diy continuous electrowinning copper sheet metal Good point, so we're back to solid copper or galvanized. From a practical standpoint, solid Cu stand ... |
3-4-2024 at 15:26 by: Johanson |
diy continuous electrowinning copper sheet metal Okay I finally understand; so you're going to make relatively thick copper sheeting (for roofing, et ... |
2-4-2024 at 19:35 by: Johanson |
Why does my Mg-Cu galvanic cell produce the wrong voltage? Out of curiosity I just set up simple Mg-Cu and Zn-Cu cells using parts laying around my workbench, ... |
29-1-2024 at 19:49 by: Johanson |
Disposing of Tollen's Reagent After Silver Mirror Reaction Frozen, sounds just like the well known silver christmas ornament lab. A little HCl will drop out wh ... |
16-12-2023 at 22:12 by: Johanson |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. "Since people believe nickel plating 'hard' to do; answers found here are useful."
Well, I only men ... |
25-11-2023 at 09:19 by: Johanson |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. I'm still following this b/c plating/electrochem fascinates me for some reason. HOWEVER, I'm still b ... |
24-11-2023 at 08:42 by: Johanson |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. Okay, your claim, "my chemistry background is weak" is obviously a bit exaggerated. Nice video BTW. ... |
23-11-2023 at 13:08 by: Johanson |
Anyone go to university chemistry seminars? Or view chem department profiles? Texium: Calm down, the original question was aimed at non-students. I'm sorry my response got under ... |
23-11-2023 at 12:57 by: Johanson |
Anyone go to university chemistry seminars? Or view chem department profiles? Yeah, I wasn't intending to promote a siege mentality, as Texium implies. I just don't have time to ... |
21-11-2023 at 17:50 by: Johanson |
Anyone go to university chemistry seminars? Or view chem department profiles? Uhhggg.... to watch your words twisted by others!
Why do I need to be villianised in your respon ... |
21-11-2023 at 15:56 by: Johanson |
Anyone go to university chemistry seminars? Or view chem department profiles? Anyone go to university chemistry seminars?
Not interested! PowerPoint presentations by chemistr ... |
21-11-2023 at 09:36 by: Johanson |
Electroplating of Nickel, waterless / organic solvent / possibly ionic liquids. No one has commented yet, so I'll give it a go....
Your persistence is impressive (400 attempts?! ... |
21-11-2023 at 08:50 by: Johanson |
Should your family know what you are doing? Q: How do you cope with this situation?
All your wife said was, "Don't set the house on fire". So ... |
24-10-2023 at 18:13 by: Johanson |
Potassium mirror ? Dang nice! Would you mind showing us your heating arrangement/apparatus? |
16-8-2023 at 13:09 by: Johanson |
Non polar/oil soluble copper salts synthesis? "The purpose is for outdoor wood preservation"
The classic copper-based product was known as Cupr ... |
16-8-2023 at 13:04 by: Johanson |
How to make the air in my lab less oxidizing?? Sulaiman: "I suppose that UK/EU heating costs have risen significantly since I was home due to the i ... |
14-8-2023 at 09:48 by: Johanson |
How to make the air in my lab less oxidizing?? "Does anybody know a good way to do this?"
First, your location says "Sweden" so I assume it's cold ... |
12-8-2023 at 21:58 by: Johanson |
How does silicone react with bleach and mold removal foam? Several methods you could try, depending on what your countertop is made of
1. a little heat and a ... |
12-8-2023 at 21:27 by: Johanson |
Plastic Recycling Factory Up In Smoke Looks like a polyethylene pipe manufacturer, "United Poly Systems". Massive fire indeed.
That's on ... |
7-8-2023 at 14:35 by: Johanson |
Lactic acid From "Industrial Chemistry", sorry for the quality:
"Lactic acid is formed by the action of Bacte ... |
2-8-2023 at 14:31 by: Johanson |
Lactic acid Interesting problem. Apparently not easy to separate from water via distillation due to its affinity ... |
1-8-2023 at 21:50 by: Johanson |
getting rid of hydrogen gas "...but what apparatus would a professional lab use to deal with very large amounts of h2 gas that i ... |
29-7-2023 at 08:55 by: Johanson |
getting rid of hydrogen gas "....what sort of fan and filter would be effective?"
Gransolo you are going to blow yourself up, ... |
27-7-2023 at 11:18 by: Johanson |
Chemical computers/Chemical electronic devices "....and having a monthly budget so small that it might as well be inexistent"
Okaaay... then why d ... |
9-7-2023 at 12:26 by: Johanson |
Chemical computers/Chemical electronic devices The "integration of chemistry and electronic devices" (from your original post) is exemplified by ba ... |
8-7-2023 at 18:13 by: Johanson |