Reclaiming Pd from scrap SMD ceramic capacitors
[rquote=233553&tid=18520&author=Fleaker]No, palladium is completely soluble in 30% nitric ac ...
19-1-2012 at 16:13
by: Samuel-a
Reclaiming Pd from scrap SMD ceramic capacitors
[rquote=233373&tid=18520&author=Arthur Dent]Okay so to recap the procedure described above:
...
16-1-2012 at 12:43
by: Samuel-a
Reclaiming Pd from scrap SMD ceramic capacitors
Hi Aqua_Fortis_100%

Nice to see your experiment.

As i understand, the black solution was obtai ...
15-1-2012 at 14:53
by: Samuel-a