Rookie question - drying potassium hydroxide Putting it in a stainless steel pot and just heating it on the stove works pretty well imo. If you h ... |
5-10-2024 at 11:40 by: Junk_Enginerd |
NO2 refusing to condense What about the oxygen in the air?
Yes, 60% technical grade nitric acid, pure copper. I mean, clea ... |
24-2-2024 at 08:29 by: Junk_Enginerd |
NO2 refusing to condense I wanted to make some liquid NO2/N2O4 just as an interesting thing to do and because it looks pretty ... |
24-2-2024 at 01:30 by: Junk_Enginerd |
Nitric acid bottles growing exterior crystals? Ahhh yeah of course. I was wondering what on earth the supposed NO2 could be forming salts with just ... |
22-1-2024 at 05:52 by: Junk_Enginerd |
Nitric acid bottles growing exterior crystals? I have a bottle of nitric acid that's started growing crystals after a year or so. It's mostly aroun ... |
21-1-2024 at 05:33 by: Junk_Enginerd |
Can hydrogen peroxide be vacuum distilled straight from sodium percarbonate? Oh I will [b]not[/b] be mixing it with anything that can be regarded as fuel lol. At least not in th ... |
21-1-2024 at 05:26 by: Junk_Enginerd |
Can hydrogen peroxide be vacuum distilled straight from sodium percarbonate? [rquote=690265&tid=160113&author=Fery]This is an interesting idea. But H2O has lower b.p. an ... |
19-1-2024 at 06:02 by: Junk_Enginerd |
Can hydrogen peroxide be vacuum distilled straight from sodium percarbonate? The way I've understood it, it's basically sodium carbonate hydrated by h2o2 instead of h2o. Could o ... |
18-1-2024 at 12:50 by: Junk_Enginerd |
Non polar/oil soluble copper salts synthesis? [rquote=686728&tid=159805&author=Fery]Maybe precipitating Cu soaps like CuSO4 (aq) + Na palm ... |
17-8-2023 at 05:43 by: Junk_Enginerd |
Non polar/oil soluble copper salts synthesis? [rquote=686728&tid=159805&author=Fery]Maybe precipitating Cu soaps like CuSO4 (aq) + Na palm ... |
17-8-2023 at 00:13 by: Junk_Enginerd |
Non polar/oil soluble copper salts synthesis? I want to experiment with copper salts that are soluble in oil. The purpose is for outdoor wood pres ... |
16-8-2023 at 09:36 by: Junk_Enginerd |
Fortifying UV curing 3d printer acrylic resin with polyester resin? Hmm. I looked at some video a while ago that explained why acrylic is usually the base of these resi ... |
6-2-2023 at 23:24 by: Junk_Enginerd |
Fortifying UV curing 3d printer acrylic resin with polyester resin? [rquote=681260&tid=159305&author=Twospoons]Resin based 3d printing is not new. Its been arou ... |
6-2-2023 at 03:58 by: Junk_Enginerd |
Confusion on SO3 Synthesis [rquote=680793&tid=159069&author=SaccharinSlayer157]This is not going as planned...
There ... |
5-2-2023 at 06:12 by: Junk_Enginerd |
Fortifying UV curing 3d printer acrylic resin with polyester resin? Seems like it's such a new industry that I wouldn't be surprised if it was uncharted territory. I al ... |
5-2-2023 at 04:36 by: Junk_Enginerd |
Fortifying UV curing 3d printer acrylic resin with polyester resin? My limited understanding of how the UV curing resins that DLP 3d printers use work suggests that I s ... |
4-2-2023 at 02:05 by: Junk_Enginerd |
What is soldering iron tip refresher? [rquote=680332&tid=159225&author=Sulaiman]My google skills failed me!
I did not find an ms ... |
15-1-2023 at 01:40 by: Junk_Enginerd |
best route to WFNA Related to this, I have a question... If you have RFNA, but it's not maximum concentration, and you ... |
15-1-2023 at 01:32 by: Junk_Enginerd |
hho electrolysis plate configuration [rquote=680043&tid=159183&author=Mateo_swe]Junk_Enginerd, you said you used at maximum 1500W ... |
4-1-2023 at 06:41 by: Junk_Enginerd |
Is there a not too complex route to make benzyl alcohol from styrene? It sounds like an interesting synthesis to try out. Apparently styrene can be oxidized to benzyl alc ... |
4-1-2023 at 06:21 by: Junk_Enginerd |
Why can't I make soft clay by mixing with oil rather than water? Well I'll be damned. Laundry softener did it. Soft supple clay, using paraffin oil as base. I did NO ... |
2-1-2023 at 06:17 by: Junk_Enginerd |
Nitric acid skin burn Thought my thread might be mentioned. It took two or three months IIRC until it
was fully healed, ... |
2-1-2023 at 06:14 by: Junk_Enginerd |
hho electrolysis plate configuration [rquote=679965&tid=159183&author=Parakeet]Sorry if this question is off topic.
I have a so ... |
31-12-2022 at 05:14 by: Junk_Enginerd |
Tungsten trioxide My gut says it's not soluble in anything really, and wikipedia reinforces that by suggesting hydrofl ... |
31-12-2022 at 05:05 by: Junk_Enginerd |
hho electrolysis plate configuration Clever and simple design. One thing that stopped me from trying a separated output cell like this wa ... |
29-12-2022 at 13:01 by: Junk_Enginerd |