Homemade carbon electrodes
I conducted several more experiments with electrodes with saturated polyurethane varnishes and alkyd ...
18-2-2024 at 21:35
by: Hexabromobenzene
Sulfur, calcium thiosulfate from gypsum
500 gr powder of burned gypsum board was mixed with 150 grams powder of charcoal. The mixture was ...
18-2-2024 at 21:25
by: Hexabromobenzene
Synthesis of benzene from PET water bottles
[rquote=690439&tid=160130&author=dettoo456]Nice job. The yield is kind of shit considering t ...
26-1-2024 at 10:26
by: Hexabromobenzene
Synthesis of benzene from PET water bottles
Have you had problems with clogged pipes? When pyrolyzing PET bottles WITHOUT calcium oxide, a large ...
26-1-2024 at 10:20
by: Hexabromobenzene
Homemade carbon electrodes
If you have a lot of graphite, you can use it. The task of the first baking to form an electrical co ...
24-1-2024 at 05:33
by: Hexabromobenzene
Homemade carbon electrodes
I also conducted experiments with the production of carbon electrodes.
The main problem from the el ...
4-1-2024 at 18:00
by: Hexabromobenzene
NaClO3 by electrolysis
I used technical salt with magnesium impurties. Works better due tu cathode protection by magnesium ...
20-10-2023 at 10:55
by: Hexabromobenzene
Plant Ash
I leached more 100 kg different plant ashes for many years. Mainly trees. Average soluble salt conte ...
20-10-2023 at 10:46
by: Hexabromobenzene
Diammonium phosfate uses
Diammonium phosphate decomposes to polyphosphoric acid and ammonia. Polyphosphoric acid may be easy ...
20-10-2023 at 10:38
by: Hexabromobenzene
Homemade carbon electrodes
Experiments with homemade carbon electrodes have been completed. Here is the information that was ob ...
20-10-2023 at 10:28
by: Hexabromobenzene
Butyric acid and butanol fermentation revisited
A fermentation of starch raw materials can be obtained by butanol or butyric acid. An article was wr ...
5-8-2023 at 18:36
by: Hexabromobenzene
Homemade carbon electrodes
Lead salts under these conditions form lead. During electrolysis, it forms lead dioxide. But I do no ...
17-6-2023 at 08:32
by: Hexabromobenzene
Homemade carbon electrodes
I also conducted experiments on the manufacture of carbon electrodes. This time I tried catalytic gr ...
16-6-2023 at 07:57
by: Hexabromobenzene
Homemade carbon electrodes
Here is a graph of the conductivity of carbon from fiberboard as a function of temperature. For char ...
24-5-2023 at 15:35
by: Hexabromobenzene
Homemade carbon electrodes
The electrodes were saturated with sugar syrup and again in the furnace. They became better. Now the ...
24-5-2023 at 14:26
by: Hexabromobenzene
Homemade carbon electrodes
For the preparation of electrodes, a denser coal was tested. It was made from laminated MDF fiberboa ...
21-5-2023 at 19:03
by: Hexabromobenzene
Homemade carbon electrodes
As i know charcoal is hard carbon. Its not grapitizate. But strong heat may increase conductivity. N ...
18-5-2023 at 07:42
by: Hexabromobenzene
Homemade carbon electrodes
[rquote=684126&tid=159561&author=mysteriusbhoice][rquote=684113&tid=159561&author=Jo ...
16-5-2023 at 05:50
by: Hexabromobenzene
Homemade carbon electrodes
Yes, but this need to buy it. My method allows you to make an electrode of any size and shape yours ...
14-5-2023 at 14:17
by: Hexabromobenzene
Homemade carbon electrodes
The inert anode is a very important thing for electrochemistry. Both organic and not organic. Typica ...
13-5-2023 at 16:50
by: Hexabromobenzene
HELP! EU/DE/FR: Impending infrastructural apocalypse and possibility of civil war
The topic is initially politicized. But I expressed my thoughts in accordance with amateur chemistry ...
8-3-2023 at 08:19
by: Hexabromobenzene
HELP! EU/DE/FR: Impending infrastructural apocalypse and possibility of civil war
[rquote=682132&tid=158800&author=blogfast25][rquote=682107&tid=158800&author=Hexabro ...
8-3-2023 at 00:18
by: Hexabromobenzene
EU illegal chemicals -> useful legal ones?
If you have a hobby at home chemistry then it is better not to tell anyone about it. Most people do ...
6-3-2023 at 12:20
by: Hexabromobenzene
HELP! EU/DE/FR: Impending infrastructural apocalypse and possibility of civil war
[rquote=676113&tid=158800&author=Tsjerk][rquote=676089&tid=158800&author=Hexabromobe ...
6-3-2023 at 12:14
by: Hexabromobenzene
Trying to Build First Electrolytic Cell: Diaphragm/Ion Permeable Membrane?
I dont have PVC glue and solvent for PVC. I can make polystyrene glu
6-3-2023 at 12:06
by: Hexabromobenzene
[Next Page]

  Go To Top