| Search |
Sell out... (Europe only) [rquote=475449&tid=71954&author=TheMrbunGee][rquote=475424&tid=71954&author=Alzador] ... |
21-2-2017 at 12:34 by: Alzador |
Sell out... (Europe only) How much for the phosphorus? And the NaBH4?
[Edited on 21-2-2017 by Alzador] |
21-2-2017 at 04:22 by: Alzador |
Science equipment looking for a home Hi!
Would anyone have a hot plate stirrer for sale located in the EU? I can only find shitty ones ... |
21-2-2017 at 02:10 by: Alzador |
Synthesis of Natural Smells [rquote=430559&tid=64584&author=Amos]I just made benzaldehyde recently, and its smell is EXA ... |
10-12-2015 at 13:27 by: Alzador |
Separation of Potassium ions from solution. Thank you for your answer I will try this. Never heard of this before . Basically I just wanted ... |
6-12-2015 at 02:10 by: Alzador |
Separation of Potassium ions from solution. Hello everyone!
Yesterday I did an experiment: I had some KMnO[sub]4[/sub] solution on hand that ... |
6-12-2015 at 00:52 by: Alzador |
Preparation of Chromate/Dichromate [rquote=419816&tid=63317&author=blogfast25][rquote=419806&tid=63317&author=Alzador]I ... |
19-9-2015 at 22:36 by: Alzador |
Preparation of Chromate/Dichromate Apart from producing alkaline conditions in the reaction, is there any benefit from mixing K[sub]2[/ ... |
18-9-2015 at 02:56 by: Alzador |
Molybdenum at home Well since I only have coffee filter atm at home I highly doubt it will filter
but once I get my ... |
4-2-2015 at 10:18 by: Alzador |
Molybdenum at home Will do but I highly doubt it that I could filter it off..it's particle size is extremely fine.. I t ... |
4-2-2015 at 06:17 by: Alzador |
Molybdenum at home That sounds really nice but I don't know how to catch the low boiling vapours for separation from th ... |
4-2-2015 at 05:27 by: Alzador |
Molybdenum at home Could other solvents be used to wash the solid from? Pentane or Heptane? Or something more polar lik ... |
4-2-2015 at 01:17 by: Alzador |
Molybdenum at home Well.. here you can see my source of MoS[sub]2[/sub]: a red can of rust dissolver/lubricant. Sadly I ... |
2-2-2015 at 13:37 by: Alzador |
Molybdenum at home Thank you very much for the thorough explanation I will post pics when I will
obtain results. 
... |
31-1-2015 at 22:51 by: Alzador |
Molybdenum at home Could you explain how slag fluidisers work? |
29-1-2015 at 08:14 by: Alzador |
Molybdenum at home Well thank you for your thoughts I'm going to try the aluminothermic way in the
next few days and ... |
29-1-2015 at 00:17 by: Alzador |
Molybdenum at home yes :/ i'm aware that carbon reduction is not an option at home. I think I should go with hydrogen ... |
28-1-2015 at 05:49 by: Alzador |
Molybdenum at home Thank you for the fast reply!
My goal with this would absolutely not be to obtain 99.99% pure Mo ... |
28-1-2015 at 03:10 by: Alzador |
Molybdenum at home Hi guys!
Recently I found a can of dry lubricant which - according to the label - contains molybd ... |
28-1-2015 at 02:16 by: Alzador |