Search |
Plating silver over copper I have been looking all over the internet on electroplating silver without the use of AgCN and final ... |
2-8-2013 at 23:21 by: Mitchell |
Copper Cathode Electrolysis Thank you everyone for your responses.
I think I have solved the problem. So after finally gett ... |
2-8-2013 at 21:52 by: Mitchell |
Copper Cathode Electrolysis Oh I almost forgot, when I reversed the polarity of the salt cell the copper was anode and plat ... |
1-8-2013 at 16:29 by: Mitchell |
Copper Cathode Electrolysis So based on the first point.I have tried using MgSO4 as an electrolyte and using the same electrodes ... |
1-8-2013 at 13:26 by: Mitchell |
Copper Cathode Electrolysis To start out this isn't another chlorate post. As I realize how much it is frowned upon among th ... |
31-7-2013 at 20:11 by: Mitchell |
Copper Cathode Electrolysis 25430 |
31-7-2013 at 20:11 by: Mitchell |